Post electron-beam irradiation oxidation of orthopaedic UHMWPE

Polymer Degradation and Stability - Tập 93 Số 9 - Trang 1695-1703 - 2008
L. Costa1, I. Carpentieri1, Pierangiola Bracco1
1Dipartimento di Chimica IFM and NIS-Centre of Excellence, University of Torino, Via Giuria 7, 10125 Torino, Italy

Tóm tắt

Từ khóa


Tài liệu tham khảo

Kurtz, 1999, Advances in the processing, sterilization and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplasty, Biomaterials, 20, 1639, 10.1016/S0142-9612(99)00053-8

Costa, 1998, Oxidation in orthopaedic UHMWPE sterilized by gamma-radiation and ethylene oxide, Biomaterials, 19, 659, 10.1016/S0142-9612(97)00160-9

Kurtz, 2004

Bracco, 2006, Oxidation behaviour in prosthetic UHMWPE components sterilised with high energy radiation in a low oxygen environment, Polym Degrad Stab, 91, 2030, 10.1016/j.polymdegradstab.2006.02.003

Costa, 2006, A survey of oxidation and oxidation potential in contemporary packaging for polyethylene total joint replacement components, J Biomed Mater Res B: Appl Biomater, 78B, 20, 10.1002/jbm.b.30454

Bracco, 2006, Oxidation behaviour in prosthetic UHMWPE components sterilised with high energy radiation in the presence of oxygen, Polym Degrad Stab, 91, 3057, 10.1016/j.polymdegradstab.2006.08.002

Lacoste, 1992, Gamma-, photo-, and thermally-initiated oxidation of linear low density polyethylene: a quantitative comparison of oxidation products, J Polym Sci Part A: Polym Chem, 30, 493, 10.1002/pola.1992.080300316

Mallégol, 2001, Post-γ-irradiation reactions in vitamin E stabilised and unstabilised HDPE, Nucl Instrum Methods Phys Res B, 85, 283, 10.1016/S0168-583X(01)00944-2

Mallégol, 2001, A comparison of phenolic antioxidant performance in HDPE at 32–80°C, Polym Degrad Stab, 73, 259, 10.1016/S0141-3910(01)00086-6

Mallégol, 2001, Antioxidant effectiveness of vitamin E in HDPE and tetradecane at 32°C, Polym Degrad Stab, 73, 269, 10.1016/S0141-3910(01)00087-8

Rimnac, 1994, Post-irradiation aging of ultra-high molecular weight polyethylene, J Bone Joint Surg Am, 76, 1052, 10.2106/00004623-199407000-00014

Kurtz, 2005, In vivo degradation of polyethylene liners after gamma sterilization in air, J Bone Joint Surg Am, 87, 815, 10.2106/JBJS.D.02111

Costa, 2000

Brunella, 2007, Lifetime of alkyl macroradicals in irradiated UHMWPE, Polym Degrad Stab, 92, 1498, 10.1016/j.polymdegradstab.2007.05.005

Jahan, 1999, Radiation-sterilization and subsequent oxidation of medical grade polyethylene: an ESR study, Nucl Instrum Methods Phys Res B, 151, 207, 10.1016/S0168-583X(99)00083-X

Jacobson, 2001, Effects of microtoming on oxidation of ultra high molecular weight polyethylene, Polym Degrad Stab, 73, 141, 10.1016/S0141-3910(01)00080-5

De Kock, 1964, Infrared determination of unsaturation in polyethylene, J Polym Sci Polym Lett, 2, 339, 10.1002/pol.1964.110020405

Costa, 2001, Effects of microtomy on the material properties of ultra high molecular weight polyethylene, Polym Test, 20, 649, 10.1016/S0142-9418(00)00088-X

Costa L, Bracco P. Mechanism of crosslinking and oxidative degradation of UHMWPE [chapter 11]. pp. 235–50 in Ref. 3.

Ohnishi, 1961, Electron spin resonance studies of irradiated polymers. I. Factors affecting the electron spin resonance spectra of irradiated polymers, Polymer, 2, 119, 10.1016/0032-3861(61)90017-9

Ohnishi, 1963, Electron spin resonance study of radiation oxidation of polymers. IIIA. Results for polyethylene and some general remarks, J Polym Sci Part A: Polym Chem, 1, 605

Igarashi, 1983, Free radical identification by ESR in polyethylene and nylon, J Polym Sci: Polym Chem Ed, 21, 2405, 10.1002/pol.1983.170210824

Lin-Vien, 1991

2004

Hummel, 1988

2007

Durant, 2005, EPR power saturation techniques and spectral differentiation are used to isolate and simulate radical species in UHMWPE, Nucl Instrum Methods Phys Res B, 236, 160, 10.1016/j.nimb.2005.04.011

Alam, 2004, γ-Irradiation of ultra-high-molecular weight polyethylene: electron paramagnetic resonance and nuclear magnetic resonance spectroscopy and imaging studies of the mechanism of subsurface oxidation, J Polym Sci Part A: Polym Chem, 42, 5929, 10.1002/pola.20415

Bolland, 1949, Kinetics of olefin oxidation, Quart Rev Chem Soc, 3, 1, 10.1039/qr9490300001

Pauly, 1999, Permeability and diffusion data

Pratt, 2003, Role of hyperconjugation in determining carbon–oxygen bond dissociation enthalpies in alkylperoxyl radicals, J Am Chem Soc, 125, 5801, 10.1021/ja034182j

Mowery, 2005, Solid-state 13C NMR investigation of the oxidative degradation of selectively labeled polypropylene by thermal ageing and γ-irradiation, Macromolecules, 38, 5035, 10.1021/ma047381b

Rivaton, 2004, Influence of the structure on the γ-irradiation of polypropylene and on the post-irradiation effects, Nucl Instrum Methods Phys Res B, 222, 187, 10.1016/j.nimb.2004.02.012

Ivanov, 1992

Barabas K, Iring M, Kelen T, Tudos F. Study of the thermal oxidation of polyolefines. V. Volatile products in the thermal oxidation of polyethylene. In: 15th IUPAC microsymposium on macromolecules: degradation and stability of polyolefines; 1977; 57:65-71.

Lazar, 1989

Costa, 1997, Ultra high molecular weight polyethylene: II. Thermal- and photo-oxidation, Polym Degrad Stab, 58, 41, 10.1016/S0141-3910(97)00010-4