Use of ultrasound irradiation during acid etching of the 2024 aluminum alloy: Effect on corrosion resistance after anodization
Tài liệu tham khảo
Huda, 2009, Characterization of 2024–T3: an aerospace aluminum alloy, Mater. Chem. Phys., 113, 515, 10.1016/j.matchemphys.2008.09.050
Niu, 2019, Exfoliation corrosion of friction stir welded dissimilar 2024-to-7075 aluminum alloys, Mater. Charact., 147, 93, 10.1016/j.matchar.2018.11.002
Buchheit, 1997, Local dissolution phenomenon associated with S phase (Al2CuMg) particles in aluminum alloy AA 2024-T3, J. Electrochem. Soc., 144, 2621, 10.1149/1.1837874
Guillaumin, 1999, Localized corrosion of 2024 T3 aluminum alloy in chloride media, Corros. Sci., 41, 421, 10.1016/S0010-938X(98)00116-4
Boag, 2010, Stable pit formation on AA2024-T3 in NaCl environment, Corros. Sci., 52, 90, 10.1016/j.corsci.2009.08.043
Prakashaih, 2018, Corrosion inhibition of 2024–T3 aluminum alloy in 3.5% NaCl by thiosemicarbazione derivates, Corros. Sci., 136, 326, 10.1016/j.corsci.2018.03.021
Moutarlier, 2001, Electrochemical characterisation of anodic oxidation films formed in presence of corrosion inhibitors, Appl. Surf. Sci., 183, 1, 10.1016/S0169-4332(01)00364-6
Moutarlier, 2002, Characterisation of pitting corrosion in sealed anodic films formed in sulphuric, sulphuric/molybdate and chromic media, Appl. Surf. Sci., 206, 237, 10.1016/S0169-4332(02)01240-0
Tiringer, 2017, Effects of mechanical and chemical pre-treatemnts on the morphology and composition of surfaces of aluminum alloys 7075–T6 and 2024–T3, Corros. Sci., 119, 46, 10.1016/j.corsci.2017.02.018
Lunder, 2002, Pre-treatment of AA6060 aluminum alloy for adhesive bonding, Int. J. Adhes. Adhes., 22, 143, 10.1016/S0143-7496(01)00049-5
Sorrentino, 2009, 2024 aluminum alloy wettability and superficial cleaning improvement by air cold plasma treatment, J. Mater. Process. Technol., 209, 1400, 10.1016/j.jmatprotec.2008.03.061
Prolongo, 2009, Effect of surface pre-treatment on the adhesive strength of epoxy-aluminum joints, Int. J. Adhes. Adhes., 29, 23, 10.1016/j.ijadhadh.2008.01.001
Critchlow, 1996, Review of surface pretreatments for aluminum alloys, Int. J. Adhes. Adhes., 16, 255, 10.1016/S0143-7496(96)00014-0
Qi, 2016, Influence of pre- and post-treatments on formation of trivalent chromium conversion coating on AA2024 alloy, Thin Solid Film, 616, 270, 10.1016/j.tsf.2016.08.044
Habazaki, 1995, Oxidation of copper and mobility of copper ions during anodizing of an Al-1.5wt% cu alloy, Surf. Interface Anal., 23, 892, 10.1002/sia.740231307
Zhuravlyova, 2002, Oxygen evolution within barrier layer oxide films, Corros. Sci., 44, 2153, 10.1016/S0010-938X(02)00025-2
Saenz de Miera, 2010, Preferential anodic oxidation of second-phase constituents during anodizing of AA2024-T3 and AA7075-T6 alloys, Surf. Interface Anal., 42, 241, 10.1002/sia.3191
Ji, 2018, Controlled”golf ball shape” structuring of Mg surface under acoustic cavitation, Ultrason. Sonochem., 40, 30, 10.1016/j.ultsonch.2017.06.018
Verdan, 2003, Structural changes of metallic surfaces induced by ultrasound, Ultrason. Sonochem., 10, 291, 10.1016/S1350-4177(03)00106-8
Moutarlier, 2015, Power ultrasound irradiation during the alkaline etching process of the 2024 aluminum alloy, Appl. Surf. Sci., 355, 26, 10.1016/j.apsusc.2015.07.098
Hu, 2017, Ultrasonic effect on etching tunnel morphology and distribution of aluminum foil, Appl. Surf. Sci., 392, 375, 10.1016/j.apsusc.2016.09.074
Kang, 2005, Growth of etch pits formed during sonoelectroetching of aluminum, Electrochim. Acta, 51, 1012, 10.1016/j.electacta.2005.04.070
Bibi, 2018, Comparative study of the modification of multi-wall carbon nanotubes by gamma irradiation and sonochemically assisted acid etching, Mater. Chem. Phys., 207, 23, 10.1016/j.matchemphys.2017.12.047
Yang, 2006, Ultrasonically treated multi-walled carbon nanotubes (MWCNTs) as PtRu catalyst supports for methanol electooxidation, J. Power Sources, 160, 187, 10.1016/j.jpowsour.2006.05.015
