Characterization of chitin, chitosan and their carboxymethyl derivatives by differential scanning calorimetry

Carbohydrate Polymers - Tập 49 Số 2 - Trang 185-193 - 2002
Farooqahmed S. Kittur1, K.V. Harish Prashanth1, K. Udaya Sankar2, Rudrapatnam N. Tharanathan1
1Department of Biochemistry and Nutrition, Central Food Technological Research Institute, Mysore 570013, India
2Department of Food Engineering, Central Food Technological Research Institute, Mysore 570013, India

Tóm tắt

Từ khóa


Tài liệu tham khảo

Aiba, 1986, International Journal of Biological Macromolecules, 8, 173, 10.1016/0141-8130(86)90022-X

Appelqvist, 1993, Carbohydrate Polymers, 20, 291, 10.1016/0144-8617(93)90102-A

Berens, 1982, Macromolecules, 15, 756, 10.1021/ma00231a015

Biliaderis, 1982, Journal of Agricultural and Food Chemistry, 30, 925, 10.1021/jf00113a029

Chatterjee, 1972, TAPPI, 55, 111

Gidley, 1988, Journal of American Chemical Society, 110, 3820, 10.1021/ja00220a016

Hayes E. R. (1986). USPatent No. 4,619,995.

Hirano, 1989, Agricultural and Biological Chemistry, 53, 3065, 10.1271/bbb1961.53.3065

Hirano, 1992, Carbohydrate Research, 225, 175, 10.1016/0008-6215(92)80052-3

Hodge, 1982, Macromolecules, 15, 762, 10.1021/ma00231a016

Jiang, 1999, Journal of Applied Polymer Science, 61, 1163, 10.1002/(SICI)1097-4628(19960815)61:7<1163::AID-APP12>3.0.CO;2-Z

Kacurakova, 1998, Journal of the Science of Food and Agriculture, 77, 38, 10.1002/(SICI)1097-0010(199805)77:1<38::AID-JSFA999>3.0.CO;2-5

Kendra, 1989, Physiology and Molecular Plant Pathology, 35, 215, 10.1016/0885-5765(89)90052-0

Livings, 1997, Carbohydrate Polymers, 34, 347, 10.1016/S0144-8617(97)00126-4

Miya, 1980, International Journal of Biological Macromolecules, 2, 323, 10.1016/0141-8130(80)90056-2

Miyashita, 1997, Carbohydrate Polymers, 34, 221, 10.1016/S0144-8617(97)00110-0

Moore, 1980, International Journal of Biological Macromolecules, 2, 115, 10.1016/0141-8130(80)90040-9

Muzzarelli, 1982, Carbohydrate Research, 107, 199, 10.1016/S0008-6215(00)80539-X

Nahalka, 1998, Biotechnology Letters, 20, 841, 10.1023/A:1005307408135

Niola, 1993, Carbohydrate Research, 238, 1, 10.1016/0008-6215(93)87001-9

Nishimura, 1986, Carbohydrate Research, 146, 251, 10.1016/0008-6215(86)85044-3

Ottoy, 1996, Carbohydrate Polymers, 29, 17, 10.1016/0144-8617(95)00154-9

Pangburn, 1984, 3

Phillips, 1996, Food Hydrocolloids, 10, 11, 10.1016/S0268-005X(96)80048-8

Pizzoli, 1991, Carbohydrate Research, 222, 205, 10.1016/0008-6215(91)89018-B

Rinaudo, 1993, International Journal of Biological Macromolecules, 15, 281, 10.1016/0141-8130(93)90027-J

Sandford, 1989

Sato, 1998, Analytical Chemistry, 70, 7, 10.1021/ac9706685

Struszezyk, 1987, Journal of Applied Polymer Science, 33, 177, 10.1002/app.1987.070330115

Suzuki S., Watanabe T., Mikami T. & Suzuki M. (1990). Proceedings of the 5th International Conference on Chitin and Chitosan, USA, pp. 96–105.

Tokura, 1983, Polymer Journal (Tokyo), 15, 485, 10.1295/polymj.15.485

Varum, 1991, Carbohydrate Research, 217, 19, 10.1016/0008-6215(91)84113-S

Yunlin, 1998, Carbohydrate Polymers, 36, 61, 10.1016/S0144-8617(97)00251-8