Studies on mechanical strength, thermal expansion of layering porcelains to alumina and zirconia ceramic core materials

Dental Materials Journal - Tập 28 Số 3 - Trang 352-361 - 2009
Yoshitaka SHIJO1, Akikazu Shinya1,2, Harunori Gomi1, Lippo Lassila2, Pekka K. Vallittu2, Akiyoshi Shinya1
1Department of Crown and Bridge, School of Life Dentistry at Tokyo, The Nippon Dental University
2Department of Prosthetic Dentistry and Biomaterials Science, Institute of Dentistry, University of Turku

Tóm tắt

Từ khóa


Tài liệu tham khảo

1) Morena R, Lockwood PE, Fairhurst CW. Fracture toughness of commercial dental porcelains. Dent Mater 1986; 2: 58-62.

2) Drummond JL, King TJ, Bapna MS, Koperski RD. Mechanical property evaluation of pressable restorative ceramics. Dent Mater 2000; 16: 226-233.

3) Cattell MJ, Palumbo RP, Knowles JC, Clarke RL, Samarawickrama DYD. The effect of veneering and heat treatment on the flexural strength of Empress 2 ceramics. J Dent 2002; 30: 161-169.

4) Kuroda Y, Shinya A, Matsuda T, Katagiri S. The mechanical properties of the pressable ceramics and its optimal crystallization. J J Dent Mater 2003; 22: 221-230.

10.1016/j.dental.2003.05.003

10.1016/j.dental.2003.05.002

10.1016/S0109-5641(03)00093-9

8) White SN, Miklus VG, McLaren EA, Lang LA, Caputo AA. Flexural strength of a layered zirconia and porcelain dental all-ceramic system. J Prosthet Dent 2005; 94: 125-131.

9) Yilmaz H, Aydin C, Gul BE. Flexural strength and fracture toughness of dental core ceramics. J Prosthet Dent 2007; 98: 120-128.

10) Kim JW, Kim JH, Thompson VP, Zhang Y. Sliding contact fatigue damage in layered ceramic structures. J Dent Res 2007; 86: 1046-1050.

10.1016/j.dental.2006.09.003

12) Kanno T, Milleding P, Wennerberg A. Topography, microhardness, and precision of fit on ready-made zirconia abutment before/after sintering process. Clin Implant Dent Relat Res 2007; 9: 156-165.

10.4012/dmj.26.766

14) Raigrodski AJ, Chiche G J, Potiket N, Hochstedler JL, Mohamed SE, Billiot S, Mercante DE. The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study. J Prosthet Dent 2006; 96: 237-244.

15) Sailer I, Feher A, Filser F, Gauckler LJ, Luthy H, Hammerle CHF. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prosthodont 2007; 20: 383-388.

16) Iwata T. Studies on physical properties of porcelain fused to metal — the effect of final fusing temperature. Shigaku 1980; 2: 58-62.

17) Williamson RT, Kovarik RE, Mitchell RJ. Effects of grinding, polishing, and overglazing on the flexure strength of a high-leucite feldspathic porcelain. Int J Prosthodont 1996; 9: 30-37.

18) Ohnuki Y. Mechanical properties of low-fusing porcelains for multi-purpose gold alloys. J J Dent Mater 1997; 16: 27-37.

19) Oilo G. Flexural strength and internal defects of some dental porcelains. Acta Odontol Scand 1988; 46: 313-322.

20) Kimura H, Horng CJ, Okazaki M, Takahashi J. Oxidation effects on porcelain-titanium interface reactions and bond strength. Dent Mater 1990; 9: 91-99.

10.1016/j.jdent.2007.07.008

22) Anusavice KJ, Phillips RW. Phillips' science of dental materials, 11<SUP>th</SUP> ed, Saunders, St. Louis, MI, 2003, pp.676-678.

10.1016/j.dental.2005.11.014

24) Tinschert J, Natt G, Mautsch W, Augthun M, Spiekermann H. Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study. Int J Prosthodont 2001; 14: 231-238.

25) Ban S. Ceramics in dental crown restoration and their properties. Ceramics 2008; 43: 303-307.

26) Aboushelib MN, de Jager N, Kleverlaan CJ, Feilzer AJ. Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems. Dent Mater 2007; 23: 952-959.

27) Att W, Stamouli K, Gerds T, Strub JR. Fracture resistance of different zirconium dioxide three-unit all-ceramic fixed partial dentures. Acta Odontol Scand 2007; 65: 14-21.

28) Kim B, Zhang Y, Pines M, Thompson VP. Fracture of porcelain-veneered structures in fatigue. J Dent Res 2007; 86: 142-146.

29) Tsalouchou E, Cattell MJ, Knowles JC, Pittayachawan P, McDonald A. Fatigue and fracture properties of yttria partially stabilized zirconia crown systems. Dent Mater 2008; 24: 308-318.

30) Hjerppe J, Narhi T, Froberg KAJ, Vallittu PK, Lassila LVJ. Effect of shading the zirconia framework on biaxial strength and surface microhardness. Acta Odontol Scand 2008; 66: 262-267.

10.1016/j.dental.2005.11.035

32) Hjerppe J, Vallittu PK, Froberg K, Lassila LVJ. Effect of sintering time on biaxial strength of zirconium dioxide. Dent Mater 2009; 25: 166-171.