Micro differential scanning calorimetry and micro hot table method for quantifying deterioration of historical leather
Tóm tắt
The aim of this study was to advance the current understanding on the mechanism of deterioration of historical vegetable tanned leathers and establish new criteria for quantifying their deterioration using micro differential scanning calorimetry (micro DSC) and micro hot table (MHT) method. Ten historical leather objects were investigated to this purpose. The calorimetric indices of macromolecular change identified for fibrous collagen provided quantitative results on the bulk material and deconvolution of DSC denaturation peaks revealed the dynamics of deterioration in historical leather. The results brought clear evidence that long-term natural ageing of leather induces the destabilization of chemically modified collagen thereby promoting its partial de-tanning and allowing micro-unfolding of chemically unmodified collagen. As deterioration continues toward the extreme, collagen molecules become highly unstable allowing for gelatinisation and irreversible denaturation. It is thus explained the coexistence of collagen populations with distinct thermal stability in historical leather. They are grouped in three main structural domains, namely “leather-like”, “parchment-like” and “gelatine-like”, whose mass percentages determines leather stability against further natural ageing and deterioration. As a result of the MHT and micro DSC parameters correlation, a more comprehensive set of criteria, including Tf and Tl values, as well ∆C and ∆T intervals’ lengths, was introduced for better interpreting the shrinking activity of collagen in historical vegetable-tanned leathers and open thus the way for the highly sought in situ evaluation of leather artefacts.
Tài liệu tham khảo
Forbes RJ. Leather in antiquity. Studies in ancient technology, vol. 5. 1st ed. Leiden: Brill Publishers; 1957. p. 1–77.
Haslam E. Vegetable tannage: where do the tannins go? J Soc Leather Technol Chem. 1997;81:45–51.
Hassan RRA. A preliminary study on using line seed oil emulsion in dressing archaeological leather. J Cult Herit. 2016;21:786–95.
Hassan RRA, Ali MF, Fahmy AA. Use of SEM, FTIR and amino acid analysis methods to assess the damage of some historical leather bindings from the XIXth century, stored in National Archive, Cairo. Int J Conserv Sci. 2018;9(1):127–36.
Leather Thomson R. In: May E, Jones M, editors. Conservation science: heritage materials. Cambridge: The Royal Society of Chemistry; 2006. p. 67.
Falcão L, Araújo MEM. Tannins characterisation in new and historic vegetable tanned leathers fibres by spot tests. J Cult Herit. 2011;12(2):149–56.
Bate-Smith EC, Swain T. Flavonoid compounds. In: Mason HS, Florkin AM, editors. Comparative biochemistry. New York: Academic Press; 1962. p. 755–809.
Khanbabaee K, van Ree T. Tannins: classification and definition. Nat Prod Rep. 2001;18:641–9.
Covington AD. Modern tanning chemistry. Chem Soc Rev. 1997;26:111–26.
Weir CE. Rate of shrinkage of tendon collagen—heat, entropy, and free energy of activation of the shrinkage of untreated tendon. Effect of acid, salt, pickle, and tannage on the activation of tendon collagen. J Am Leather Chem Assoc. 1949;44:108–40.
Pankhurst K. “Incipient shrinkage” of collagen and gelatin. Nature. 1947;159:538.
Larsen R. Experiments and observations in the study of environmental impact on historical vegetable tanned leathers. Thermochim Acta. 2000;365:85–99.
Larsen R, Poulsen Sommer DV, Mühlen Axelsson K. Scientific approach in conservation and restoration of leather and parchments objects in archives and libraries. In: Engel P, editor. New approaches to book and paper conservation-restoration. Wien: Verlag Berger; 2011. p. 239–58.
Larsen R, Vest M, Nielsen K. Determination of hydrothermal stability (shrinkage temperature) of historical leathers by Micro Hot Table technique. J Soc Leather Technol Chem. 1993;77:151–6.
Carsote C, Kövari L, Albu C, Hadîmbu E, Badea E, Miu L, Dumitrescu G. Bindings of rare books from the collections of the Romanian Academy Library—a multidisciplinary study. Leather Footwear J. 2018;18(4):307–20.
