Phase behavior and a modified Kwei equation for ternary polymer blends containing stereoregular PMMA

Thermochimica Acta - Tập 441 - Trang 137-143 - 2006
Wen-Ping Hsu1
1Department of Chemical Engineering, National United University, 1, Lien-Da, Kung-Ching Li, Miao-Li 36003, Taiwan, Republic of China

Tài liệu tham khảo

Kwei, 1977, Macromolecules, 10, 157, 10.1021/ma60055a032 Wang, 1981, Polym. Eng. Sci., 21, 47, 10.1002/pen.760210108 Rigby, 1985, Macromolecules, 18, 2269, 10.1021/ma00153a036 Shah, 1986, J. Appl. Polym. Sci., 32, 3863, 10.1002/app.1986.070320306 Equizabal, 1986, J. Appl. Polym. Sci., 32, 5945, 10.1002/app.1986.070320723 Goh, 1986, Thermochim. Acta, 105, 191, 10.1016/0040-6031(86)85235-2 Goh, 1986, Thermochim. Acta, 102, 281, 10.1016/0040-6031(86)85336-9 Christiansen, 1987, J. Appl. Polym. Sci., 34, 537, 10.1002/app.1987.070340209 Zhang, 1994, Polymer, 35, 5379, 10.1016/S0032-3861(05)80001-1 Hsu, 2002, J. Appl. Polym. Sci., 83, 1425, 10.1002/app.2303 Hsu, 2004, J. Appl. Polym. Sci., 91, 35, 10.1002/app.13147 Hsu, 2004, J. Appl. Polym. Sci., 92, 2797, 10.1002/app.20293 Fox, 1956, J. Appl. Bull. Am. Phys. Soc., 1, 123 Kwei, 1984, J. Polym. Sci. Polym. Lett. Ed., 22, 306, 10.1002/pol.1984.130220603 Pomposo, 1994, Macromolecules, 27, 252, 10.1021/ma00079a038 Brekner, 1988, Polymer, 29, 78, 10.1016/0032-3861(88)90203-0