Effects of adhesive modulus and curing conditions on curing behavior of silicate based ceramic coatings on carbon fiber reinforced resin matrix composites

Ceramics International - Tập 47 - Trang 11089-11096 - 2021
Meimei Ji1,2, Shizhen Zhu1,2, Zhuang Ma1,2, Hezhang Li1
1School of Materials Science and Engineering, Beijing Institute of Technology, Beijing 100081, China
2National Key Laboratory of Science and Technology on Materials under Shock and Impact, Beijing, 100081, China

Tài liệu tham khảo

Zhong, 2016, The impact of adhesive resin solution on carbon fibers cloth and jute-reinforced epoxy resin matrix composites, J. Text. Inst., 107, 1264, 10.1080/00405000.2015.1100818 Jian, 2007, Effects of polycarbosilane infiltration processes on the microstructure and mechanical properties of 3D-Cf/SiC composites, Ceram. Int., 33, 905, 10.1016/j.ceramint.2006.02.005 Krenkel, 2005, C/C-SiC composites for space applications and advanced friction systems, Mater. Sci. Eng., 412, 177, 10.1016/j.msea.2005.08.204 Glime, 1995, Oxidation of carbon fibers and films in ceramic matrix composites: a weak link process, Carbon, 33, 1053, 10.1016/0008-6223(95)00034-B Fan, 2018, Design and optimization of oxidation resistant coating for C/C aircraft brake materials, Ceram. Int., 44, 175, 10.1016/j.ceramint.2017.09.156 Bartuli, 2002, Plasma spray deposition and high temperature characterization of ZrB2-SiC protective coatings, Surf. Coating. Technol., 155, 260, 10.1016/S0257-8972(02)00058-0 Niessen, 2011, Plasma spray-PVD: a new thermal spray process to deposit out of the vapor phase, J. Therm. Spray Technol., 20, 736, 10.1007/s11666-011-9654-9 Goral, 2017, The influence of process parameters on structure of ceramic coatings deposited by PS-PVD method, Solid State Phenom., 267, 243, 10.4028/www.scientific.net/SSP.267.243 Masanta, 2009, Development of a hard nano-structured multi-component ceramic coating by laser cladding, Mater. Sci. Eng., 508, 134, 10.1016/j.msea.2008.12.031 Wang, 2014, Microstructural characterization of Al2O3-13wt.% TiO2 ceramic coatings prepared by squash presetting laser cladding on GH4169 superalloy, Surf. Coating. Technol., 254, 195, 10.1016/j.surfcoat.2014.06.011 Yuan, 2007, Comparison of femtosecond and nanosecond laser-induced damage in HfO2 single-layer film and HfO2-SiO2 high reflector, J. Opt. Soc. Am. B, 24, 538, 10.1364/JOSAB.24.000538 Goto, 2005, Thermal barrier coatings deposited by laser CVD, Surf. Coating. Technol., 198, 367, 10.1016/j.surfcoat.2004.10.084 Pietrzyk, 2018, Low friction nanocomposite aluminum oxide/MoS2 coatings prepared by sol-gel method, Ceram. Int., 44, 8534, 10.1016/j.ceramint.2018.02.055 Liu, 2019, Development of T-ZnOw@Al2O3-incorporated low-temperature curing aluminium phosphate coating on Ti–6Al–4V alloy, Ceram. Int., 45, 18406, 10.1016/j.ceramint.2019.06.056 Xiong, 2005, The oxidation behavior and mechanical performance of Ti60 alloy with enamel coating, Surf. Coating. Technol., 190, 195, 10.1016/j.surfcoat.2004.09.005 Ramasamy, 2010, EBC development for hot-pressed Y2O3/Al2O3 doped silicon nitride ceramics, Mater. Sci. Eng., 527, 5492, 10.1016/j.msea.2010.05.067 Han, 2019, A novel phosphate-ceramic coating for high temperature oxidation resistance of Ti65 alloys, Ceram. Int., 45, 23895, 10.1016/j.ceramint.2019.06.218 Kim, 2003, Fabrication and properties of thermal insulating glass fiber reinforced composites from low temperature curable polyphosphate inorganic polymers, Compos. Sci. Technol., 63, 493, 10.1016/S0266-3538(02)00229-4 Han, 2003, Studies on curing chemistry of aluminum-chromium-phosphates as low temperature curable binders, J. Sol. Gel Sci. Technol., 26, 223, 10.1023/A:1020799015594 Halasz, 2007, Monitoring the structure of water soluble silicates, Catal. Today, 126, 196, 10.1016/j.cattod.2006.09.032 Lucas, 2011, Interactions between silica sand and sodium silicate solution during consolidation process, J. Non-Cryst. Solids, 357, 1310, 10.1016/j.jnoncrysol.2010.12.016 Kouassi, 2011, Consolidation mechanism of materials obtained from sodium silicate solution and silica-based aggregates, J. Non-Cryst. Solids, 357, 3013, 10.1016/j.jnoncrysol.2011.04.006 Hong, 2007, Development of Cr-free aluminum phosphate binders and their composite applications, Compos. Sci. Technol., 67, 1195, 10.1016/j.compscitech.2006.05.025 Chen, 2013, High-temperature resistance performance of an inorganic adhesive for concrete structures strengthened with CFRP sheets, J. Wuhan Univ. Technol., 28, 950, 10.1007/s11595-013-0799-x Shen, 2011, The oxidation and oxygen permeation resistance of quartz particle-reinforced aluminosilicate glass coating on titanium alloy, J. Am. Ceram. Soc., 94, 2436, 10.1111/j.1551-2916.2011.04587.x Ma, 2015 Liu, 2019, Influence of curing temperature on corrosion protection property of chemically bonded phosphate ceramic coatings with nano-titanium dioxide reinforcement, Ceram. Int., 45, 1595, 10.1016/j.ceramint.2018.10.034 Phanasgaonkar, 2009, Influence of curing temperature, silica nanoparticles-and cerium on surface morphology and corrosion behaviour of hybrid silane coatings on mild steel, Surf. Coating. Technol., 203, 2260, 10.1016/j.surfcoat.2009.02.020 Watanabe, 2007, A large, freestanding, 20 nm thick nanomembrane based on an epoxy resin, Adv. Mater., 19, 909, 10.1002/adma.200601630 Bera, 2016, Water-based & eco-friendly epoxy-silane hybrid coating for enhanced corrosion protection & adhesion on galvanized steel, Prog. Org. Coating, 101, 24, 10.1016/j.porgcoat.2016.07.010 Liu, 2019, Diamine-functional bisphthalonitrile: synthesis, characterization and its application in curing epoxy resin, Eur. Polym. J., 121, 109304, 10.1016/j.eurpolymj.2019.109304 Wu, 2006, Synthesis and characterization of polydimethylsiloxane-cured organically modified silicate hybrid coatings, Polym. Degrad. Stabil., 91, 2917, 10.1016/j.polymdegradstab.2006.08.016