Novel and efficient purification of silicon through ultrasonic-Cu catalyzed chemical leaching
Tài liệu tham khảo
Ni, 2014, Modeling and simulation of silicon epitaxial growth in Siemens CVD reactor, J. Cryst. Growth, 404, 89, 10.1016/j.jcrysgro.2014.07.006
Ding, 2012, Boron removal from metallurgical-grade silicon using lithium containing slag, J. Non-Cryst. Solids, 358, 2708, 10.1016/j.jnoncrysol.2012.06.031
Tan, 2014, Removal of aluminum and calcium in multicrystalline silicon by vacuum induction melting and directional solidification, Vacuum, 99, 272, 10.1016/j.vacuum.2013.06.015
Sun, 2013, Purification of metallurgical-grade silicon via acid leaching, calcination and quenching before boron complexation, Hydrometallurgy, 139, 64, 10.1016/j.hydromet.2013.07.002
Khalifa, 2012, Purification of silicon powder by the formation of thin porous layer followed byphoto-thermal annealing, Nanoscale Res. Lett., 7, 1, 10.1186/1556-276X-7-444
Xi, 2018, Removal of impurities from metallurgical grade silicon with metal assisted chemical leaching, Hydrometallurgy, 178, 250, 10.1016/j.hydromet.2018.05.013
Swamy, 2005, Bioleaching with ultrasound, Ultrason. Sonochem., 12, 301, 10.1016/j.ultsonch.2004.01.035
Anjum, 2010, Enhanced bioleaching of metals from black shale using ultrasonics, Hydrometallurgy, 100, 122, 10.1016/j.hydromet.2009.10.016
Xia, 2012, Iron removal from kaolin using thiourea assisted by ultrasonic wave, Ultrason. Sonochem., 19, 38, 10.1016/j.ultsonch.2011.05.008
Zhao, 2007, Removal of iron from silica sand by surface cleaning using power ultrasound, Miner. Eng., 20, 816, 10.1016/j.mineng.2006.10.005
Trumbore, 1960, Solid solubilities of impurity elements in germanium and silicon, Bell Labs Tech. J., 39, 205, 10.1002/j.1538-7305.1960.tb03928.x
Meteleva-Fischer, 2012, Microstructure of metallurgical grade silicon during alloying refining with calcium, Intermetallics, 25, 9, 10.1016/j.intermet.2012.02.009
Milanese, 2002, Reactive diffusion in the system vanadium–silicon, Acta Mater., 50, 1393, 10.1016/S1359-6454(01)00445-1
Franti, 1977, On the equilibrium silicide in beta Ti-V alloys containing Si, Metall. Mater. Trans. A, 8, 1639, 10.1007/BF02644871
Wang, 2017, Micro-structured inverted pyramid texturization of Si inspired by self-assembled Cu nanoparticles, Nanoscale, 9, 907, 10.1039/C6NR08126F
Lai, 2016, Enhanced acid leaching of metallurgical grade silicon in hydrofluoric acid containing hydrogen peroxide as oxidizing agent, Hydrometallurgy, 164, 103, 10.1016/j.hydromet.2016.06.003
Huang, 2011, Metal-assisted chemical etching of silicon: a review, Adv. Mater., 23, 285, 10.1002/adma.201001784
Li, 2000, Metal-assisted chemical etching in HF/H2O2 produces porous silicon, Appl. Phys. Lett., 77, 2572, 10.1063/1.1319191
Xi, 2018, Simple and high-effective purification of metallurgical-grade silicon through cu-catalyzed chemical leaching, JOM, 70, 2041, 10.1007/s11837-018-3058-y
Yusuf, 2001, Adewuyi, Sonochemistry: environmental science and engineering applications, Ind. Eng. Chem. Res., 40, 4681, 10.1021/ie010096l
Li, 2014, Recovery of valuable metals from spent lithium-ion batteries by ultrasonic-assisted leaching process, J. Power Sources, 262, 380, 10.1016/j.jpowsour.2014.04.013
Ma, 2009, Hydrometallurgical purification of metallurgical grade silicon, Rare Met., 28, 221, 10.1007/s12598-009-0043-1
Hajji, 2007, Electrical properties of purified solar grade silicon substrates using a combination of porous silicon and SiCl4, Appl. Surf. Sci., 253, 5341, 10.1016/j.apsusc.2006.12.006
Zhang, 2011, Effect of heating treatment on the resistivity of polycrystalline silicon, Mater. Sci. Forum, 675–677, 113
Lin, 2004, Effects of rapid thermal processing on oxygen precipitation in czochralski silicon wafer, Semicond. Sci. Tech., 19, 630, 10.1088/0268-1242/19/5/012
Araki, 2015, Impact of rapid thermal oxidation at ultrahigh-temperatures on oxygen precipitation behavior in Czochralski-Silicon crystals III, ECS Solid State Lett., 4, 63, 10.1149/2.0071508ssl