Kumari, 2014, Failure analysis of gas turbine rotor blades, Eng. Fail Anal., 45, 234, 10.1016/j.engfailanal.2014.06.003
Kovacı, 2019, The effect of surface plastic deformation produced by shot peening on corrosion behavior of a low-alloy steel, Surf. Coat. Technol., 360, 78, 10.1016/j.surfcoat.2019.01.003
Liu, 2015, Characterization of surface layer in TC17 alloy treated by air blast shot peening, Mater Des., 65, 120, 10.1016/j.matdes.2014.09.019
Ion, 2019, Multilayer protective coatings obtained by pulsed laser deposition, Appl. Surf. Sci., 479, 1124, 10.1016/j.apsusc.2019.02.186
Qiao, 2019, Influence parameters and development application of laser shock processing, Surface Technol., 48, 1
Cao, 2019, Laser shock processing improving the high temperature oxidation resistance of the aluminized coating on GH202 by pack cementation, Appl. Surf Sci., 493, 729, 10.1016/j.apsusc.2019.07.028
Lu, 2019, Effect of initial surface roughness on the actual intensity of laser shock processing, Surface Topogr. Metrol. Prop., 7, 10.1088/2051-672X/ab0d9d
Shen, 2020, Residual stresses induced by laser shock peening in orthopaedic Ti-6Al-7Nb alloy, Opt. Laser Technol., 131, 10.1016/j.optlastec.2020.106446
Luo, 2016, Tensile properties, residual stress distribution and grain arrangement as a function of sheet thickness of Mg-Al-Mn alloy subjected to two-sided and simultaneous LSP impacts, Appl. Surf Sci., 369, 366, 10.1016/j.apsusc.2016.02.045
Cui, 2019, Microstructure evolution and mechanical properties of aging 6061 Al alloy via laser shock processing, J. Alloys Compd., 803, 1112, 10.1016/j.jallcom.2019.06.347
Ren, 2016, Microstructure evolution and grain refinement of Ti-6Al-4V alloy by laser shock processing, Appl. Surf Sci., 363, 44, 10.1016/j.apsusc.2015.11.192
Guo, 2018, Laser shock peening of laser additive manufactured Ti6Al4V titanium alloy, Surface Coat. Technol., 349, 503, 10.1016/j.surfcoat.2018.06.020
Wu, 2020, A method to determine the material constitutive model parameters of FGH4095 alloy treated by laser shock processing, Appl. Surface Sci. Adv., 1, 10.1016/j.apsadv.2020.100029
Sun, 2019, Effect of laser shock processing with post-machining and deep cryogenic treatment on fatigue life of GH4169super alloy, Int. J. Fatigue, 119, 261, 10.1016/j.ijfatigue.2018.10.012
Zhou, 2017, Laser shock processing on Ni-based superalloy K417 and its effect on thermal relaxation of residual stress, Int. J. Adv. Manuf. Technol., 88, 675, 10.1007/s00170-016-8796-9
Wang, 2014
Lu, 2017, Effect of laser shock on tensile deformation behavior of a single crystal nickel-base superalloy, Mater. Sci. Eng. A, 686, 46, 10.1016/j.msea.2017.01.039
Geng, 2020, Evolutions of microstructure, phase, microhardness, and residual stress of multiple laser shock peened Ni-based single crystal superalloy after short-term thermal exposure, Opt. Laser Technol., 123, 10.1016/j.optlastec.2019.105917
Ge, 2016, Effect of laser shock peening on microstructure and fatigue crack growth rate of AZ31B magnesium alloy, J. Alloys Compd., 680, 544, 10.1016/j.jallcom.2016.04.179
Johnson, 1971, Dynamic deformation twinning in shock loaded iron, J. Appl. Phys., 42, 4171, 10.1063/1.1659750
Peyre, 1995, Laser shock processing: a review of the physics and applications, Opt. Quantum Electr., 27, 1213, 10.1007/BF00326477
Hu, 2020, Numerical simulation of the surface morphology and residual stress field of IN718 alloy by Gaussian mode laser shock, Optik, 207, 1, 10.1016/j.ijleo.2020.164441
Gill, 2013, Comparison of mechanisms of advanced mechanical surface treatments in nickel-based superalloy, Mater. Sci. Eng. A, 576, 346, 10.1016/j.msea.2013.04.021
Liu, 2019, Research on the dynamic yield strength and forming depth of microscale laser shock imprinting, Opt. Laser Technol., 116, 189, 10.1016/j.optlastec.2019.03.026
2012
Chen, 2014
Chen, 2012, X-ray diffraction analysis for residual stress in shot peened layer of DD3 nickel-based single crystal high temperature alloy[J], Mater. Mech. Eng., 3, 76
An, 1990
Chen, 2004, Characterization of plastic deformation induced by microscale laser shock peening, J. Appl. Mech. Trans. ASME, 71, 713, 10.1115/1.1782914
Lu, 2016, Nonuniformity of morphology and mechanical properties on the surface of single crystal superalloy subjected to laser shock peening, J. Alloys Compd., 658, 721, 10.1016/j.jallcom.2015.10.238
Lu, 2019, Surface microstructure evolution analysis of TiAl alloy by laser shock peening, Rare Met. Mater. Eng., 48, 841
Zhang, 2011, Influence of cavity morphology on creep behaviors of single crystal nickel-base superalloy, Chin. J. Nonferrous Metals, 21, 762
Huang, 2020, Formation mechanism of microporosity in complex nickel-based single crystal casting, J. Mater. Eng., 48, 123
Fatoba, 2018, Evaluation of microstructure, microhardness, and electrochemical properties of laser-deposited Ti-Co coatings on Ti-6Al-4V Alloy, Int. J. Adv. Manuf. Technol., 97, 2341, 10.1007/s00170-018-2106-7
Garcia-Giron, 2018, Combined surface hardening and laser patterning approach for functionalising stainless steel surfaces, Appl. Surf. Sci., 439, 516, 10.1016/j.apsusc.2018.01.012
Zan, 2019, Effect of laser shock processing on residual stress and microstructure of Ti834 titanium alloy, Rare Met. Mater. Eng., 48, 3535
Wu, 2018, Acoustic wave detection of laser shock peening, Opto Electron. Adv., 1, 10.29026/oea.2018.180016
Wang, 2016, Effects of laser shock processing on microstructure and mechanical properties of K403 nickel-alloy, Mater Des., 89, 582, 10.1016/j.matdes.2015.10.022
Liu, 2011, Influence of temperature on tensile behavior and deformation mechanism of Re-containing single crystal superalloy, Trans. Nonferrous Metals Soc. China, 21, 1518, 10.1016/S1003-6326(11)60890-X
Shen, 2017, Improvement in mechanical properties of titanium alloy (Ti-6Al-7Nb) subject to multiple laser shock peening, Surf. Coat. Technol., 327, 101, 10.1016/j.surfcoat.2017.08.009