Budrugeac P, Carşote C, Miu L. Application of thermal analysis methods for damage assessment of leather in an old military coat belonging to the History Museum of Braşov-Romania. J Therm Anal Calorim. 2017;127(1):765–72.
Mühlen Axelsson K, Larsen R, Poulsen Sommer DV, Melin R. Degradation of collagen in parchment under the influence of heat-induced oxidation: preliminary study of changes at macroscopic, microscopic, and molecular levels. Stud Conserv. 2016;61(1):46–57.
Chahine C. Changes in hydrothermal stability of leather and parchment with deterioration: a DSC study. Thermochim Acta. 2000;365:101–10.
Budrugeac P, Miu L. The suitability of DSC method for damage assessment and certification of historical leathers and parchments. J Cult Herit. 2008;9:146–53.
Miu OA, Badea E, Carsote C, Ciobanu S. Automatic detection of collagen fibres shrinkage activity using Σ-Δ filtering. In: Proceedings Book of the 5th international conference on advanced materials and systems (ICAMS 2014). Bucharest: Certex; 2014. p. 539–42.
Badea E, Poulsen Sommer DV, Mühlen Axelsson K, Larsen R, Kurysheva A, Miu L, Della Gatta G. Damage ranking in historical parchments: from microscopic study of fibres structure to collagen denaturation assessment by micro DSC. e-Preserv Sci. 2012;9:97–109.
Badea E, Şendrea C, Carşote C, Adams A, Blümich B, Iovu H. Unilateral NMR and thermal microscopy studies of vegetable tanned leather exposed to dehydrothermal treatment and light irradiation. Microchem J. 2016;129:158–65.
Sendrea C, Carșote C, Radu M, Badea E, Miu L. The effect of gamma irradiation on shrinkage activity of collagen in vegetable tanned leather. Rev Chim. 2017;68(7):1535–8.
Sebestyén Z, Jakab E, Badea E, Barta-Rajnai E, Şendrea C, Czégény ZS. Thermal degradation study of vegetable tannins and vegetable tanned leathers. J Anal Appl Pyrol. 2019;138:178–87.
Gill P, Moghadam TT, Ranjbar B. Differential scanning calorimetry techniques: applications in biology and nanoscience. J Biomol Tech. 2010;21(4):167–93.
Badea E, Della Gatta G, Usacheva T. Effects of temperature and relative humidity on fibrillar collagen within parchment: a micro Differential Scanning Calorimetry (micro DSC) study. Polym Degrad Stab. 2011;97:346–53.
Badea E, Usacheva T, Della Gatta G. The use of differential scanning calorimetry to characterise collagen deterioration in parchment. Rossiiskii Khimicheskii Zhurnal - Zhurnal Rossiiskogo Khimicheskogo Obshchestva im. D.I. Mendeleeva (Russian Chem J). 2015;59(1):28–41.
Miles CA. Kinetics of collagen denaturation in mammalian lens capsules studied by differential scanning calorimetry. Int J Biol Macromol. 1993;15:265–71.
Samouillan V, Delaunay F, Dandurand J, Merbah N, Gardou JP, Yousfi M, Gandaglia A, Spina M, Lacabanne C. Use of thermal techniques for the characterization and selection of natural biomaterials. J Funct Biomater. 2011;2:230–48.
Della Gatta G, Badea E, Ceccarelli R, Usacheva T, Mašić A. Assessment of damage in old parchment by DSC and SEM. J Therm Anal Calorim. 2005;82:637–49.
Badea E, Della Gatta G, Budrugeac P. Characterisation and evaluation of the environmental impact on historical parchments by DSC. J Therm Anal Calorim. 2011;104(2):495–506.
Carşote C, Badea E, Miu L, Della Gatta G. Study of the effect of tannins and animal species on the thermal stability of vegetable leather by differential scanning calorimetry. J Therm Anal Calorim. 2016;124(3):1255–66.
Badea E, Miu L, Budrugeac P, Giurginca M, Mašić A, Badea N, Della Gatta G. Study of deterioration of historical parchments by various thermal analysis techniques, complemented by SEM, FTIR, UV-Vis-NIR and unilateral NMR investigations. J Therm Anal Calorim. 2008;91:17–27.
