Tài liệu tham khảo
Shi, 2015, Effects of Cr content on microstructure and mechanical properties of single crystal superalloy, Trans. Nonferrous Metals Soc. China, 25, 776, 10.1016/S1003-6326(15)63663-9
Wang, 2015, Effect of minor carbon additions on the high-temperature creep behavior of a single-crystal nickel-based superalloy, Mater. Charact., 104, 81, 10.1016/j.matchar.2015.04.007
Li, 2006, The effect of γ′ content on the densities of Ni-based superalloys, Metall. Mater. Trans. B Process Metall. Mater. Process. Sci., 37, 781, 10.1007/s11663-006-0060-5
Tiley, 2009, Coarsening kinetics of γ′ precipitates in the commercial nickel base Superalloy René 88 DT, Acta Mater., 57, 2538, 10.1016/j.actamat.2009.02.010
Yu, 2014, Effect of carbon addition on carbide morphology of single crystal Ni-based superalloy, Trans. Nonferrous Metals Soc. China, 24, 339, 10.1016/S1003-6326(14)63066-1
Aghajani, 2016, Identification of Mo-rich M23C6 carbides in alloy 718, Metall. Mater. Trans. A, 47, 4382, 10.1007/s11661-016-3593-5
Sundararaman, 1997, Carbide precipitation in nickel base superalloys 718 and 625 and their effect on mechanical properties, Superalloys, 367
Wang, 2017, Effect of melt heat treatment on MC carbide formation in nickel-based superalloy K465, Results Phys., 7, 2111, 10.1016/j.rinp.2017.06.020
Yin, 2007, Effect of melt treatment on carbides formation in a cast nickel-base superalloy M963, J. Mater. Process. Technol., 183, 440, 10.1016/j.jmatprotec.2006.11.002
Donachie, 2002
Gong, 2016, Investigation of solidification and segregation characteristics of cast Ni-base superalloy K417G, J. Mater. Sci. Technol.
Yang, 2013, Effects of heat treatments on the microstructure and mechanical properties of Rene 80, Mater. Des., 43, 66, 10.1016/j.matdes.2012.06.039
Xiang, 2017, Site preference of metallic elements in M23C6 carbide in a Ni-based single crystal superalloy, Mater. Des., 129, 9, 10.1016/j.matdes.2017.05.023
Sun, 2015, Thermal stability of primary MC carbide and its influence on the performance of cast Ni-base superalloys, Mater. Des., 69, 81, 10.1016/j.matdes.2014.12.038
Singh, 2011, Influence of cooling rate on the development of multiple generations of γ′ precipitates in a commercial nickel base superalloy, Mater. Charact., 62, 878, 10.1016/j.matchar.2011.06.002
Singh, 2013, Mechanisms related to different generations of γ′ precipitation during continuous cooling of a nickel base superalloy, Acta Mater., 61, 280, 10.1016/j.actamat.2012.09.058
D'Souza, 2017, Key aspects of carbide precipitation during solidification in the Ni-base superalloy, MAR M002, J. Alloys Compd., 702, 6, 10.1016/j.jallcom.2017.01.104
Dubiel, 2017, Influence of high-temperature annealing on morphological and compositional changes of phases in Ni-base single crystal superalloy, Mater. Charact., 131, 266, 10.1016/j.matchar.2017.07.021
Collins, 2015, Time-resolved synchrotron diffractometry of phase transformations in high strength nickel-based superalloys, Acta Mater., 94, 244, 10.1016/j.actamat.2015.04.046
Peterlechner, 2015, EELS analysis of the nitrogen content of carbide particles in a commercial γ′-strengthened nickel-base superalloy, Scr. Mater., 107, 42, 10.1016/j.scriptamat.2015.05.016
Li, 2014, Effect of solidification condition and carbon content on the morphology of MC carbide in directionally solidified nickel-base superalloys, J. Mater. Sci. Technol., 30, 1296, 10.1016/j.jmst.2014.06.010
Liu, 2017, Effects of microporosity and precipitates on the cracking behavior in polycrystalline superalloy Inconel 718, Mater. Charact., 132, 175, 10.1016/j.matchar.2017.08.012
Prasad, 2016, Role of shrinkage pores, carbides on cyclic deformation behaviour of conventionally cast nickel base superalloy CM247LC® at 870 °C, Mater. Sci. Eng. A, 654, 381, 10.1016/j.msea.2015.12.054
Liu, 2003, Formation of carbides and their effects on stress rupture of a Ni-base single crystal superalloy, Mater. Sci. Eng. A, 361, 191, 10.1016/S0921-5093(03)00517-3
García de la Yedra, 2012, Thermo-mechanical fatigue behaviour and life prediction of C-1023 nickel based superalloy, Int. J. Eng. Sci. Technol., 3, 10.4314/ijest.v3i6.8
Kolagar, 2017, Failure analysis of gas turbine first stage blade made of nickel-based superalloy, Case Stud. Eng. Fail. Anal., 8, 61, 10.1016/j.csefa.2017.04.002
García de la Yedra, 2014, Thermomechanical fatigue tests development and life prediction of a nickel base superalloy, Exp. Tech., 40, 777, 10.1007/s40799-016-0078-9
Tin, 2006, Investigation of oxidation characteristics and atomic partitioning in platinum and ruthenium bearing single-crystal Ni-based superalloys, Metall. Mater. Trans. A, 37, 1389, 10.1007/s11661-006-0083-1
Kraemer, 2017, Application-oriented description of time−/temperature dependent crack growth in a conventionally cast nickel-based superalloy, Int. J. Fatigue, 96, 78, 10.1016/j.ijfatigue.2016.11.025