Microstructure, adhesion and growth kinetics of protective scales on metals and alloys

Springer Science and Business Media LLC - Tập 18 Số 5-6 - Trang 245-284 - 1982
H. M. Hindam1, D. P. Whittle2
1Molecular and Materials Research Division, Lawrence Berkeley Laboratory and Department of Materials Science and Mineral Engineering, University of California, Berkeley,
2Department of Materials Science and Mineral Engineering, University of California, Berkeley

Tóm tắt

Từ khóa


Tài liệu tham khảo

Kofstad and K. P. Lillerud,J. Electrochem. Soc. 127, 2410 (1980).

D. P. Whittle and J. Stringer,Philos. Trans. R. Soc. London A Ser. 295, 309 (1980).

G. C. Wood and F. H. Stott, Proceedings of NACE Conference on ?High Temperature Corrosion,? San Diego, California (March 1981).

F. Elrefaie and W. W. Smeltzer,J. Electrochem. Soc. 128, 2237 (1981).

H. Davies and W. W. Smeltzer,J. Electrochem. Soc. 121, 543 (1971).

A. U. Seybolt,J. Electrochem. Soc. 107, 147 (1960).

M. A. J. Th. Laheij, F. J. J. Van Loo, and R. Metselaar,Oxid. Met. 14, 207 (1980).

L. M. Atlas and W. K. Sumida,J. Am. Ceram. Soc. 41, 157 (1958).

J. A. Imlach and F. F. Glasser,Trans. J. Br. Ceram. Soc. 70, 227 (1971).

F. S. Pettit,Trans. Metall. Soc. AIME 239, 1296 (1967).

N. Birks and H. Rickert,J. Inst. Met. 91, 308 (1963).

C. Wagner,J. Electrochem. Soc. 99, 369 (1952).

D. P. Whittle, G. C. Wood, D. J. Evans, and D. B. Scully,Acta Metall. 15, 1747 (1965).

C. S. Giggins and F. S. Pettit,Trans. Metall. Soc. AIME,245, 2509 (1969).

P. Moulin, F. Armanet, G. Beranger, and P. Lacombe,Mem. Sci. Rev. Metall. 74, 143 (1977).

C. Wagner,Corros. Sci. 5, 751 (1965).

J. Stringer, B. A. Wilcox, and R. I. Jaffee,Oxid. Met. 5, 11 (1972).

J. Stringer, Electric Power Research Institute, Palo Alto, California, private communication.

C. S. Giggins and F. S. Pettit,Trans. Metal. Soc. AIME 245, 2495 (1969).

I. A. Kvernes,Oxid. Met. 6, 45 (1973).

H. M. Flower and B. A. Wilcox,Corros. Sci. 17, 243 (1977).

P. Moulin, A. M. Huntz, G. Beranger, and P. Lacombe,Scr. Metall. 11, 533 (1977).

M. J. Fleetwood,J. Inst. Met. 94, 218 (1966).

J. D. Whittenberger,Metall. Trans. 4, 715 (1973).

D. Delaunay, A. M. Huntz, and P. Lacombe,Scr. Metall. 13, 419 (1979).

A. Green, M. Eng. thesis, University of Liverpool, United Kingdom (1975).

G. W. Roper and D. P. Whittle,Met. Sci. J. 14, (1980).

E. Scheil and E. H. Schulz,Arch. Eisenhuttenwes. 6, 155 (1932).

G. R. Wallwork and A. Z. Hed,Oxid. Met. 3, 171; 213; 229; 243 (1971).

W. H. Gitzen, ed.,Al2O3 as a Ceramic Material, American Ceramic Society Publication No. 4 (1970).

F. S. Gallasso,Structure and Properties of Inorganic Solids, International Series in Solid State Physics, Vol. 7 (1970).

F. A. Kröger, Proceedings of NACE Conference on ?High Temperature Corrosion,? San Diego, California (March 1981).

K. A. Hay, Report RD/L/R 1673, Central Electricity Research Laboratory, Leatherhead, England (1970).

R. Linder and Å. Åkertrøm,Z. Phys. Chem. N. F. 6, 162 (1956).