Budrugeac P, Badea E, Della Gatta G, Miu L, Comănescu A. DSC study of deterioration caused by environmental chemical pollutants to parchment, a collagen based material. Thermochim Acta. 2010;500:51–62.
Carşote C, Budrugeac P, Decheva R, Haralampiev NS, Miu L, Badea E. Characterization of a byzantine manuscript by infrared spectroscopy and thermal analysis. Rev Rou Chim. 2014;59:429–36.
Falcão L, Araújo MEM. Vegetable tannins used in the manufacture of historic leathers. Molecules. 2018;23(5):1081.
Tang HR, Hancock RA, Covington AD. Study on the composition and structure of commercial chestnut tanning agent. Basic Life Sci. 1992;59:221–43.
Pasch H, Pizzi A, Rode K. MALDI-TOF mass spectrometry of polyflavonoid tannins. Polymer. 2001;42(18):7531–9.
Miles CA, Burjanadze TV, Bailey AJ. The kinetics of the thermal denaturation of collagen in unrestrained rat tail tendon determined by differential scanning calorimetry. J Mol Biol. 1995;245(4):437–46.
Luescher M, Ruegg M, Schindler P. Effect of hydration upon the thermal stability of tropocollagen and its dependence on the presence of neutral salts. Biopolymer. 1974;13:2489–503.
Miu OA, Ciobanu S, Badea E. Automatic method for damage assessment of historical and archeological leather and parchment. Patent application A/001253-05.07.2014.
Hulmes DJ. Building collagen molecules, fibrils and suprafibrillar structures. J Struct Biol. 2002;137(2):2–10.
Buehler MJ. Nature designs tough collagen: explaining the nanostructures of collagen fibrils. Proc Natl Acad Sci USA. 2006;3(33):12285–90.
Wess TJ. Collagen fibrillas structures and hierarchies. In: Fratzl P, editor. Collagen: structure and mechanics. New York: Springer; 2008. p. 49.
Covington AD. The mechanism of chrome tanning. Glob J Inorg Chem. 2010;1(2):119–31.
Covington A, Song L, Suparno O, Koon H, Collins MJ. Link-lock: an explanation of the chemical stabilisation of collagen. J Soc Leather Technol Chem. 2008;92:1–7.
Bella J, Brodsky B, Berman HM. Hydration structure of collagen. Structure. 1995;9:893–906.
Leikina E, Mertts MV, Kuznetsova N, Leikin S. Type I collagen is thermally unstable at body temperature. Proc Natl Acad Sci USA. 2002;99:1314–8.
George C Na. Monomer and oligomer of type I collagen: molecular properties and fibril assembly. Biochemistry. 1989;28:7161–7.
Tiktopulo EI, Kajava AV. Denaturation of type I collagen fibrils is an endothermic process accompanied by a noticeable change in the partial heat capacity. Biochemistry. 1998;37:8147–52.
Miles CA, Ghelashvili M. Polymer-in-a-box mechanism for the thermal stabilization of collagen molecules in fibers. Biophys J. 1999;76:3243–52.
Miles CA, Bailey AJ. Thermal denaturation of collagen revisited. Proc Indian Acad Sci (Chem. ScL). 1999;111(1):71–80.
Lin SJ, Lo W, Dong CY. Prediction of heat-induced collagen shrinkage by use of second harmonic generation microscopy. J Biomed Opt. 2006;11(3):34020.
Bozec L, Odlyha M. Thermal denaturation studies of collagen by microthermal analysis and atomic force microscopy. Biophys J. 2011;101(1):228–36.
Cucos A, Gaidau C, Badea E, Miu L. Influence of glycerin on denaturation temperature of chrome- and vegetable-tanned leather. Rev Roum Chim. 2015;60(11–12):1093–6.
Yao Q, Wang Y, Chen H, Huang H, Liu B. Mechanism of high chrome uptake of tanning pickled pelt by carboxyl-terminated hyper-branched polymer combination chrome tanning. Chem Select. 2019;4(2):670–80.
Sebestyén Z, Czégény Z, Badea E, Carsote C, Sendrea C, Barta-Rajnai E, János B, Miu L, Jakab E. Thermal characterization of new, artificially aged and historical leather and parchment. J Anal Appl Pyrol. 2015;115:419–27.