Polylactide (PLA)/bamboo fiber biocomposites treated with an alkali solution and
a silane coupling agent were prepared by melt compounding. The PLA composite
containing delignified bamboo fibers showed a narrow decomposition range of
300–400 °C compared to the PLA composite containing pristine bamboo fiber
(210–430 °C). The tensile and flexural moduli of the treated PLA/bamboo fiber
composite incr... hiện toàn bộ