Modelling flow and work hardening behaviour of cold worked Zr–2.5Nb pressure tube material in the temperature range of 30–600̊C

Nuclear Engineering and Design - Tập 269 - Trang 52-56 - 2014
A.K. Dureja1, S.K. Sinha1, D.N. Pawaskar2, P. Seshu2, J.K. Chakravartty3, R.K. Sinha4
1Reactor Design and Development Group, Bhabha Atomic Research Centre, Trombay, Mumbai, India
2Department of Mechanical Engineering, Indian Institute of Technology Bombay, Mumbai, India
3Mechanical Metallurgy Division, Bhabha Atomic Research Centre, Trombay, Mumbai, India
4Department of Atomic Energy, Anushakti-Bhavan, Near Gateway of India, Mumbai, India

Tài liệu tham khảo

Choudhary, 2001, Mater. Sci. Technol., 17, 223, 10.1179/026708301101509890 Dureja, 2011, Flow behaviour of autoclaved, 20% cold worked, Zr–2.5Nb alloy pressure tube material in the temperature range of room temperature to 800̊C, Journal of Nuclear Materials, 412, 22, 10.1016/j.jnucmat.2011.01.023 Glasston, 1988 Guimaraes, 1975, Scripta Metall., 9, 1147, 10.1016/0036-9748(75)90395-6 Hollomon, 1945, Trans. Am. Inst. Min. Metall. Eng., 162, 268 Kapoor, 1995, High-temperature mechanical behavior of cold-worked stress-relieved Zr–2.5Nb, JMEPEG, 4, 610, 10.1007/BF02649594 Kassam Zulfikar, 1992, Mater. Sci. Eng. A, 158, 185, 10.1016/0921-5093(92)90007-N Ludwigson, 1971, Metall. Trans., 2, p2825, 10.1007/BF02813258 Ludwik, 1909 Northwood, 1975, J. Nucl. Mater., 55, 299, 10.1016/0022-3115(75)90071-9 Ramberg, 1943 Singh, 2005, J. Nucl. Mater., 345, 146, 10.1016/j.jnucmat.2005.05.008 Swift, 1952, J. Mech. Phys. Solids, 1, p1, 10.1016/0022-5096(52)90002-1 Voce, 1948, J. Inst. Met., 74, 537