Springer Science and Business Media LLC - Tập 34 - Trang 200-202 - 2002
L. A. Zlatoustova1, V. N. Smirnova1, V. A. Medvedev1, A. T. Serkov1
1All-Russian Scientific-Research Institute of Polymer Fibres, Mytishchi

Tóm tắt

The closed porosity of polyacrylonitrile fibres wet-spun from dimethyl acetamide solutions was investigated in raising the spinning bath temperature from 2 to 20°C. The dependence of the porosity of the fibre on the conditions of plasticization treatment is established. The fibre treated in saturated vapor medium has higher porosity values (narrow transmission factors in chlorobenzene) than the fibre treated with a hot aqueous solution of dimethyl acetamide. The dependence of the fibre porosity on the drying and repeated washing and subsequent drying temperatures is demonstrated. The mobility of the structural elements increases and the porosity of the fibre decreases with an increase in the drying temperature.

Tài liệu tham khảo

A. T. Serkov, Khim. Volokna, No. 2, 41–45 (2001). Qian Baojun, Qin Jian, and Zhou Lhanlong, Textile Asia, 20,No. 4, 40, 49–56 (1989).