X-ray and differential scanning calorimetry study of the crystallization of amorphous Fe73.5 Cu1Nb3 Si13.5B9 alloy
Materials Science and Engineering B: Solid-State Materials for Advanced Technology - Tập 34 - Trang 204-209 - 1995
Tài liệu tham khảo
Yoshizawa, 1988, J. Appl. Phys., 64, 6044, 10.1063/1.342149
Yoshizawa, 1990, Mater. Trans. Jpn. Inst. Met., 31, 307
Kim, 1994, Mater. Sci. Eng. A, 179–180, 309
Zhou, 1994, Mater, Sci. Eng. A, 181–182, 1419, 10.1016/0921-5093(94)90876-1
Varga, 1994, Mater. Sci. Eng. A, 179–180, 567, 10.1016/0921-5093(94)90268-2
Varga, 1978
1985, Vol. 2
Kissinger, 1957, Anal, Chem., 29, 1702, 10.1021/ac60131a045
Häβner, 1985, Z. Metallkd., 76, 198
Avrami, 1939, J. Chem. Phys., 7, 1103, 10.1063/1.1750380
Noh, 1990, J. Appl. Phys., 67, 5568, 10.1063/1.345887
He, 1994, J. Appl. Phys., 75, 3684, 10.1063/1.356086
Rixecker, 1992, J. Phys.: Condens. Matter, 4, 10295, 10.1088/0953-8984/4/50/017
Ueda, 1994, Mater. Sci. Eng. A, 181–182, 992, 10.1016/0921-5093(94)90786-2
Calka, 1988, Mater. Sci. Eng. A, 97, 241, 10.1016/0025-5416(88)90050-X