L. C. Walters and R. E. Grace,J. Appl. Phys. 36, 2331 (1965).

Y. Oishi and W. D. Kingery,J. Chem. Phys. 33, 480 (1960).

A. E. Paladino and W. D. Kingery,J. Chem. Phys. 37, 957 (1962).

K. P. R. Reddy and A. R. Cooper, Abstracts,Am. Ceram. Soc. Bull. 55, 402, (1976);57, 306 (1978); quoted in Ref. 41.

D. J. Reed and B. J. Wuensch,J. Am. Ceram. Soc. 63, 88 (1980).

W. C. Hagel and A. U. Seybolt,J. Electrochem. Soc. 108, 1146 (1961).

W. C. Hagel,J. Am. Ceram. Soc. 48, 70 (1965).

C. S. Griggins and F. S. Pettit,Metall. Trans. 2, 1071 (1971).

W. C. Hagel, P. L. Jorgensen, and D. S. Tomalin,J. Am. Ceram. Soc. 49, 23 (1966).

P. D. Ownby and G. E. Jungguist,J. Am. Ceram. 55, 433 (1971).

J. W. Halloran and H. U. Anderson,J. Am. Ceram. 57, 150 (1974).

J. M. Neve and R. L. Coble,J. Am. Ceram. 57, 274 (1974).

H. A. Wang and F. A. Kröger,J. Am. Ceram. 63, 613 (1980).

J. K. Tien and F. S. Pettit,Metall. Trans,3, 1587 (1972).

K. P. R. Reddy, J. L. Smialek, and A. R. Cooper, preprint.

D. J. Young and M. Cohen,J. Electrochem. Soc. 124, 769; 775 (1977).

J. L. Smialek,Metall. Trans. 9A, 309 (1978).

H. Hindam and W. W. Smeltzer,J. Electrochem. Soc. 127, 1630 (1980).

E. J. Felten and F. S. Pettit,Oxid. Met. 10, 189 (1976).

J. S. Sheasby and D. B. Jory,Oxid. Met. 12, 527 (1978).

D. Caplan, A. Harvey, and M. Cohen,Corros. Sci. 3, 161 (1963).

D. Caplan and G. I. Sproule,Oxid. Met. 9, 459 (1975).

T. Homma, H. Hindam, Y. Pyun, and W. W. Smeltzer, in press.

D. Mortimer and M. L. Post,Corros. Sci. 8, 499 (1968).

K. P. Lillerud and P. Kofstad,J. Electrochem. Soc 127, 2397 (1980).

F. A. Golightly, F. H. Stott, and G. C. Wood,Oxid. Met. 10, 163 (1976).

F. A. Golightly, F. H. Stott, and G. C. Wood,J. Electrochem. Soc. 126, 1035 (1979).

F. A. Golightly, G. C. Wood, and F. H. Stott,Oxid. Met. 14, 217 (1980).

D. G. Barnes, J. M. Calvert, K. A. Hay, and D. G. Lees,Philos. Mag. 28, 1303 (1973).

D. G. Lees and J. M. Calvert,Corros. Sci. 16, 767 (1976).

Y. Ikeda and K. Nii,Oxid. Met. 12, 487 (1978).

J. Stringer and I. G. Wright,Oxid. Met. 5, 59 (1972).

I. G. Wright and B. A. Wilcox,Oxid. Met. 8, 283 (1974).

O. T. Goncel, J. Stringer, and D. P. Whittle,Corros. Sci. 18, 701 (1978).

H. Hindam and D. P. Whittle, in press.

C. S. Giggins and F. S. Pettit, Report ARL 75-0234, Pratt and Whitney Aircraft, Connecticut (1975).

J. D. Kuenzly and D. L. Douglass,Oxid. Met. 8, 139 (1974).

A. Kumar, M. Hasrallah, and D. L. Douglass,Oxid. Met. 8, 227 (1974).

J. Stringer, I. M. Allam, and D. P. Whittle,Thin Solid Films,45, 377 (1977).

I. M. Allam, D. P. Whittle, and J. Stringer,Oxid. Met. 12, 35 (1978).

I. M. Allam, Ph.D. thesis, University of Liverpool (1979).

I. M. Allam, D. P. Whittle, and J. Stringer,Oxid. Met. 13, 381 (1979).

J. L. Smialek, NASA Technical Memorandum 81676, Cleveland, Ohio (1981).

Hindam, ?Microstructure and Growth of Al2O3 on Ni-Al Alloys,? Ph.D. thesis, McMaster University, Hamilton, Ontario (1979).

