Modelling of the effects of welding conditions on dilution of stainless steel claddings produced by gas metal arc welding procedures

Journal of Materials Processing Technology - Tập 196 - Trang 339-344 - 2008
A.S. Shahi1, Sunil Pandey2
1Department of Mechanical Engineering, SLIET, Longowal, Punjab 148106, India
2Department of Mechanical Engineering, Indian Institute of Technology Delhi, New Delhi, 110016, India

Tài liệu tham khảo

Benyounis, 2005, Optimizing the laser-welded butt joints of medium carbon steel using RSM, J. Mater. Process. Technol., 164–165, 986, 10.1016/j.jmatprotec.2005.02.067 Cochran, 1957 Douglas, 1984 Halmøy, 1979, Wire melting rate, droplet temperature and effective anode potential, 49 Harris, 1986, TIG hot wire offers high quality, high deposition, Metal Construct., 445 Huismann, 1999, Sensing metal inert gas process by measuring wire feed rate and current, Sci. Technol. Weld. Joining, 4, 352, 10.1179/136217199101537996 Kim, 2002, Modelling and optimization of GMA welding process by genetic algorithm and response surface methodology, Int. J. Prod. Res., 40, 1611, 10.1080/00207540110119964 Mallaya, 1993, Effect of magnetic steering of the arc on clad quality in submerged arc strip cladding, Weld. J., 289s Modensi, 2005, Wire melting rate phenomena in gas metal arc welding, Sci. Technol. Weld. Joining, 10, 120 Murugan, 1997, Stainless steel cladding deposited by automatic gas metal arc welding, Weld. J., 391s Ramazan, 2004, An investigation on the explosive cladding of 316L stainless steel-din-P355 GH steel, J. Mater. Process. Technol., 91 Oh, 1990, Low-dilution electroslag cladding for shipbuilding, Weld. J., 37 Pandey, 1999, Development of advanced gas metal arc welding process, 12 Shahi, 2006, Welding current prediction in GMAW and UGMAW process using response surface methodology, Sci. Technol. Weld. Joining, 11, 341, 10.1179/174329306X113253 Stol, 1985, Advanced gas metal arc welding process, 493 Suban, 2001, Dependence of melting rate in MIG/MAG welding on the type of shielding gas used, J. Mater. Process. Technol., 119, 15, 10.1016/S0924-0136(01)00940-2 Waszink, 1982, Heat generation and heat flow in the filler metal in GMA welding, Weld. J., 269s