Magnesium–samarium oxide nanocomposites: Room-temperature depth-sensing nanoindentation response

M. Haghshenas1, X. Song2, V. Hasannaeimi3, S. Mukherjee3, M. Gupta4
1Micro/Nano-Mechanics Laboratory, Department of Mechanical Engineering, University of Toledo, Toledo, OH, USA
2Department of Mechanical Engineering, Weifang University, Weifang, China
3Department of Materials Science and Engineering, University of North Texas, Denton, TX, USA
4Department of Mechanical Engineering, National University of Singapore, Singapore

Tài liệu tham khảo

Robson, 2016, Grain boundary segregation of rare-earth elements in magnesium alloys, Metall. Mater. Trans. A, 47, 522, 10.1007/s11661-015-3199-3 Tekumalla, 2015, Mechanical properties of magnesium-rare earth alloy systems: a review, Metals, 5, 1, 10.3390/met5010001 Hassan, 2007, Development of nano-Y2O3 containing magnesium nanocomposites using solidification processing, J. Alloy. Comp., 429, 176, 10.1016/j.jallcom.2006.04.033 Ding, 2014, Effect of Re addition on the ignition resistance of pure magnesium, Mater. Sci. Forum, 788, 88, 10.4028/www.scientific.net/MSF.788.88 Navrotsky, 2015, Thermodynamics of solid phases containing rare earth oxides, J. Chem. Thermodyn., 88, 126, 10.1016/j.jct.2015.04.008 Martienssen, 2006 Kujur, 2017, Significantly enhancing the ignition/compression/damping response of monolithic magnesium by addition of Sm2O3 nanoparticles, Metals, 7, 357, 10.3390/met7090357 Li, 1991, The mechanisms of indentation creep, Acta Metall. Mater., 39, 3099, 10.1016/0956-7151(91)90043-Z Li, 2004, Size effects of nanoindentation creep, J. Mater. Res., 19, 513, 10.1557/jmr.2004.19.2.513 Zhao, 2018, Indentation size and loading strain rate dependent creep deformation of nanocrystalline Mo, Thin Solid Films, 653, 365, 10.1016/j.tsf.2018.03.068 Haghshenas, 2018, Indentation-based rate-dependent plastic deformation of polycrystalline pure magnesium, Mater. Sci. Eng., 716, 63, 10.1016/j.msea.2018.01.036 Haghshenas, 2019, Depth sensing indentation of magnesium/boron nitride nanocomposites, J. Compos. Mater., 53, 1751, 10.1177/0021998318808358 Sankaranarayanan, 2015, Review on mechanical properties of magnesium (nano) composites developed using energy efficient microwaves, Powder Metall., 58, 183, 10.1179/1743290115Y.0000000009 Wu, 2019, Effects of annealing on microstructure and mechanical properties of rapidly solidified Cu-3 wt% Ag-1 wt% Zr, Mater. Sci. Eng., 739, 357, 10.1016/j.msea.2018.10.062 Nam, 2018, Structural effect of two-dimensional BNNS on grain growth suppressing behaviors in Al-matrix nanocomposites, Sci. Rep., 8, 1614, 10.1038/s41598-018-20150-5 Hassold, 1990 Mirza, 2015, A unified model for the prediction of yield strength in particulate-reinforced metal matrix nanocomposites, Materials, 8, 5138, 10.3390/ma8085138 Oliver, 1992, An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments, J. Mater. Res., 7, 1564, 10.1557/JMR.1992.1564 Jian, 2013, Dislocation energetics and Pop-ins in AlN thin films by Berkovich nanoindentation, Materials, 6, 4259, 10.3390/ma6094259 Lorenz, 2003, Pop-in effect as homogeneous nucleation of dislocations during nanoindentation, Phys. Rev. B, 67, 172101, 10.1103/PhysRevB.67.172101 Ghasemi, 2018, Microstructure and nanoindentation analysis of Mg-SiC nanocomposite powders synthesized by mechanical milling, Mater. Char., 142, 137, 10.1016/j.matchar.2018.05.023 Bočan, 2015, Nanomechanical analysis of AZ31 magnesium alloy and pure magnesium correlated with crystallographic orientation, Mater. Sci. Eng., 644, 121, 10.1016/j.msea.2015.07.055 Guo, 2016, Distinguishing between slip and twinning events during nanoindentation of magnesium alloy AZ31, Scr. Mater., 110, 10, 10.1016/j.scriptamat.2015.07.034 Cao, 2006, On the determination of reduced Young's modulus and hardness of elastoplastic materials using a single sharp indenter, J. Mater. Res., 21, 215, 10.1557/jmr.2006.0018 Greer, 2005, Size dependence of mechanical properties of gold at the micron scale in the absence of strain gradients, Acta Mater., 53, 1821, 10.1016/j.actamat.2004.12.031 Nix, 1998, Indentation size effects in crystalline materials: a law for strain gradient plasticity, J. Mech. Phys. Solids, 46, 411, 10.1016/S0022-5096(97)00086-0 Bonn, 2009, Wetting and spreading, Rev. Mod. Phys., 81, 739, 10.1103/RevModPhys.81.739 Kozbial, 2014, Study on the surface energy of graphene by contact angle measurements, Langmuir, 30, 8598, 10.1021/la5018328 Dean, 2013, A procedure for extracting primary and secondary creep parameters from nanoindentation data, Mech. Mater., 65, 124, 10.1016/j.mechmat.2013.05.014 Sharma, 2000, Hot hardness and indentation creep studies of a Fe–28Al–3Cr–0.2 C alloy, Mater. Sci. Eng., 278, 106, 10.1016/S0921-5093(99)00590-0 De La Torre, 1991, Indentation creep of lead and lead-copper alloys, J. Mater. Sci., 26, 4351, 10.1007/BF00543650 Haghshenas, 2019, Magnesium nanocomposites: an overview on time-dependent plastic (creep) deformation, Def. Technol., 15, 123, 10.1016/j.dt.2018.08.008