Propoxylated Fatty Esters as Safe Inhibitors for Corrosion of Zinc in Hydrochloric Acid

Pleiades Publishing Ltd - Tập 56 - Trang 225-232 - 2020
M. Alfakeer1, M. Abdallah2,3, R. S. Abdel Hameed4,5
1Department of Chemistry, Faculty of Science, Princess Nourah bint Abdulrahman University Riyadh, Riyadh, Saudi Arabia
2Department of Chemistry, Faculty of Science, Benha University, Benha, Egypt.
3Department of Chemistry, Faculty of Applied Sciences, Umm Al-Qura University, Makkah, Saudi Arabia
4Department of Chemistry, Faculty of Science, Al-Azhar University, Cairo, Egypt
5Department of Basic Science, Preparatory Year, Hail University, Hail, Saudi Arabia

Tóm tắt

The inhibiting action of nonionic surfactants, namely, propoxylated fatty esters (PFE) with different number of propylene oxide toward the corrosion of Zn in 0.1 M HCl solutions was investigated. Four techniques were used in this study such as weight loss, galvanostatic polarization, potentiodynamic anodic polarization and electrochemical impedance spectroscopy. The inhibition efficiency of PFE compounds increases by increasing the concentrations of PFE, number of propylene oxide unit and with lowering temperature. The inhibition was interpreted by adsorption of PFE molecules on the Zn surface according Temkin’s isotherm. Galvanstatic polarization indicated that the PFE acts as a mixed type inhibitor. PFE molecules inhibit the pitting corrosion of Zn in a solution containing Cl– ions by moving the pitting potentials into a more noble direction. The activation thermodynamic parameters such as $$E_{{\text{a}}}^{*}$$, ΔH* and ΔS* are calculated and explained.

