Temperature and pressure effects on the degradation of polypropylene tape yarns—depletion of antioxidants

Geotextiles and Geomembranes - Tập 22 - Trang 511-530 - 2004
Mengjia Li1, Y. Grace Hsuan1
1Department of Civil, Architectural and Environmental Engineering, Drexel University, 3141 Chestnut Street, Philadelphia, PA 19104, USA

Tài liệu tham khảo

ASTM D792, 2000. Test Method for Specific Gravity (Relative Density) and Density of Plastics by Displacement, vol. 08.01. American Society for Testing and Materials, Pennsylvania, USA. ASTM D1238, 2004. Standard Test Method for Melt Flow Rates of Thermoplastics by Extrusion Plastometer, vol. 08.01. American Society for Testing and Materials, Pennsylvania, USA. ASTM D3822, 2001. Standard Test Method for Tensile Properties of Single Textile Fibers, vol. 07.02. American Society for Testing and Materials, Pennsylvania, USA. ASTM D3895, 2003. Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry, vol. 08.02. American Society for Testing and Materials, Pennsylvania, USA. ASTM D5885, 1997. Standard Test Method for Oxidative Induction Time of Polyolefin Geosynthetics by High-Pressure Differential Scanning Calorimetry, vol. 04.09. American Society for Testing and Materials, Pennsylvania, USA. Aktins, 1986 Billingham, 1975, Autoxidation of poly 4-methylpentene-1. I. The role of diffusion in autoxidation kinetics, Journal of Polymer Science, Polymer Chemistry Edition, 13, 1209, 10.1002/pol.1975.170130515 Boss, 1966, Oxygen diffusion limitation in auto-oxidation of polypropylene, Journal of Polymer Science: Part A-1, 4, 1543, 10.1002/pol.1966.150040618 Ding, 2001, Activation Energies of Polymer Degradation, 219 Elias, V., Salman, A., Juran, I., Pearce, E., Lu, S., 1999. Testing protocols for oxidation and hydrolysis of geosynthetics, Federal Highway Administration, Washington, Report No. FHWA-RD-97-144. pp. 200. Hsuan, Y.G., Guan, Z., 1998. Antioxidant depletion during thermal oxidation of high density polyethylene geomembranes. Sixth International Conference on Geosynthetics Proceedings. Atlanta, Georgia, USA, pp. 375–380. Hsuan, 1998, Antioxidant depletion lifetime in high density polyethylene geomembranes, Journal of Geotechnical and Geoenvironmental Engineering, ASCE, 124, 532, 10.1061/(ASCE)1090-0241(1998)124:6(532) Incropera, 2002 Morrison, 1992 Mueller, 2003, Oxidative resistance of high-density polyethylene geomembranes, Polymer Degradation and Stability, 79, 161, 10.1016/S0141-3910(02)00269-0 Mueller, 2003, Comparison of the oxidative resistance of various polyolefin geotextiles, Geotextiles and Geomembranes, 21, 289, 10.1016/S0266-1144(03)00032-3 Rowe, 2002, Durability of HDPE geomembranes, Geotextiles and Geomembranes, 20, 77, 10.1016/S0266-1144(02)00005-5 Salman, A., Elias, V., DiMillio, A., 1998. The effect of oxygen pressure, temperature and manufacturing process on laboratory degradation of polypropylene geosynthetics. Sixth International Conference on Geosynthetics Proceedings Atlanta, Georgia, USA, pp. 683–690. Sangam, 2002, Effects of exposure conditions on the depletion of antioxidants from HDPE geomembranes, Canadian Geotechnical Journal, 39, 1221, 10.1139/t02-074 Schroeder, H.F., Bahr, H., Herrmann, P., Kneip, G., Lorenz, E., Schmuecking, I., 2000. Durability of polyolefin geosynthetics under elevated oxygen pressure in aqueous liquids. Proceedings of second European Geosynthetics Conference (EuroGeo 2), Italy, pp. 459–464. Tikuisis, T., Lam, P., Cossar, M., 1992. High pressure oxidative inductive time analysis by differential scanning calorimetry. MQC/MQA and CQC/CQA of Geosynthetics, In: Koerner, R.M., Hsuan, Y.G. (Eds.), six GRI Conference, Philadelphia, pp. 191–201. Vink, 2000, Testing the resistance to oxidation of polypropylene geotextiles at enhanced oxygen pressures, Geotextiles and Geomembranes, 18, 333, 10.1016/S0266-1144(99)00019-9