Effects of Dental Adhesive Cement and Surface Treatment on Bond Strength and Leakage of Zirconium Oxide Ceramics

Dental Materials Journal - Tập 27 Số 2 - Trang 159-171 - 2008
Makoto TSUKAKOSHI1, Akikazu Shinya1,2, Harunori Gomi1, Lippo Lassila2, Pekka K. Vallittu2, Akiyoshi Shinya1
1Department of Crown and Bridge, School of Life Dentistry at Tokyo, The Nippon Dental University
2Department of Prosthetic Dentistry and Biomaterials Science, Institute of Dentistry, University of Turku

Tóm tắt

Từ khóa


Tài liệu tham khảo

10.1016/S0142-9612(98)00010-6

2) Akagawa Y, Ichikawa Y, Nikai H, Tsuru H. Interface histology of unloaded and early loaded partially stabilized zirconia endosseous implant in initial bone healing. J Prosthet Dent 1993; 69: 599-604.

3) Rizkalla AS, Jones DW. Mechanical properties of commercial high strength ceramic core materials. Dent Mater 2004; 20: 207-212.

4) Guazzato M, Albakry M, Ringer SP, Swain MV. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I: Pressable and alumina glass-infiltrated ceramics. Dent Mater 2004; 20: 441-448.

10.1016/j.dental.2003.05.002

6) Sundh A, Molin M, Sjögren G. Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing. Dent Mater 2005; 21: 476-482.

7) Sundh A, Sjögren G. Fracture resistance of all-ceramic zirconia bridges with differing phase stabilizers and quality of sintering. Dent Mater 2006; 22: 778-784.

10.1016/S0022-3913(99)70103-4

9) Odman P, Andersson B. Procera AllCeram Crowns followed for 5 to 10.5 years: A prospective clinical study. Int J Prosthodont 2001; 14: 504-509.

10) Filser F, Kocher P, Weibel F, Luthy H, Scharer P, Gauckler L. Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM). Int J Computerized Dentistry 2001; 4: 89-106.

11) Matsuda T, Shin-ya A, Tomita S, Shin-ya A, Mitobe C, Hasebe S, Hioki M. A clinical report and a small study of fitness on Procera<SUP>&reg;</SUP> AllCeram crown. J J Prosthodont Soc 2004; 48: 543-548.

10.1016/S0109-5641(98)00011-6

13) Derand T, Molin M, Kvam K. Bond strength of composite luting cement to zirconia ceramic surfaces. Dent Mater 2005; 21: 1158-1162.

10.1002/jbm.820160307

15) Nemoto M. Study on the marginal leakage of all ceramic crowns luted with resin cement <I>in vitro</I>: Evaluation after cyclic load. J Nihon Univ Sch Dent 2001; 75: 429-436.

16) Nishiyama N, Komatsu K, Teshima H, Nemoto K, Horie K. Study on a silane coupling agent&mdash;Hydrolytic stability of di-methacrylate silane. J J Dent Mater 1993; 12: 169-173.

17) Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhesive Dent 2000; 2: 139-147.

MATSUMURA H, 1987, 6, 135, 10.4012/dmj.6.135

19) Nihei T, Kurata S, Kondo Y, Umemoto K, Yoshino N, Teranaka T. Effect of silane coupling agents with a fluoroalkyl and a methacryloyl groups in a molecule. Treatment of silane mixture of the silane&frasl;3-meth-acryloxypropyltrimethoxsilane. J J Dent Mater 2002; 21: 104-115.

20) Hinokiyama N, Hagiwara Y, Muramatsu T, Kawamoto Y, Tanaka S, Koizumi M, Igarashi T. A study on ceramic abutment influence of tribochemical coating on bond strength. J J Prosthodont Soc 2001; 45: 737-746.

TAKAKUWA MASANOBU, 1998, 86, 92, 10.1007/BF03039149

22) Uo M, Sjogren G, Sundh A, Watari F, Bergman M, Lerner U. Cytotoxicity and bonding property of dental ceramics. Dent Mater 2003; 19: 487-492.

23) Kajiwara H, Abiru F, Minezaki R, Kurashige N, Murahara S, Ito S. Surface treatment of zirconia ceramic for adhesion to phosphoric ester resin cement. J J Prosthodont Soc 2003; 47: 153.

24) Sato H, Yamashita D, Ban S. Structural change of zirconia surfaces by sandblasting and heat treatment. J J Dent Mater 2006; 25: 338.

25) Nakamura K, Oka K. Testing methods for bond strength of dental adhesive resins. J J Dent Mater 1992; 11: 101-114.

26) Japan Industrial Standards. JIS T6602-1993. Dental zinc phosphate cement.

27) Van Meerbeek B, De Munck J, Yoshida Y, Inoue S, Vargas M, Vijay P, <I>et al</I>. Adhesion to enamel and dentin: current status and future challenges. Oper Dent 2003; 28: 215-235.

MEERBEEK BART VAN, 2005, 24, 1, 10.4012/dmj.24.1

29) Hioki M, Nakahara R, Nakasone Y. Shear bond strength of a resin-modified glass ionomer cement for orthodontic treatment&mdash;Effects of the orthodontic bracket configuration and the tooth enamel shape. J J Dent Mater 2005; 24: 223-230.

UO MOTOHIRO, 2006, 25, 626, 10.4012/dmj.25.626

31) Kuraji N, Kojo K, Shinya A, Yokozuka S. Fractographical and stress analysis of bonding surface in varieties of bond strength testing. J J Prosthodont Soc 1998; 42: 135-146.

32) Fukai K, Nishiyama N. Study on a silane coupling agent&mdash;Influence of an acid on the adsorption and hydrolytic stability of the silane at the interface. J J Dent Mater 1992; 11: 875-880.

33) Matinlinna JP, Heikkinen T, Ozcan M, Lassila LV, Vallittu PK. Evaluation of resin adhesion to zirconia ceramic using some organosilanes. Dent Mater 2006; 22: 824-831.

34) Piwowarczyk A, Lauer HC, Sorensen JA. The shear bond strength between luting cements and zirconia ceramics after two pre-treatments. Oper Dent 2005; 30: 382-388.

35) Ernst CP, Cohnen U, Stender E, Willershausen B. <I>In vitro</I> retentive strength of zirconium oxide ceramic crowns using different luting agents. J Prosthet Dent 2005; 93: 551-558.