The role of the interface in the initiation of fatigue cracks in SCS-6/titanium MMCs

Composites - Tập 25 - Trang 692-697 - 1994
I. Greaves1, J.R. Yates2, H.V. Atkinson3
1GEC Alsthom Turbine Generators Limited, Newbold Road, Rugby, Warwickshire CV21 2NH, UK
2Department of Mechanical & Process Engineering, at The University of Sheffield, PO Box 600, Mappin Street, Sheffield S1 4DU, UK
3Department of Engineering Materials, at The University of Sheffield, PO Box 600, Mappin Street, Sheffield S1 4DU, UK

Tài liệu tham khảo

Driver, 1990, Materials and process directions for advanced aeroengine design, 883 Wei, 1992, High temperature MMC's for aero-engines: challenge and potential, Metals and Materials, 8, 430 Civil Aviation Authority, 1981 Kantzos, 1991, Fatigue crack growth in a unidirectional SCS-6/Ti-15-3 composite, 711 Greaves, 1994, The growth of naturally initiating fatigue cracks in titanium-silicon carbide MMCs Jeng, 1991, Fracture mechanisms of fiber-reinforced titanium alloy matrix composites, Part IV: Low cycle fatigue, Mater Sci & Engng, A148, 67, 10.1016/0921-5093(91)90866-L Cox, 1989, Failure mechanisms in titanium aluminide/SiC composites, 313 Partridge, 1993, Processing of advanced continuous fibre composites: current practice and potential developments, Int Mater Rev, 38, 1, 10.1179/095066093790150901 Wawner, 1988, Boron and silicon carbide/carbon fibers, 371 Ning, 1991, The microstructure of SCS-6 SiC fiber, J Mater Res, 6, 2234, 10.1557/JMR.1991.2234 Cook, 1991, Control of fibre matrix interactions in SiC/Ti MMC, European Community Report EUR 13614, Industrial processes series Lerch, 1990, Microstructure of a SiC/Ti-15-3 composite, Composites, 21, 216, 10.1016/0010-4361(90)90236-P Jones, 1989, The characterization of an SCS6/Ti-6Al-4V MMC interphase, J Mater Res, 4, 327, 10.1557/JMR.1989.0327 Yang, 1989, Interfacial reactions in titanium-matrix composites, J Metals, 41, 56 Lee, R.J. (AEA Technology, Harwell Laboratory, Oxfordshire, UK) Private communication de los Rios, 1989, Experimental techniques to observe and monitor short fatigue cracks, 265 Curtin, 1993, Ultimate strengths of fibre-reinforced ceramics and metals, Composites, 24, 98, 10.1016/0010-4361(93)90005-S Miller, 1991, Metal fatigue — past, current and future: 27th John Player Lecture, 205, 291 1986 Rhodes, 1985, Fiber-matrix reaction zone growth kinetics in SiC-reinforced Ti-6Al-4V as studied by transmission electron microscopy, 864, 585