Strengthening of Ti3AlC2 by incorporation of Al2O3

Scripta Materialia - Tập 50 - Trang 897-901 - 2004
J.X. Chen1, Y.C. Zhou1
1High-Performance Ceramic Division, Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang 110016, PR China

Tài liệu tham khảo

Pietzka, 1994, J. Phase Equilib., 15, 392, 10.1007/BF02647559 Tzenov, 2000, J. Am. Ceram. Soc., 83, 825, 10.1111/j.1151-2916.2000.tb01281.x Finkel, 2000, J. Appl. Phys., 87, 1701, 10.1063/1.372080 Barsoum, 2000, Phys. Rev. B, 62, 10194, 10.1103/PhysRevB.62.10194 Zhou, 2001, J. Phys: Condens. Matter, 13, 10001, 10.1088/0953-8984/13/44/313 Zhou, 2001, J. Mater. Chem., 11, 2335, 10.1039/b101520f Zhou, 2002, Acta Mater., 50, 3141, 10.1016/S1359-6454(01)00353-6 Barsoum, 2001, J. Electrochem. Soc., 148, C551, 10.1149/1.1380256 Wang, 2003, Corros. Sci., 45, 891, 10.1016/S0010-938X(02)00177-4 Tong, 1995, J. Mater. Sci., 30, 3087, 10.1007/BF01209221 Radhakrishnan, 1996, Scr. Mater., 34, 1809, 10.1016/1359-6462(95)00663-X Luo, 2002, Key Engr. Mater., 224–226, 347, 10.4028/www.scientific.net/KEM.224-226.347 Luo, 2002, J. Am. Ceram Soc., 85, 3099, 10.1111/j.1151-2916.2002.tb00589.x Wang, 2002, Ceram. Int., 28, 931, 10.1016/S0272-8842(02)00076-7 Zhou, 1998, Mater. Res. Innovat., 2, 142, 10.1007/s100190050076 Wang, 2002, Z. Metalkd., 93, 66, 10.3139/146.020066 Wang, 2002, J. Mater. Chem., 12, 455, 10.1039/b108685e El-Raghy, 1997, J. Am. Ceram Soc., 80, 513, 10.1111/j.1151-2916.1997.tb02861.x Bao, 2004, J. Eur. Ceram Soc., 24, 8551, 10.1016/S0955-2219(03)00328-5 Selsing, 1961, J. Am. Ceram. Soc., 44, 419, 10.1111/j.1151-2916.1961.tb15475.x Nihara, 1991, J. Ceram. Soc. Jpn., 99, 974, 10.2109/jcersj.99.974 Nihara, 1991