H. Hindam and D. P. Whittle, in preparation.

J. Stringer, A. Z. Hed, G. R. Wallwork, and B. A. Wilcox,Corros. Sci. 12, 625 (1972).

H. E. Evans, D. A. Hilton, R. A. Holm and S. J. Webster,Oxid. Met. 12, 473 (1978).

H. Hindam and D. P. Whittle,J. Electrochem. Soc. 129, 1147 (1982).

J. Markali, inMechanical Properties of Engineering Ceramics, W. W. Kriegel and H. Palmour, eds. (Interscience, New York, 1961).

D. J. Barber,Philos. Mag. 10, 75 (1964).

E. A. Gulbransen,Mem. Sci. Rev. Metall. 62, 253 (1965).

R. L. Tallman and E. A. Gulbransen,J. Electrochem. Soc. 114, 1227 (1967).

G. C. Wood and T. Hodgkiess,J. Electrochem. Soc. 113, 319 (1966).

G. C. Wood and D. P. Whittle,J. Electrochem. Soc. 115, 126; 133 (1968).

H. W. Paxton and E. J. Pasierb,Trans. AIME 218, 794 (1960).

D. M. Poole and P. M. Thomas,J. Inst. Met. 90, 228 (1962).

C. S. Tedmon, Jr.,J. Electrochem. Soc. 114, 788 (1967).

D. P. Whittle, D. J. Evans, D. B. Scully, and G. C. Wood,Acta Metall. 15, 1421; 1747 (1967).

H. E. Evans, D. A. Hilton, and R. A. Holm,Oxid. Met. 10, 149 (1976).

J. C. Killeen, A. F. Smith and R. K. Wild,Corros. Sci. 16, 551 (1976).

B. D. Bastow, D. P. Whittle, and G. C. Wood,Oxid. Met. 12, 413 (1978).

T. Hodgkiess, G. C. Wood, D. P. Whittle, and B. D. Bastow,Oxid. Met. 12, 439 (1978).

G. C. Wood and D. P. Whittle,Corros. Sci. 4, 263; 293 (1964).

G. C. Wood, T. Hodgkiess, and D. P. Whittle,Corros. Sci. 6, 129 (1966).

G. C. Wood and D. P. Whittle,Corros. Sci. 7, 763 (1967).

M. M. P. Janssen,Metall. Trans. 4, 1623 (1973).

F. N. Rhines and J. S. Wolf,Metall. Trans. 1, 1701 (1970).

V. R. Howes,Metall. Trans. 8, 221 (1968);Metall. Trans. 1, 99 (1970).

V. R. Howes,J. Electrochem. Soc. 116, 1286 (1969).

C. S. Giggins, B. H. Kear, F. S. Pettit, and J. K. Tien,Met. Trans. 5, 1685 (1974).

B. W. Dunnington, F. H. Beck, and M. G. Fontana,Corrosion 8, 2t (1952).

G. B. Gibbs and R. Hales,Corros. Sci. 17, 487 (1977).

G. B. Gibbs,Oxid. Met. 16, 147 (1981).

B. Lustman,Trans. Metall. Soc. AIME,188, 995 (1950).

J. E. Antill and K. A. Peakall,J. Iron Steel Inst. London 1136 (November 1967).

C. E. Lowell, D. L. Deadmore, S. J. Grisaffe, and I. L. Drell, NASA TN D-6290, Lewis Research Center, Cleveland, Ohio, (April 1971).

H. Nagai, M. Okabayashi, and H. Mitani,Trans. Jpn. Inst. Met. 21, 341 (1980).

C. A. Barrett, A. S. Kahn, and C. E. Lowell,J. Electrochem. Soc. 128, 25 (1981).

P. Kofstad,Nonstoichiometry, Diffusion and Electrical Conductivity in Binary Metal Oxides (Wiley-Interscience, New York, 1972).