Tài liệu tham khảo

Shah, M.D., Patel, A.S., Mudaliar, G.V., and Shah, N.K., Port. Electrochim. Acta, 2011, vol. 29, p. 10. Abdallah, M., Corros. Sci., 2003, vol. 45, p. 2705. Agrawal, Y.K., Talati, J.D., Desai, M.N., and Shah, N.K., Corros. Sci., 2004, vol. 46, p. 633. Abdallah, M., El-Etre, A.Y., and Moustafa, M.F., Port. Electrochim. Acta, 2009, vol. 27, p. 615. Fouda, A.S., Abdallah, M., Atwa, S.T., and Salem, M.M., Mod. Appl. Sci., 2010, vol. 4, p. 41. Abdallah, M., Zaafarany, I., Fouda, A.S., and Abd El-Kader, D., J. Mater. Eng. Perform., 2012, vol. 21, p. 995. Saadawy, M., Int. J. Electrochem. Sci., 2018, vol. 13, pp. 9600–9617. Abdallah, M., Atwa, S.T., Salem, M.M., and Fouda, A.S., Int. J. Electrochem. Sci., 2013, vol. 8. p. 10001. Wang, L., Pu, J.X., and Luo, H., Corros. Sci., 2002, vol. 45, p. 677. Fouda, A.S., Rashwan, S., Emam, A., and El-Morsy, F.E., Int. J. Electrochem. Sci., 2018, vol. 13, p. 3719. Abdallah, M., Zaafarany, I.A., Fouda, A.S., and El-Nagar, W., J. Electrochem. Plat. Technol., 2014, vol. 2, p. 2. Popoola, A.P.I. and Fayomi, O.S.I., Int. J. Electrochem. Sci., 2011, vol. 6, p. 4581. Abdallah, M., Zaafarany, I.A., and AL Jahdaly, B.A., J.Mater. Environ. Sci., 2016, vol. 7, p. 1107. Yousif, E., Win, Y., Al-Hamadani, A.H., Al-Amiery, A.A., Kadhum, A.A., and Mohamad, A., Int. J. Electrochem. Sci., 2015, vol. 10, p. 1708. M. Abdallah, Elshafie A. M. Gad, Jabir H Al-Fahemi, and M. Sobhi // Protection of Metals and Physical Chemistry of Surfaces, 2018, Vol. 54, No. 3, pp. 503–512. https://doi.org/10.1134/S207020511803022X Abdallah, M., Hazazi, O.A., Fouda, A.S., and Abdel-Fatah, A., Prot. Met. Phys. Chem. Surf., 2015, vol. 51, p. 473. Abdallah, M., Hegazy, M.A., Alfakeer, M., and Ahmed, H., Green Chem. Lett. Rev., 2018, vol. 11, p. 457. Fawzy, A., Zaafarany, I.A., Ali, H.M., and Abdallah, M., Int. J. Electrochem. Sci., 2018, vol. 13, p. 4575. Fawzy, A., Abdallah, M., Zaafarany, I.A., Ahmed, S.A., and Althagafi, I.I., J. Mol. Liq., 2018, vol. 265, p. 276. Abdallah, M., Al Jahdaly, B.A., and Al-Malyo, O.A., Int. J. Electrochem. Sci., 2015, vol. 10, p. 2740. Abdallah, M., Al Jahdaly, B.A., Sobhi, M., and Ali, A.I., Int. J. Electrochem. Sci., 2015, vol. 10, p. 4482. Hegazy, M.A., Abdallah, M., Alfakeer, M., and Ahmed, H., Int. J. Electrochem. Sci., 2018, vol. 13, p. 6824. Sobhi, M., El-Sayed, R., and Abdallah, M., J. Surfactants Deterg., 2013, vol. 16, p. 937. Sobhi, M., El-Sayed, R., and Abdallah, M., Chem. Eng. Commun., 2016, vol. 203, p. 758. Mathur, P.B. and Vasudevan, T., Corrosion, 1982, vol. 38, p. 17. Hazazi, O.A. and Abdallah, M., Int. J. Electrochem. Sci., 2013, vol. 8, p. 8138. Graciaa, A., Barakat, Y., Schechter, R.S., Wade, W.H., and Yiv S., J. Colloid Interface Sci., 1982, vol. 89, p. 219. Sobhi, M., Abdallah, M., and Khairou, K.S., Monatsh. Chem., 2012, vol. 143, p. 1379. Laidler, K.J., Chemical Kinetics, New York: McGraw-Hill, 1965. Abdallah, M., Salem, M.M., AL Jahdaly, B.A., Awad-E. Helal, M.I., and Fouda, A.S., Int. J. Electrochem. Sci., 2017, vol. 12. p. 4543. Abdallah, M., Fouda, A.S., El-Nagar, D.A.M., and Ghoneim, M.M., Prot. Met. Phys. Chem. Surf., 2018, vol. 54, p. 1204. Bayol, E., Kayakirilmaz, K., and Erbil, M., Mater. Chem. Phys., 2007, vol. 104, p. 74. Benali, O., Larabi, L., Traisnel, M., Gengembre, L., and Harek, Y., Appl. Surf. Sci., 2007, vol. 253, p. 6130. Abdallah, M., Al-Karane, S.A., and Fattah, A.A.A., Prot. Met. Phys. Chem. Surf., 2009, vol. 50, p. 205. Hameed, R.S.A. and Abdallah, M., Prot. Met. Phys. Chem. Surf., 2018, vol. 54, p. 113. Abdallah, M., Altass, H.M., AL-Jahdaly, B.A., and Salem, M.M., Green Chem. Lett. Rev., 2018, vol. 11, p. 189. Abdallah, M., AL-Jahdaly, B.A., Salem, M.M., Fawzy, A., and Fattah, A.A.A., J.Mater. Environ. Sci., 2017, vol. 8, p. 2599. Putilova, I., Balezin, S., and Barannik, V., Metallic Corrosion Inhibitors, Oxford: Pergamon, 1960. Temkin, M.I., Zh. Fiz. Khim., 1941, vol. 15, p. 296. Fouda, A.S., Abdallah, M., Al-Ashry, S.M., and Fattah, A.A.A., Desalination, 2010, vol. 250, p. 538. Tedeschi, X.R.J., Corrosion, 1975, vol. 31, p.130. Zaafarany, I. and Abdallah, M., Int. J. Electrochem. Sci., 2010, vol. 5, p. 18.