Microstructure and mechanical behaviour of Ti―6Al―7Nb alloy produced by selective laser melting

Materials Characterization - Tập 62 Số 5 - Trang 488-495 - 2011
Edward Chlebus1, Bogumiła Kuźnicka1, Tomasz Kurzynowski1, Bogdan Dybała1
1Centre for Advanced Manufacturing Technologies, Wrocław University of Technology, 50-371, Wrocław, Poland

Tóm tắt

Từ khóa


Tài liệu tham khảo

Kruth, 2005, Binding mechanism in selective laser sintering and selective laser melting, Rapid Prototyping Journal, 11, 26, 10.1108/13552540510573365

Yadroitsev, 2007, Parametric analysis of the selective laser melting process, Applied Surface Science, 253, 8064, 10.1016/j.apsusc.2007.02.088

Chlebus, 2009, Rapid prototyping and advanced manufacturing, 733

Vandenbroucke, 2007, Selective laser melting of biocompatible metals for rapid manufacturing of medical parts, Rapid Prototyping Journal, 13, 196, 10.1108/13552540710776142

Murr, 2009, Microstructure and mechanical behavior of Ti―6Al―4V produced by rapid-layer manufacturing, for biomedical applications, Journal of the Mechanical Behavior of Biomedical Materials, 2, 20, 10.1016/j.jmbbm.2008.05.004

Lipowicz, 2009, Rapid manufacturing in medicine, Journal of Material Testers Magazine, 1, 27

Kurzynowski, 2009, SLM processing of metal powders, 398

Niinomi, 2008, Mechanical biocompatibilities of titanium alloys for biomedical application, Journal of the Mechanical Behavior of Biomedical Materials, 1, 30, 10.1016/j.jmbbm.2007.07.001

Iijima, 2003, Wear properties of Ti and Ti―6Al―7Nb castings for dental prostheses, Biomaterials, 24, 1519, 10.1016/S0142-9612(02)00533-1

Hollander, 2006, Structural, mechanical and in vitro characterization of individually structured Ti―6Al―4V produced by direct laser forming, Biomaterials, 27, 955--63, 10.1016/j.biomaterials.2005.07.041

Tamilselvi, 2006, Corrosion behavior of Ti―6Al―7Nb and Ti―6Al―4V ELI alloys in the simulated body fluid solution by electrochemical impedance spectroscopy, Electrochimica Acta, 52, 839, 10.1016/j.electacta.2006.06.018

Meticoš-Huković, 2003, The influence of niobium and vanadium on passivity of titanium-based implants in physiological solution, Biomaterials, 24, 3765, 10.1016/S0142-9612(03)00252-7

Liu, 2004, Surface modification of titanium, titanium alloys, and related materials for biomedical application, Materials Science and Engineering, R47, 49, 10.1016/j.mser.2004.11.001

López, 2002, In vitro corrosion behaviour of titanium alloys without vanadium, Electrochimica Acta, 47, 1359, 10.1016/S0013-4686(01)00860-X

Lütjering, 1998, Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys, Materials Science and Engineering, A243, 32, 10.1016/S0921-5093(97)00778-8

Ajeel, 2007, Influence of heat treatment conditions on microstructure of Ti―6Al―7Nb alloy as used surgical implant materials, Engineering and Technology, 25, 431, 10.30684/etj.25.3.15

Yadroitsev, 2007, Strategy of manufacturing components with designed internal structure by selective laser melting of metallic powder, Applied Surface Science, 254, 980, 10.1016/j.apsusc.2007.08.046

Sercombe, 2008, Heat treatment of Ti―6Al―7Nb components produced by selective laser melting, Rapid Prototyping Journal, 14, 300, 10.1108/13552540810907974

Kobryn, 2003, Microstructure and texture evolution during solidification processing of Ti―6Al―4V, Journal of Materials Processing Technology, 135, 330, 10.1016/S0924-0136(02)00865-8

Boyer, 1994

Mercelis, 2006, Residual stress in selective laser sintering and selective laser melting, Rapid Prototyping Journal, 12, 254, 10.1108/13552540610707013