Assessment of Hydrogen Cracking Risk in Multipass Weld Metal of 2.25Cr-1Mo-0.25V-TiB (T24) Boiler Steel
Tóm tắt
Từ khóa
Tài liệu tham khảo
Lukkari J.: Creep resisting steels and welding, ESAB Group Ltd. (to be published in 2004).
EN 1011–2:2001, Welding- Recommendations for welding of metallic materials — Part 2: Arc welding of ferritic steels, CEN/TC 121, CEN 2001, 113 p.
Okuda N., Ogata Y., Nishikawa Y., Aoki T., Goto A., Abe T., Welding Journal, May 1987, 66, pp. 141s–146s.
Suzuki H., Yurioka N., Australian Welding Journal, Autumn 1982, 27, 1, pp. 9–27.
Pargeter R.J., TWI Research Report (CRP), November 1992, No. 461, The Welding Institute, UK.
Graville B.A.: A short review of weld metal hydrogen cracking, Doc. IIW-851-86 (ex. Doc. IX-1903–98), Welding in the World, 1986, vol. 24, No. 9/10, pp. 190–199.
Gedeon S.A., Eagar T.W., Welding Journal, June 1990, 69, pp. 213–s–219–s.
Yurioka N.: Test result of cold cracking in multipass weld metal, IIW-Doc. IX-1903–98, 1998.
Standard WES 1105–1985, Japanese Welding Association, Japan, 1985, 38 p.
Nevasmaa P.: Controlling factors affecting hydrogen cold cracking in high-strength multipass weld metals: Comparison of the cracking test results between SMAW and SAW welds, IIW-Doc. IX-2027–02, VTT Industrial Systems, Espoo 2002, 46 p.
Nevasmaa P.: Prevention of weld metal hydrogen cracking in high-strength multipass welds, Doc. IIW-1617-03 (ex-Doc. IX-2066–03), Welding in the World, 2004, vol. 48, No. 5/6, pp. 2–18, VTT Industrial Systems, Espoo 2003.
Nevasmaa P., Acta Universitatis Ouluensis: C Technica 191. University of Oulu: Department of Mechanical Engineering, Oulu 2003, 212 p.
Nevasmaa P.: Hydrogen cold cracking in high-strength multipass weld metal — A procedure for predicting the cracking risk and necessary precautions for safe welding, IIW-Doc. IX-2088–04, VTT Industrial Systems, Espoo 2004. 26 p.
Kuebler R., Pitrun M., Pitrun I., Australian Welding Journal, 1st Quarter 2000, 45, pp 38–47.
Håkansson K.: Submerged arc welding of Weldox 900E in 50 mm plate thickness — Hydrogen cracking tests, IIW-Doc. II-A-117-03II-1495–03, Kockums AB, Laboratory, Sweden, 2003.
Åström H., Svetsen, 2001, 60, 5, pp. 7–14.
Alcãntara N.G., Rogerson J.H., Welding Journal, 1984, 63, 4, pp. 116s–122s.
Yurioka N.: Predictive methods for prevention and control of hydrogen assisted cold cracking, IIW-Doc. IX-1938–99, 1999. 16 p.
Karppi R., Ruusila J., Toyoda M., Satoh K., Vartiainen K., Scandinavian Journal of Metallurgy, 1984, 13, pp. 66–74.
Karppi R., Publication No 1/1976, Helsinki University of Technology, Laboratory of Materials Technology, Espoo 1976, 422 p.
Karppi R., VTT Publications No 9, Technical Research Centre of Finland, Espoo 1982, 119 p.
Terasaki T., Karppi R., Satoh K., Transactions of the Japan Welding Society, 1979, 10, 1, pp. 53–57.
Yurioka N., Ohshita S., Nakamura H., Asano K.: An analysis of effects of microstructure, strain and stress on the hydrogen accumulation in the weld heat-affected zone, IIW-Doc. IX-1161–80, 1980, 20 p.
Yurioka N.: A review of numerical analyses on the hydrogen diffusion in welding of steel, IIW-Doc. IX-1553–89, 1989, 12 p.
Wong R.J.: Hydrogen cracking resistance of high strength steels in single-pass and multiple-pass weld- ability tests, Proc. Conf. “Materials Week’ 95 Symposium: Welding and Weld Automation in Ship-building”, Cleveland, Ohio, 29 Oct. — 2 Nov. 1995, The Minerals, Metals and Materials Society, USA 1996, pp. 33–46.
Lee H.W., Kang S.W., Welding Journal, August 2003, 82, pp. 225s–230s.
Standard ISO 3690:1977, Welding — Determination of hydrogen in deposited weld metal arising from the use of covered electrodes for welding mild and low alloy steels, International Organisation for Standardisation, 1977. 4 p.
Nevasmaa P., Karppi R., Research Report VAL-B-202 / Jernkontorets Forskning TO 40–39, Jern- kontoret, Stockholm, 1998, 81 p.
Standard SFS-EN 288–3:1992. Finnish Standards Association, 1992 (in Finnish).
Final Draft Standard: prEN ISO 15614–1, CEN/TC 121 N 998, CEN/ISO, 2002. 28 p.
Yurioka N.: Prediction of weld metal strength (Report III), IIW-Doc. IX-2058–03, 35 p.
VTT Tutkimusselostus TUO74–033322. VTT Tuotteet ja tuotanto, Espoo 2003 (in Finnish).
Nevasmaa P., Laukkanen A., Häkkilä J.: Evaluation of Weld Metal Hydrogen Cracking Risk in a 2.25Cr-1Mo-0.25V-TiB (T24) Boiler Steel, Proc. Conf. “6th International Conference on Life Management and Maintenance for Power Plants (Baltica VI)”, Helsinki-Stockholm-Helsinki, 8–10 June 2004, The Finnish Maintenance Society (FMS), Finland 2004, vol. 2, pp. 393–407.
Karppi R., Nevasmaa P.: Contribution to comparisons of methods for determining welding procedures for the avoidance of hydrogen cracking, IIW-Doc. IX-1673–92 /VTT Publications No 107, Technical Research Centre of Finland, Espoo 1992, 50 p.
Karppi R., Ruusila J., Toyoda M., Satoh K., Vartiainen K., VTT Research Reports No. 240, Technical Research Centre of Finland, Espoo 1984, 22 p.
Nevasmaa P., Cederberg M., Vilpas M., VTT Research Notes No. 1406. Espoo 1992, 31 p.
Laukkanen A., Nevasmaa P., Alhainen J.: Numerical Evaluation of Hydrogen Cracking using Transient Finite Element Analysis and Concentration Dependent Damage Mechanics Constitutive Model, Proc. Conf. “7th International Seminar: Numerical Analysis of Weldability (NAW-7)”, Graz — Seggau, 29 Sept. — 1 Oct. 2003, Institute for Materials Science, Welding and Forming (IWS) & Graz University of Technology (TUG), Austria 2003, 16 p. (to be released in 2005).