Pitting and galvanic corrosion behavior of laser-welded stainless steels
Tài liệu tham khảo
J. Mazumder, Laser beam welding, ASM Handbook, vol. 6, 10th ed., Welding, Brazing, and Soldering, ASM International, Materials Park, OH, USA, 1990, pp. 263–268.
Schuocker, 1999, Welding with lasers
Gluszek, 1992, Galvanic coupling of 316L steel with titanium, niobium, and tantalum in Ringer's solution, Br. Corros. J., 27, 135, 10.1179/bcj.1992.27.2.135
Reclaru, 2002, Pitting, crevice and galvanic corrosion of REX stainless-steel/CoCr orthopedic implant material, Biomaterials, 23, 3479, 10.1016/S0142-9612(02)00055-8
Shih, 2005, Galvanic current induced by heterogeneous structures on stainless steel wire, Corros. Sci., 47, 2199, 10.1016/j.corsci.2004.09.017
Blasco-Tamarit, 2006, Effect of aqueous LiBr solutions on the corrosion resistance and galvanic corrosion of an austenitic stainless steel in its welded and non-welded condition, Corros. Sci., 48, 863, 10.1016/j.corsci.2005.02.028
Vilpas, 1999
Cullity, 1978
ASTM Standard E975-03, Standard Practice for X-Ray Determination of Retained Austenite in Steel with Near Random Crystallographic Orientation, ASTM International, Philadelphia, 2003.
Jatczak, 1980
ASTM Standard G61-94, Standard Method for Conducting Cyclic Potentiodynamic Polarisation Measurements for Localised Corrosion Susceptibility of Iron-, Nickel-, or Cobalt-Based Alloys, Annual Book of ASTM Standards, ASTM International, Philadelphia, 1994.
ASTM Standard G71-81, Conducting and Evaluating Galvanic Tests in Electrolytes, Annual Book of ASTM Standards, ASTM International, Philadelphia, 1992.
D.N. Noble, Selection of wrought duplex stainless steels, ASM Handbook, vol. 6, 10th ed., Welding, Brazing, and Soldering, ASM International, Materials Park, OH, USA, 1990, pp. 471–481.
Robinson, 1995, CO2 laser welding of duplex and super-duplex stainless steels (the effect of argon–nitrogen assist gas mixtures), 499
McPherson, 2003, Steel microstructure in autogenous laser welds, J. Laser Appl., 15, 200, 10.2351/1.1619997
Muthupandi, 2003, Corrosion behavior of duplex stainless steel weld metals with nitrogen additions, Corros. Sci. Technol., 38, 303, 10.1179/147842203225008895
McPherson, 2003, Submerged arc welding of stainless steel and the challenge from the laser welding process, J. Mater. Process. Technol., 134, 174, 10.1016/S0924-0136(02)00466-1
Li, 1997, Localized corrosion of laser surface cladded UNS S31254 superaustenitic stainless steel on mild steel, Surf. Coat. Technol., 88, 90, 10.1016/S0257-8972(96)02865-4
Li, 1997, Localized corrosion performance of laser surface cladded UNS S44700 superferritic stainless steel on mild steel, Surf. Coat. Technol., 88, 96, 10.1016/S0257-8972(96)02895-2
Kwok, 1998, Cavitation erosion and pitting corrosion of laser surface melted stainless steels, Surf. Coat. Technol., 99, 295, 10.1016/S0257-8972(97)00624-5
McCafferty, 1986, Electrochemical behavior of laser-processed metal surfaces, J. Electrochem. Soc., 133, 1090, 10.1149/1.2108792
Akgun, 1992, Desensitization of sensitized 304 stainless steel by laser surface melting, J. Mater. Sci., 30, 2147, 10.1007/BF01117929
Carbucicchio, 1998, Improvement of surface properties of AISI 304 stainless steel by laser melting, Hyperfine Interact., 112, 19, 10.1023/A:1011007820797
Carboni, 2002, Influence of high power diode laser surface melting on the pitting corrosion resistance of type 316L stainless steel, J. Mater. Sci., 37, 3715, 10.1023/A:1016569527098
Pan, 1998, The improvement of localized corrosion resistance in sensitized stainless steel by laser surface remelting, Surf. Coat. Technol., 102, 245, 10.1016/S0257-8972(98)00358-2
Gooch, 1996, Corrosion behavior of welded stainless steel, Weld. J., 75, 135s
David, 2003, Welding: solidification and microstructure, JOM, 55, 14, 10.1007/s11837-003-0134-7
Suutala, 1983, Effect of solidification condition on the solidification mode in austenitic stainless steels, Metall. Trans. A, 14, 191, 10.1007/BF02651615
Cieslak, 1981, Pitting corrosion of stainless steel weldments, 361
A. Wahid, D.L. Olson, D.K. Matlock, Corrosion of weldments, ASM Handbook, vol. 6, 10th ed., Welding, Brazing, and Soldering, ASM International, Materials Park, OH, USA, 1990, pp. 1065–1069.
Hack, 1995, Galvanic corrosion, 186