Selected corrosion of X80 pipeline steel welded joints induced by Desulfovibrio desulfuricans

Corrosion Science - Tập 202 - Trang 110313 - 2022
Qin Wang1, Xiaobao Zhou1, Qiao Ma1, Tangqing Wu1, Meng Liu2, Minghua Zhang1, Zhi Li1, Fucheng Yin1
1Key Laboratory of Materials Design and Preparation Technology of Hunan Province, School of Materials Science and Engineering, Xiangtan University, Xiangtan 411105, China
2Pipeline Engineering Research Center, Pipe China Science and Technology Institute, Langfang 065000, China

Tài liệu tham khảo

Zhou, 2020, A novel Cu-bearing high-entropy alloy with significant antibacterial behavior against corrosive marine biofilms, J. Mater. Sci. Technol., 46, 201, 10.1016/j.jmst.2020.01.039

Tang, 2021, Stainless steel corrosion via direct iron-to-microbe electron transfer by Geobacter species, ISME J., 15, 3084, 10.1038/s41396-021-00990-2

Xu, 2017, Accelerated corrosion of 2205 duplex stainless steel caused by marine aerobic Pseudomonas aeruginosa biofilm, Bioelectrochemistry, 113, 1, 10.1016/j.bioelechem.2016.08.001

Wei, 2021, Effect of sulfate-reducing bacteria on corrosion of X80 pipeline steel under disbonded coating in a red soil solution, J. Mater. Sci. Technol., 87, 1, 10.1016/j.jmst.2020.12.076

Ilhan-Sungur, 2007, Microbial corrosion of galvanized steel by a freshwater strain of sulphate reducing bacteria (Desulfovibrio sp.), Corros. Sci., 49, 1097, 10.1016/j.corsci.2006.05.050

Xu, 2016, Mechanistic modeling of biocorrosion caused by biofilms of sulfate reducing bacteria and acid producing bacteria, Bioelectrochemistry, 110, 52, 10.1016/j.bioelechem.2016.03.003

Zhou, 2021, Effects of non-viable microbial film on corrosion of pipeline steel in soil environment, Corros. Commun., 3, 23, 10.1016/j.corcom.2021.11.003

Xu, 2011, The effects of sulfate reducing bacteria on corrosion of carbon steel Q235 under simulated disbonded coating by using electrochemical impedance spectroscopy, Corros. Sci., 53, 1554, 10.1016/j.corsci.2011.01.037

Wu, 2014, Microbiological corrosion of pipeline steel under yield stress in soil environment, Corros. Sci., 88, 291, 10.1016/j.corsci.2014.07.046

Wu, 2019, Stress corrosion of pipeline steel under disbonded coating in a SRB-containing environment, Corros. Sci., 157, 518, 10.1016/j.corsci.2019.06.026

Anandkumar, 2016, Corrosion characteristics of sulfate-reducing bacteria (SRB) and the role of molecular biology in SRB studies: an overview, Corros. Rev., 34, 41, 10.1515/corrrev-2015-0055

Li, 2018, Reconstruction of X80 pipeline steel welded joints and corrosion behavior in NACE solution, J. China Univ. Pet. Ed. Nat. Sci., 42, 153

Antony, 2010, Role of microstructure on corrosion of duplex stainless steel in presence of bacterial activity, Corros. Sci., 52, 1404, 10.1016/j.corsci.2009.12.003

Liu, 2014, Rapid MIC attack on 2205 duplex stainless steel pipe in a yacht, Eng. Fail. Anal., 42, 109, 10.1016/j.engfailanal.2014.04.001

Chen, 2018, Effects of sulfate-reducing bacteria on marine corrosion of weld joints of EH40, Equip. Environ. Eng., 15, 51

Sreekumari, 2001, Bacterial attachment to stainless steel welds: Significance of substratum microstructure, Biofouling, 17, 303, 10.1080/08927010109378490

Mohammadi, 2012, Corrosion of simulated weld HAZ of API X-80 pipeline steel, Corros. Sci., 63, 323, 10.1016/j.corsci.2012.06.014

Cao, 2020, Corrosion behavior of the weld joint of X80 pipeline steel in an acidic red soil, Mater. Res. Express, 7, 10.1088/2053-1591/ab71c8

Brug, 1984, The analysis of electrode impedances complicated by the presence of a constant phace element, J. Electroanal. Chem. Interfacial Electrochem., 176, 275, 10.1016/S0022-0728(84)80324-1

Liao, 2020, Physical properties obtained from measurement model analysis of impedance measurements, Electrochim. Acta, 354, 10.1016/j.electacta.2020.136747

Orazem, 2013, Dielectric properties of materials showing constant-phase-element (CPE) impedance response, J. Electrochem. Soc., 160, C215, 10.1149/2.033306jes

Hirschorn, 2010, Determination of effective capacitance and film thickness from constant-phase-element parameters, Electrochim. Acta, 55, 6218, 10.1016/j.electacta.2009.10.065

Javed, 2013, The effect of metal microstructure on the initial attachment of Escherichia coli to 1010 carbon steel, Biofouling, 29, 939, 10.1080/08927014.2013.820826