The degradation behavior of UHTCs based coatings coated PIP-C/SiC composites in thermal cycling environment
Tài liệu tham khảo
Li, 2012, Preparation and mechanical properties of C/SiC nuts and bolts, Mater Sci Eng A, 547, 1, 10.1016/j.msea.2012.03.045
Li, 2013, Design, preparation and properties of online-joints of C/SiC-C/SiC with pins, Compos Part B Eng, 48, 134, 10.1016/j.compositesb.2012.09.093
Jian, 2007, Effects of polycarbosilane infiltration processes on the microstructures and mechanical properties of 3D-Cf/SiC composites, Ceram Int, 33, 905, 10.1016/j.ceramint.2006.02.005
Xiang, 2012, Oxidation behavior of oxidation protective coatings for PIP–C/SiC composites at 1500°C, Ceram Int, 38, 9, 10.1016/j.ceramint.2011.06.063
Xiang, 2012, Ablative property of ZrC–SiC multilayer coating for PIP-C/SiC composites under oxy-acetylene torch, Ceram Int, 38, 2893, 10.1016/j.ceramint.2011.11.063
Blum, 2006
Xiang, 2013, ZrB2/SiC as a protective coating for C/SiC composites: effect of high temperature oxidation on mechanical properties and anti-ablation property, Compos Part B Eng, 45, 1391, 10.1016/j.compositesb.2012.07.007
Xiang, 2014, Thermal shock properties of 3D-C/SiC composites prepared via polymer infiltration pyrolysis (PIP), Ceram Int, 40, 9087, 10.1016/j.ceramint.2014.01.122
Zhang, 2012, Mechanical behavior of C/SiC composites under simulated space environments, Mater Sci Eng A, 534, 408, 10.1016/j.msea.2011.11.087
Jia, 1999, Study on poly (methyl methacrylate)/carbon nanotube composites, Mater Sci Eng A, 271, 395, 10.1016/S0921-5093(99)00263-4
Mark, 2005, The effect of thermal cycling on the properties of a carbon fibre reinforced magnesium composite, Mater Sci Eng A, 397, 249, 10.1016/j.msea.2005.02.025
Lin, 2002, Thermal cycling induced deformation and damage in carbon fiber reinforced copper composite, Scr Mater, 46, 169, 10.1016/S1359-6462(01)01217-9
Xiang, 2012, Microstructures and mechanical properties of CVD-SiC coated PIP-C/SiC composites under high temperature, Surf Coat Technol, 209, 197, 10.1016/j.surfcoat.2012.08.055
Powder diffraction file, Joint Committee on Powder Diffraction Standard, Card 06–0610.
Powder diffraction file, Joint Committee on Powder Diffraction Standard, Card 35–0784.
Chamberlain, 2009, Reactive hot pressing of zirconium diboride, J Eur Ceram Soc, 29, 3401, 10.1016/j.jeurceramsoc.2009.07.006
Zhang, 2013, Thermal shock properties of a 2D-C/SiC composite prepared by chemical vapor infiltration, J Mater Eng Perform, 22, 1680, 10.1007/s11665-012-0465-z
Wang, 1996, Thermal shock behavior of two dimensional woven fiber-reinforced ceramic composites, J Am Ceram Soc, 79, 1783, 10.1111/j.1151-2916.1996.tb07996.x
Kagawa, 1993, Thermal shock resistance of SiC fiber-reinforced borosilicate glass and lithium aluminosilicate matrix composites, J Mater Sci, 28, 735, 10.1007/BF01151250
Xiang, 2012, Preparation of UHTC based coatings for C–SiC composites by slurry and CVD, Mater Technol, 27, 257, 10.1179/106678512X13333821993928
Xiang, 2015, The degradation behavior of SiC coated PIP-C/SiC composites in thermal cycling environment, Compos Part B Eng, 79