ZrB2-SiC as a protective coating for C/SiC composites: Effect of high temperature oxidation on thermal shock property and protection mechanism

Journal of Asian Ceramic Societies - Tập 4 - Trang 159-163 - 2016
Xiang Yang1, Cao Feng1, Wang Qing1
1Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, National University of Defense Technology, Changsha 410073, Hunan, China

Tài liệu tham khảo

Li G.D., 2012, Mater. Sci. Eng. A, 547, 1, 10.1016/j.msea.2012.03.045 Li G.D., 2013, Composites Part B: Eng., 48, 134, 10.1016/j.compositesb.2012.09.093 Jian K., 2007, Ceram. Int., 33, 905, 10.1016/j.ceramint.2006.02.005 Yang X., 2012, Ceram. Int., 38, 9, 10.1016/j.ceramint.2011.06.063 Liu Q.M., 2010, J. Am. Ceram. Soc., 93, 3990, 10.1111/j.1551-2916.2010.04178.x Wang Y.G., 2009, Mater. Sci. Eng. A, 524, 129, 10.1016/j.msea.2009.07.005 Mattia D., 2005, J. Eur. Ceram. Soc., 25, 1789, 10.1016/j.jeurceramsoc.2004.12.011 Y.BlumJ.MarschallAFRL-ML-WP-TR-2006-420020061116 Yang X., 2013, Composites Part B: Eng., 45, 1391, 10.1016/j.compositesb.2012.07.007 Yajima S., 1978, J. Mater. Sci., 13, 2569 Yang X., 2014, Ceram. Int., 40, 9087, 10.1016/j.ceramint.2014.01.122 Chamberlain A.L., 2009, J. Eur. Ceram. Soc., 29, 3401, 10.1016/j.jeurceramsoc.2009.07.006 Fahrenholtz W., 2005, J. Am. Ceram. Soc., 88, 3509, 10.1111/j.1551-2916.2005.00599.x Wang H., 1996, J. Am. Ceram. Soc., 79, 1783, 10.1111/j.1151-2916.1996.tb07996.x Kagawa Y., 1993, J. Mater. Sci., 28, 735, 10.1007/BF01151250 Zhang C.Y., 2013, J. Mater. Eng. Perform., 22, 1680, 10.1007/s11665-012-0465-z Kastritseas C., 2008, J. Mater. Sci., 43, 4112, 10.1007/s10853-007-2314-2 Fu Q.G., 2006, Mater. Sci. Eng. A, 434, 335, 10.1016/j.msea.2006.07.031