Microstructure evolution of a new directionally solidified Ni-based superalloy after long-term aging at 950 °C upto 1 000 h
Tài liệu tham khảo
GUO, 2008
SUN, 2001, Research and development of disc PM superalloy [J], Aviation Engineering and Maintenance, 28
ZHANG, 2002, Hot tearing of nickel-based superalloys during directional solidification [J], Acta Materialia, 50, 1869, 10.1016/S1359-6454(02)00042-3
ZHOU, 2005, Influence of solidification conditions on the castability of nickel-base superalloy IN792 [J], Metallurgical and Materials Transaction A, 36, 651, 10.1007/s11661-005-0181-5
YANG, 2010, Effects of heat treatments on the microstructure of IN792 alloy [J], Materials Science and Engineering A, 527, 1016, 10.1016/j.msea.2009.10.026
SRINIWASAN, 2004, Effect of long-time exposure on the evolution of minor phases in alloy 718 [J], Materials Science and Engineering A, 364, 27, 10.1016/j.msea.2003.06.003
LIU, 2010, Microstructural evolution in austenitic heat-resistant cast steel 35Cr25Ni12NNbRE during long-term service [J], Materials Science and Engineering A, 527, 2772, 10.1016/j.msea.2010.01.002
GUO, 2006, Microstructure properties and heat treatment process of powder metallurgy superalloy FGH95 [J], Journal of Iron and Steel Research, 13, 65, 10.1016/S1006-706X(06)60097-6
SAJJADI, 2006, Microstructure evolution of high-performance Ni-base superalloy GTD-111 with heat treatment parameters [J], Journal of Materials Processing Technology, 175, 376, 10.1016/j.jmatprotec.2005.04.021
SAFARI, 2006, On the heat treatment of Rene-80 nickel-base superalloy [J], Journal of Materials Processing Technology, 176, 240, 10.1016/j.jmatprotec.2006.03.165
GUAN, 2010, Effects of Ti on γ' phase in aging structure of Ni-based superalloy [J], Non Ferrous and Metallurgy, 26, 32
MA, 2010, Carbides of a new directional solidification superalloy DZ68 [J], Heat Treatment of Metals, 35, 10
WU, 2010, Carbides in a new type Hf-Ta-containing nickel-based superalloy powder [J], Journal of University of Science and Technology Beijing, 32, 1464
SHI, 2010, Effect of Hf content on the microstructures and stress rupture properties of DD6 single crystal superalloy [J], Rare Metal Materials and Engineering, 39, 1334, 10.1016/S1875-5372(10)60116-6
LIU, 2008, Effect of Al, Ti and Ta contents on the microstructure in Ni-base single crystal superalloy during aging [J], Rare Metal Materials and Engineering, 37, 1253
ZHENG, 2008, Investigation of the solidification behavior of a high Cr content cast Ni-Base superalloy K4648 [J], Rare Metal Materials and Engineering, 37, 1539