M. M. El-Aiat and F. A. Kröger,J. Am. Ceram. Soc. 65, 280 (1982).

J. C. Pivin, C. Roques-Carmes, P. Moulin, A. M. Huntz, and P. Lacombe,Mem. Sci. Rev. Metall. 75, 639 (1978).

E. Tsuzi,Metall. Trans. 11A, 1965 (1980).

M. Sakiyama, P. Tomaszewicz, and G. R. Wallwork,Oxid. Met. 13, 311 (1979).

J. C. Pivin, D. Delaunay, A. M. Huntz, and P. Lacombe,Corros. Sci. 20, 351 (1980).

J. Stringer,Metall. Rev. 11, 113 (1966).

H. Hindam and W. W. Smeltzer,J. Electrochem. Soc. 127, 1622 (1979).

H. Hindam and D. P. Whittle, in press.

H. Hindam and D. P. Whittle, in preparation.

C. A. Phalnikar, E. B. Evans, and W. M. Baldwin,J. Electrochem. Soc. 103, 429 (1956).

E. A. Gulbransen and K. F. Andrew,J. Electrochim. Soc. 104, 334 (1957).

W. C. Hagel,Trans. ASM 56, 583 (1963).

L. Cadiou and J. Paidassi,Mem. Sci. Rev. Metal. 66, 217 (1969).

C. S. Giggins and F. S. Pettit,Trans. Metall. Soc. AIME 245, 2495 (1969).

D. Caplan and M. Cohen,J. Electrochem. Soc. 108, 438 (1961).

H. C. Graham and H. H. Davis,J. Am. Ceram. Soc. 54, 89 (1971).

C. A. Stearns, F. J. Kohl, and G. C. Fryburg,J. Electrochem. Soc. 121, 945 (1974).

C. E. Lowell and W. A. Sanders,Oxid. Met. 5, 221 (1972).

D. R. Tenney, C. T. Young, and H. W. Herring,Metall. Trans. 5, 1001 (1974).

C. T. Young, D. R. Tenney, and H. W. Herring,Metall. Trans. 6A 2253 (1975).

G. C. Fryburg, F. J. Kohl, and C. A. Stearns,J. Electrochem. Soc. 121, 952 (1974).

Y. W. Kim and G. R. Belton,Metall. Trans. 5, 1811 (1974).

G. C. Fryburg, R. A. Miller, F. J. Kohl, and C. A. Stearns,J. Electrochem. Soc. 124, 1738 (1977).

G. M. Ecer and G. H. Meier,Oxid Met. 13, 119 (1979).

S. Espevik, R. A. Rapp, P. L. Daniel, and J. P. Hirth,Oxid. Met. 14, 85 (1980).

T. Hodgkiess, G. C. Wood, D. P. Whittle and B. D. Bastow,Oxid. Met. 14, 85 (1980).

P. Moulin, A. M. Huntz, and P. Lacombe,Acta Metall. 28, 745 (1980).

E. J. Felten,J. Electrochem. Soc. 108, 490 (1961).

J. M. Francis and W. H. Whitlow,Corros. Sci. 5, 701 (1965).

G. C. Wood and D. P. Whittle,Corros. Sci. 7, 763 (1967).

D. P. Whittle, M. E. El-Dahshan, and J. Stringer,Corros. Sci. 17, 879 (1977).

H. H. Davis, H. C. Graham, and I. A. Kvernes,Oxid. Met. 3, 431 (1971).

I. G. Wright, B. A. Wilcox, and R. I. Jaffee,Oxid. Met. 9, 275 (1975).

H. T. Michels,Metall. Trans. 7A, 379 (1976).

G. C. Wood and J. Boustead,Corros. Sci. 8, 719 (1968).

O. T. Goncel, D. P. Whittle, and J. Stringer,Oxid. Met. 15, 287 (1981).

H. Nagai, Y. Takebayashi, and H. Mitani,Metall. Trans. 12A, 435 (1981).

T. Amano, S. Yajima and Y. Saito,Trans. Jpn. Inst. Met. 20, 431 (1979).

F. S. Pettit,Trans. Metall. Soc. AIME 239, 1296 (1967).

C. S. Giggins and F. S. Pettit,J. Electrochem. Soc. 118, 1782 (1971).

A. S. Kahn, C. E. Lowell, and C. A. Barrett,J. Electrochem. Soc. 127, 671 (1980).

C. S. Wukusick and J. F. Collins,Mater. Res. Stand. 633 (1964).

C. Wagner,Z. Phys. Chem. B21, 25 (1933); inAtom-Movements, (ASM, Ohio, 1951)., p. 153.

W. W. Smeltzer and D. J. Young,Prog. Solid State Chem. 10, Part(1), 17 (1975).

J. F. Elliot and M. Bleiser, edsThermochemistry for Steel Making (Addison-Wesley, New York, 1960).

K. P. R. Reddy, Ph.D. thesis, Case Western Reserve University, Cleveland, Ohio (1979), quoted in Ref. 77.