Effects of the sterilisation method on the wear of UHMWPE acetabular cups tested in a hip joint simulator

Biomaterials - Tập 23 - Trang 1439-1446 - 2002
S. Affatato1, B. Bordini1, C. Fagnano2, P. Taddei2, A. Tinti2, A. Toni1,3
1Laboratorio di Tecnologia Medica, Istituti Ortopedici Rizzoli, Via di Barbiano 1/10, 40136 Bologna, Italy
2Dipartimento di Biochimica “G. Moruzzi”, Centro di Studio sulla Spettroscopia Raman, Sezione di Chimica e Propedeutica Biochimica, Università di Bologna, Italy
31° Divisione di Ortopedia e Traumatologia, Bologna, Italy

Tài liệu tham khảo

Collier, 1996, Overview of polyethylene as a bearing material, Clin Orthop Relat Res, 333, 76, 10.1097/00003086-199612000-00007

Lewis, 1997, Polyethylene wear in total hip and knee arthroplasties, J Biomed Mater Res, 38, 55, 10.1002/(SICI)1097-4636(199721)38:1<55::AID-JBM8>3.0.CO;2-G

Hirakawa, 1996, Comparison and quantitation of wear debris of failed total hip and total knee arthroplasty, J Biomed Mater Res, 31, 257, 10.1002/(SICI)1097-4636(199606)31:2<257::AID-JBM13>3.0.CO;2-I

Kusaba, 1997, Femoral component wear in retrieved hip prostheses, J Bone Jt Surg Br, 79, 331, 10.1302/0301-620X.79B2.7217

Schmalzried, 1992, Periprosthetic bone loss in total hip arthroplasty. Polyethylene wear debris and the concept of the effective joint space, J Bone Jt Surg Am, 74, 849, 10.2106/00004623-199274060-00006

Besong, 1999, The influence of lubricant on the morphology of ultra-high molecular weight polyethylene wear debris generated in laboratory tests, Proc Inst Mech Eng, 213, 155, 10.1243/0954411991534870

McKellop, 1999, Effect of molecular weight, calcium stearate, and sterilization methods on the wear of uhmwpe acetabular cups in a hip joint simulator, J Orthop Res, 17, 329, 10.1002/jor.1100170306

Edidin, 1999, Plasticity-induced damage layer is a precursor to wear in radiation-cross-linked uhmwpe acetabular components for total hip replacement, J Arthroplasty, 14, 616, 10.1016/S0883-5403(99)90086-4

Costa, 1998, In vivo UHMWPE biodegradation of retrieved prosthesis, Biomaterials, 19, 1371, 10.1016/S0142-9612(98)00013-1

Bargmann, 1999, Current sterilization and packaging methods for polyethylene, Clin Orthop Relat Res, 369, 49, 10.1097/00003086-199912000-00006

Saum KA. Oxidation vs. depth and time for polyethylene—gamma sterilized in air. Trans ORS 1994;130–74.

Rimnac CM, Klein RW, Burstein AH, Wright TM. In vitro chemical and mechanical degradation of UHMWPE: three month results. 19th meeting of the Society For Biomaterials, 1993.

Rimnac, 1994, Post-irradiation aging of ultra-high molecular weight polyethylene, J Bone Jt Surg Am, 76, 1052, 10.2106/00004623-199407000-00014

Grood, 1982, Analysis of retrieved implants, J Biomed Mater Res, 16, 399, 10.1002/jbm.820160408

Eyerer, 1984, Property changes of UHMW polyethylene hip cup endoprostheses during implantation, J Biomed Mater Res, 18, 1137, 10.1002/jbm.820180915

Eyerer, 1987, Characterization of UHMWPE hip cups run on joint simulators, J Biomed Mater Res, 21, 275, 10.1002/jbm.820210302

Li S, Saum KA, Collier JP, Kasprazak D. Oxidation of UHMWPE over long time periods Trans Soc Biomater 1994; 425.

Ries, 1996, Fatigue strength of polyethylene after sterilization by gamma irradiation or ethylene oxide, Clin Orthop Relat Res, 333, 87, 10.1097/00003086-199612000-00008

Kurtz, 1999, Advances in the processing sterilization, and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplasty, Biomaterials, 20, 1659, 10.1016/S0142-9612(99)00053-8

Sun DC, Wang A, Stark C, Dumbleton JH. The concept of stabilization in UHMWPE. Transactions of the Fifth World Biomaterials Congress, vol. 1, 1996. p. 195.

Premnath V, Merrill EW, Jasty M, Harris WH. Melt-irradiated UHMWPE for total hip replacements: synthesis and properties. Transactions of the 43rd Orthopeadic Research Society, vol. 22, 1997. p. 91.