Tian, 2016, Comparatively studying the ultrasound present in a mild two-stage approach on the content of functional groups in modified MWCNT, Chem. Phys. Lett., 650, 11, 10.1016/j.cplett.2016.02.050
Ng, 2013, Improved functionalization and recovery of carboxylated carbon nanotubes using the acoustic cavitation approach, Chem. Phys. Lett., 557, 97, 10.1016/j.cplett.2012.11.095
Mandroyan, 2009, Modification of the ultrasound induced activity by the presence of an electrode in a sono-reactor working at two low frequencies (20 and 40 kHz). Part II: Mapping flow velocities by particle image velocimetry (PIV), Ultrason. Sonochem., 16, 97, 10.1016/j.ultsonch.2008.05.004
Viennet, 2004, Visualisation and electrochemical determination of the active zones in an ultrasonic reactor using 20 and 500kHz frequencies, Ultrason. Sonochem., 11, 125, 10.1016/j.ultsonch.2004.01.007
Tomita, 1990, High-speed photographic observations of laser-induced cavi-tation bubbles in water, Acta Acust. United Acust., 71, 161
Gregorcic, 2007, Investigation of a cavitation bubble betweena rigid boundary and a free surface, J. Appl. Phys., 102, 10.1063/1.2805645
Niemczewski, 2007, Observations of water cavitation intensity under practical ultrasonic cleaning conditions, Ultrason. Sonochem., 14, 13, 10.1016/j.ultsonch.2005.11.009
Alventosa-deLara, 2014, Study and optimization of the ultrasound-enhanced cleaning of an ultrafiltration ceramic membrane through a combined experimental–statistical approach, Ultrason. Sonochem., 21, 1222, 10.1016/j.ultsonch.2013.10.022
Mazue, 2011, Large-scale ultrasonic cleaning system: Design of a multi-transducers device for boat cleaning (20 kHz), Ultrason. Sonochem., 18, 895, 10.1016/j.ultsonch.2010.11.021
Romdhane, 1997, Experimental study of the ultrasound attenuation in chemical reactors, Ultrason. Sonochem., 4, 235, 10.1016/S1350-4177(97)00002-3
Szklarska-Smialowska, 1999, Pitting corrosion of aluminum, Corros. Sci., 41, 1743, 10.1016/S0010-938X(99)00012-8
Moutarlier, 2005, EIS characterisation of anodic films formed on 2024 aluminum alloy, in sulphuric acid containing molybdate or permanganate species, Corros. Sci., 47, 937, 10.1016/j.corsci.2004.06.019
Moreto, 2014, SVET, SKP and EIS study of the corrosion behavior of high strength Al and Al-Li alloys used in aircraft fabrication, Corros. Sci., 84, 30, 10.1016/j.corsci.2014.03.001
Gao, 1998, An analytical electron microscopy study of constituent particles in commercial 7075–T6 and 2024–T3 alloys, Metallur. Mater. Trans. A, 29A, 1145, 10.1007/s11661-998-0240-9
Wei, 1998, A transmission electron microscopy study of constituent particle-induced corrosion in 7075–T6 and 2024–T3 aluminum alloys, Metallur. Mater. Trans. A, 29A, 1153, 10.1007/s11661-998-0241-8
Shao, 2003, A study on pitting corrosion of aluminum alloy 2024–T3 by scanning microreference electrode technique, Mater. Sci. Eng. A, 344, 323, 10.1016/S0921-5093(02)00445-8
Lacroix, 2012, Simulating the galvanic coupling between S-Al2CuMg phase particles and the matrix of 2024 aerospace aluminum alloy, Corros. Sci., 64, 213, 10.1016/j.corsci.2012.07.020
Hashimoto, 2016, Investigation of dealloying of S phase (Al2CuMg) in AA 2024–T3 aluminum alloy using high resolution 2D and 3D electron imaging, Corros. Sci., 103, 157, 10.1016/j.corsci.2015.11.013
Doche, 2003, Influence of ultrasound power and frequency upon corrosion kinetics of zinc in saline media, Ultrason. Sonochem., 10, 357, 10.1016/S1350-4177(03)00099-3
Pugin, 1987, Qualitative characterization of ultrasound reactors for heterogenous sonochemistry, Ultrasonics, 25, 49, 10.1016/0041-624X(87)90012-6
Chivate, 1995, Quantification of cavitation intensity in fluid bulk, Ultrason. Sonochem., 2, s19, 10.1016/1350-4177(94)00007-F
Nguyen, 2017, Dependance of cavitation, chemical effect, and mechanical effect thresholds on ultrasonic frequency, Ultrason. Sonochem., 39, 301, 10.1016/j.ultsonch.2017.04.037