Deformation and recrystallization behavior of a coarse-grain, nickel-base superalloy Udimet720Li ingot material

Materials Characterization - Tập 107 - Trang 398-410 - 2015
Qiangliang Yu1,2, Zhihao Yao2, Jianxin Dong2
1Beijing Institute of Aeronautical Materials, Beijing, 100095, PR China
2School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, PR China

Tóm tắt

Từ khóa


Tài liệu tham khảo

Medeiros, 2000, Mater. Sci. Eng. A, 293, 198, 10.1016/S0921-5093(00)01053-4

Tian, 2004, Mater. Sci. Eng. A, 367, 198, 10.1016/j.msea.2003.10.226

Wang, 2009, J. Alloys Compd., 474, 341, 10.1016/j.jallcom.2008.06.079

Beladi, 2009, Metall. Mater. Trans. A, 40, 1175, 10.1007/s11661-009-9799-z

Wang, 2015, J. Alloys Compd., 623, 69, 10.1016/j.jallcom.2014.10.034

Dehghan-Manshadi, 2008, Mater. Sci. Eng. A, 485, 664, 10.1016/j.msea.2007.08.026

McQueen, 2004, J. Alloys Compd., 378, 35, 10.1016/j.jallcom.2003.10.067

Ning, 2010, Mater. Sci. Eng. A, 527, 6968, 10.1016/j.msea.2010.07.018

Thomas, 2004, 959

Mao, 2000, J. Mater. Eng. Perform., 9, 204, 10.1361/105994900770346169

Hyzak, 1992, 93

Lindsley, 2000, 93

Monajati, 2005, Scr. Mater., 52, 771, 10.1016/j.scriptamat.2004.12.006

Daymond, 2007, Acta Mater., 55, 3089, 10.1016/j.actamat.2007.01.013

Zhao, 2010, 271

Semiatin, 2004, Metall. Mater. Trans. A, 35, 679, 10.1007/s11661-004-0379-y

Sellars, 1966, Acta Metall., 14, 1136, 10.1016/0001-6160(66)90207-0

Kashyap, 2000, Scr. Mater., 43, 429, 10.1016/S1359-6462(00)00453-X

Shen, 1995, Metall. Mater. Trans. A, 26, 1795, 10.1007/BF02670767

Bruni, 2002, J. Mater. Process. Technol., 125–126, 242, 10.1016/S0924-0136(02)00302-3

Courtney, 1990

Monajati, 2005, Metall. Mater. Trans. A, 36, 895, 10.1007/s11661-005-0284-z

Briottet, 1996, Acta Mater., 44, 1665, 10.1016/1359-6454(95)00257-X

Blaz, 1983, Met. Sci., 17, 609, 10.1179/030634583790420448

Humphreys, 2004

Miura, 2003, Scr. Mater., 48, 1501, 10.1016/S1359-6462(03)00053-8

Bay, 1992, Acta Metall., 40, 205, 10.1016/0956-7151(92)90296-Q

Jorge-Badiola, 2005, Mater. Sci. Eng. A, 394, 445, 10.1016/j.msea.2004.11.049

Doherty, 1982, Met. Sci., 16, 1, 10.1179/030634582790427019

Nes, 1985, Acta Metall., 33, 11, 10.1016/0001-6160(85)90214-7

Randle, 1986, Acta Metall., 34, 891, 10.1016/0001-6160(86)90062-3

Kim, 2001, Mater. Sci. Eng. A, 311, 108, 10.1016/S0921-5093(01)00917-0

Miura, 2004, Scr. Mater., 50, 65, 10.1016/j.scriptamat.2003.09.035

Wang, 2000, Mater. Sci. Eng. A, 290, 180, 10.1016/S0921-5093(00)00915-1

Beladi, 2010, Acta Metall., 58, 3531

Wang, 2002, Scr. Mater., 46, 875, 10.1016/S1359-6462(02)00072-6

Brünger, 1998, Scr. Mater., 38, 1843, 10.1016/S1359-6462(98)00124-9

Jones, 2003, Acta Mater., 51, 2149, 10.1016/S1359-6454(03)00002-8

Gourdet, 2000, Mater. Sci. Eng. A, 283, 274, 10.1016/S0921-5093(00)00733-4

Pande, 1990, Metall. Mater. Trans. A, 21, 2891, 10.1007/BF02647209

Belyakov, 1998, Mater. Sci. Eng. A, 255, 139, 10.1016/S0921-5093(98)00784-9

Randle, 1996, Philos. Mag. A, 73, 265, 10.1080/01418619608244382

Ponge, 1998, Acta Mater., 46, 69, 10.1016/S1359-6454(97)00233-4

Kaibyshev, 2001, 949