White, 1996, Effects of sterilization on wear in total knee arthroplasty, Clin Orthop Relat Res, 331, 164, 10.1097/00003086-199610000-00023

Boggan RS, Trieu HH, Richelsoph KC, Paxson RD, Carroll MC. The effect of radiation sterilization on the physical and mechanical properties of UHMWPE. The 19th Annual Meeting of the Society for Biomaterials, 1993. p. 329.

Weaver KD, Sauer WL, Beals NB. Sterilisation induced effect on UHMWPE oxidation and fatigue strength. Proceedings of the 21st Annual Meeting of the Society of Biomaterials, San Francisco, 1995. p. 129.

Shen, 1999, Potential errors in FTIR measurement of oxidation in ultrahigh molecular weight polyethylene implants, J Biomed Mater Res, 48, 203, 10.1002/(SICI)1097-4636(1999)48:3<203::AID-JBM1>3.0.CO;2-R

Witkiewicz, 1996, A differential scanning calorimetry study of retrieved orthopedic implants made of ultrahigh molecular weight polyethylene, J Biomed Mater Res, 33, 73, 10.1002/(SICI)1097-4636(199622)33:2<73::AID-JBM3>3.0.CO;2-I

Saikko, 1993, Wear of the polyethylene acetabular cup, Acta Orthop Scand, 64, 391, 10.3109/17453679308993653

Bertoluzza, 2000, Micro-Raman spectroscopy for the crystallinity characterization of UHMWPE hip cups run on joint simulators, J Mol Struct, 521, 89, 10.1016/S0022-2860(99)00427-5

Rull, 1993, Estimation of crystallinity in Polyethylene by Raman Spectroscopy, J Raman Spectrosc, 24, 545, 10.1002/jrs.1250240813

Williams, 1995, Use of Micro Raman spectroscopy for the quantitative determination of polyethylene density using partial least-squares calibration, J Raman Spectrosc, 26, 427, 10.1002/jrs.1250260606

Affatato, 1999, Mixed oxides prosthetic ceramic ball heads. Part 1, Biomaterials, 20, 971, 10.1016/S0142-9612(98)00253-1

Affatato, 1999, Mixed oxides prosthetic ceramic ball heads. Part 2, Biomaterials, 20, 1925, 10.1016/S0142-9612(99)00093-9

Affatato, 2001, Mixed oxides prosthetic ceramic ball heads. Part 3, Biomaterials, 22, 717, 10.1016/S0142-9612(00)00235-0

Painter, 1982

Chapiro, 1962

Bhateja, 1989, Radiation induced crystallinity changes in linear polyethylene, Polym J, 21, 739, 10.1295/polymj.21.739

Narkis, 1987, Structure and tensile behavior of irradiation- and peroxide-crosslinked polyethylenes, J Macromol Sci Phys, B26, 37, 10.1080/00222348708248057

Deng, 1995, Effects of gamma-irradiation, gas environments and postirradiation aging on ultrahigh molecular-weight poluethylene, J Appl Polym Sci, 58, 2111, 10.1002/app.1995.070581123

McKellop, 1999, Development of an extremely wear-resistant ultra high molecular weight polyethylene for total hip replacements, J Orthop Res, 17, 157, 10.1002/jor.1100170203

Chenery, 1997, Detection of peroxy species in ultra-high-molecular-weight polyethylene by Raman spectroscopy, Biomaterials, 18, 415, 10.1016/S0142-9612(96)00149-4

Daly, 1998, Subsurface oxidation of polyethylene, J Biomed Mater Res, 42, 523, 10.1002/(SICI)1097-4636(19981215)42:4<523::AID-JBM7>3.0.CO;2-1

Wang A, Sun DC, Stark C, Dumbleton JH. Effects of sterilization methods on the wear of ultra-high-molecular-weight-polyethylene acetabular cups. Transactions of the Fifth World Biomaterials Congress, Toronto, 1996. p. 198.

Sommerich, 1996, The effects of sterilization on contact area and wear rate of UHMWPE, Trans Orthop Res Soc, 21, 486

Polineni, 1997, Effects of sterilization methods on the wear behavior of UHMWPE acetabular cups, Trans Orthop Res Soc, 22, 779

Klapperich, 2000, Fluid sorption of orthopedic grade ultrahigh molecular weight polyethylene in a serum environment is affected by the surface area and sterilization method, J Biomed Mater Res, 53, 73, 10.1002/(SICI)1097-4636(2000)53:1<73::AID-JBM10>3.0.CO;2-A