Reductive Leaching of Low-Grade Pyrolusite with Formic Acid

Metallurgical and Materials Transactions B - Tập 46 - Trang 1709-1715 - 2015
Youzhi Lu1, Huaju Ma2, Runjun Huang2, Aiqun Yuan1, Zengwei Huang1, Zeguang Zhou1
1School of Chemistry and Chemical Engineering, Guangxi University for Nationalities, Nanning, P.R. China
2Guilin University of Technology at Nanning, Nanning, P.R. China

Tóm tắt

The extraction of manganese from low-grade pyrolusite is investigated using formic acid as reductant in sulfuric acid medium. The effects of volumes of formic acid, concentration of sulfuric acid, liquid to solid ratio (L/S), leaching time, and temperature on leaching efficiency of manganese, iron, and aluminum are valuated with single-factor experiments. The results show that the leaching efficiency of manganese reached 90.08 pct with 80.70 pct of iron and 31.55 pct of aluminum under the optical conditions: 15 pct H2SO4(v/v) 60 ml, 4 ml formic acid, and 2 hours leaching time at 363 K (90 °C).

Tài liệu tham khảo

YL Feng, ZL Cai, HR Li, ZW Du, XW Liu (2013) Int. J. Miner. Metall. Mater, 20(8):221–27. H.F. Su, Y X. Wen, F. Wang, Y.Y. Sun, and Z.F. Tong, Hydrometallurgy, 2008, vol.93(3-4), pp. 136-39. Z.L. Cai, Y.L. Feng, H.R. Li, X.W. Liu, and Z.C. Yang, JOM, 2012, vol.64(11), pp. 1296-304. S.B. Kanungo, Hydrometallurgy,1999, vol.52(3), pp. 313-30. Kanungo, S.B., Hydrometallurgy,1999, vol.52(3), pp. 331-47. J.M.M. Paixao, J.C. Amaral, L.E. Memoria, L.R. Freitas, Hydrometallurgy, 1995, vol.39(1-3), pp. 215-22. Y.B. Zhang, Z.X. You, G.H. Li, T. Jiang, Hydrometallurgy, 2013, vol.133, pp. 126-32. T.J.W. De Bruijn, T.H. Soerawidjaja, W.A. De Jongt, P.J. Van Den Berg (1980) Chem. Eng. Sci, 35(7):1591-99. J.J. Song, G.C. Zhu, P. Zhang, and Y.N. Zhao, Acta Metall. Sin., 2010, vol. 23(3), pp. 223-29. Z. Cheng, G.C. Zhu, and Y.N. Zhao, Hydrometallurgy, 2009, vol.96(1-2), pp. 176-79. Y.H. Zhou, H. Yao, Y.F. Long, J. Su, J. Liu, X.H. Zhou, T. Gan, Z.M. Lei, Y.X. Wen, Chinese Journal of Process Engineering, 2013, vol. 13(6), pp. 946-51. (in Chinese) Y.L. Feng, Z.L. Cai, H.R. Li, Z.W. Du, X.W. Liu, J. Min. Metal. Sect. B-Metall, 2013, vol. 49(1), pp. 33-41. A.A. Baba, L. Ibrahim, F.A. Adekola, R.B. Bale, M.K. Ghosh, A.R. Sheik, S.R. Pradhan, O.S. Ayanda, I.O. Folorunsho, Journal of minerals and materials characterization and engineering, 2014, vol.2(3), pp. 230-47. M. Trifoni, F. Vegliò, G. Taglieri, L. Toro, Miner. Eng, 2000, vol. 13(2), pp. 217-21. F. Vegliò, M. Trifoni, L. Toro (2001) Ind. Eng. Chem. Res, 40(18):3895-901. F. Pagnanelli, G. Furlani, P. Valentini, F. Vegliò, L.Toro, Hydrometallurgy, 2004, vol.75(1-4), pp. 157-67. F. Beolchini, M. Papini Petrangeli, L. Toro, M. Trifoni, and F. Vegliò: Miner. Eng., 2001, vol. 14 (2), pp. 175–84. F.F. Wu, H. Zhong, S. Wang, S.F. Lai, J. Cent. South Univ, 2014, vol.21(5), pp. 1763-70. F.W.Y. Momade, Z.G. Momade, Hydrometallurgy, 1999, vol.51(1), pp. 103-113. A.G. Kholmogorov, A.M. Zhyzhaev, Hydrometallurgy, 2000, vol.56(1), pp. 1-11. M.N. El Hazek, T.A Lasheen, and A.S. Helal: Hydrometallurgy, 2006, vol.84(3), pp. 187-91. W.Y. Sun, S.J. Su, Q.Y. Wang, S.L. Ding, Hydrometallurgy, 2013, vol. 133, pp. 118-25. T.A. Lasheen, M.N. El Hazek, A.S. Helal, Hydrometallurgy, 2009, vol. 98(3-4), pp. 314-17. H.F. Su, H.K. Liu, F. Wang, X.Y. Lv, Y.X. Wen, Chinese Journal of Chemical Engineering, 2010, vol. 18(5), pp. 730-35. D. Hariprasad, B. Dash, M.K. Ghosh, S. Anand, Miner. Eng, 2007, vol. 20(14), pp. 1293-95. X.K. Tian, X.X. Wen, C. Yang, Y.J. Liang, Z.B. Pi, Y.X. Wang, Hydrometallurgy, 2010, vol. 100(3-4), pp. 157-60. D. Hariprasad, M.K. Ghosh and S. Anand, Transactions of The Indian Institute of Metals, 2009, vol. 62(6), pp. 551-54. Q. Tang, H. Zhong, S. Wang, J.Z. Li, G.Y. Liu, Trans. Nonferrous Met. Soc. China, 2009, vol. 24(3), pp. 861-67.