Oxidation induced phase transformation of duplex stainless steel 25Cr–10Mn–2Ni–3Mo–0.8W–0.8Cu–0.5N

Corrosion Science - Tập 55 - Trang 233-237 - 2012
Yulai Xu1, Qiumin Jin1, Jun Li1, Xueshan Xiao1, Xin Zhang2, Laizhu Jiang2
1Laboratory for Microstructures, Institute of Materials, Shanghai University, Shanghai 200072, China
2Baoshan Iron & Steel Co., Ltd., Shanghai 200431, China

Tài liệu tham khảo

Momeni, 2011, Mater. Sci. Eng. A, 528, 1448, 10.1016/j.msea.2010.11.020 Li, 2011, Mater. Des., 32, 2199, 10.1016/j.matdes.2010.11.021 Vesel, 2008, Vacuum, 82, 228, 10.1016/j.vacuum.2007.07.014 Vesel, 2008, Appl. Surf. Sci., 255, 1759, 10.1016/j.apsusc.2008.06.017 Wu, 2010, Corros. Sci., 52, 1003, 10.1016/j.corsci.2009.11.025 Goutier, 2010, Corros. Sci., 52, 2403, 10.1016/j.corsci.2010.03.022 Peng, 2005, Acta Mater., 53, 5079, 10.1016/j.actamat.2005.07.019 Li, 2005, Corros. Sci., 47, 57, 10.1016/j.corsci.2004.05.008 Jepson, 2009, Corros. Sci., 51, 588, 10.1016/j.corsci.2008.11.023 Donik, 2009, Corros. Sci., 51, 827, 10.1016/j.corsci.2009.01.021 Douglass, 1970, Oxid. Met., 2, 207, 10.1007/BF00603657 Jian, 2006, J. Power Sources, 158, 354, 10.1016/j.jpowsour.2005.09.056 Xu, 2000, Intermetallics, 8, 769, 10.1016/S0966-9795(00)00007-8 Jin, 2010, Corros. Sci., 52, 2846, 10.1016/j.corsci.2010.04.033 Duh, 1989, J. Electrochem. Soc., 136, 847, 10.1149/1.2096755 Wild, 1977, Corros. Sci., 17, 95, 10.1016/0010-938X(77)90011-7 Beattie, 1970, J. Chem. Soc. A, 980, 10.1039/j19700000980 Ramesh, 2008, Catal. Today, 131, 477, 10.1016/j.cattod.2007.10.061 Verble, 1974, Phys. Rev. B, 9, 5236, 10.1103/PhysRevB.9.5236 Douglass, 1986, Oxid. Met., 25, 235, 10.1007/BF00655899