Low-Temperature Degradation of Zirconia and Implications for Biomedical Implants

Annual Review of Materials Research - Tập 37 Số 1 - Trang 1-32 - 2007
Jérôme Chevalier1, Laurent Grémillard1, Sylvain Deville2
1Mateis, INSA Lyon, CNRS UMR 5510, 69621 Villeurbanne, France;
2Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, California, 94720

Tóm tắt

This review describes the mechanisms responsible for low-temperature degradation (LTD) of zirconia ceramics and its detrimental consequences for biomedical devices. Special emphasis is given to the critical issue of zirconia degradation actually observed for hip prostheses. Experimental methods to accurately measure and predict LTD in a given zirconia ceramic are presented. Different solutions to inhibit LTD or at least reduce its kinetics are reviewed, with the objective of highlighting alternative options for the generation of new zirconia-based biomedical ceramic devices.

Từ khóa


Tài liệu tham khảo

10.1038/258703a0

10.1007/BF00553200

Christel PS, 1989, Bull. Hosp. Joint Dis. Orthop. Inst., 49, 170

10.1016/0167-2738(81)90138-7

10.1007/BF01756800

10.1111/j.1151-2916.2003.tb03639.x

10.1111/j.1151-2916.1999.tb02055.x

Lilley E, 1990, Ceram. Trans., 10, 387

10.1002/jbm.820280512

US Food and Drug Administration. 2001. Recall of zirconia ceramic femoral heads for hip implants.http://www.fda.gov/cdrh/recalls/zirconiahip.html

Saint Gobain Desmarquest. 2004. Information on breakages reported on Prozyr® zirconia heads.http://www.prozyr.com/PAGES_UK/Biomedical/figures.htm

10.2106/00004623-200300004-00009

10.1016/S0079-6425(00)00005-0

Deville S, 2004, Acta Mater., 52, 5697

10.1007/BF00809057

10.1007/BF01031853

Fabrichnaya O, 2004, Zeitschr. Metallk. Mater. Res. Adv. Tech., 95, 27

10.1111/j.1151-2916.1986.tb07415.x

10.1016/j.jeurceramsoc.2004.03.025

10.1111/j.1151-2916.2004.tb07505.x

10.1111/j.1151-2916.1986.tb04789.x

Deville S, 2004, Acta Mater., 52, 5709

10.1111/j.1151-2916.1999.tb02180.x

10.1007/BF00819957

10.1007/BF01352217

Christian JW, 1965, The Theory of Transformations in Metals and Alloys., 2

Chevalier J, 1997, Bioceramics: Proc. Int. Symp. Ceram. Med., 10th, Paris, 10, 135

10.1016/j.jeurceramsoc.2003.11.025

10.1002/jbm.b.30123

10.1111/j.1151-2916.1972.tb11290.x

10.1111/j.1151-2916.1984.tb19614.x

10.1111/j.1151-2916.1987.tb04972.x

10.1111/j.1151-2916.1982.tb10445.x

10.1117/1.1647547

10.1016/S0955-2219(00)00273-9

10.1006/jssc.1999.8565

10.1111/j.1151-2916.1997.tb02796.x

10.1016/j.surfcoat.2005.07.089

10.1016/S0924-0136(99)00157-0

10.1111/j.1151-2916.2003.tb03639.x

Pee JH, Tada M, Hayakawa M. 2006. Crystallographic study of the isothermal and athermal martensites of yttria-doped zirconia. Mater. Sci. Eng. A. In press. doi:10.1016/j.msea.2005.12.062

10.1111/j.1151-2916.1993.tb06627.x

10.1016/S0142-9612(01)00206-X

US Food and Drug Administration. 1997. Steam re-sterilization causes deterioration of zirconia ceramic heads of total hip prostheses.http://www.fda.gov/cdrh/steamst.html

10.1302/0301-620X.83B7.12122

10.1023/A:1025678525474

10.1016/j.arth.2004.06.017

10.1016/j.biomaterials.2005.07.034

10.1302/0301-620X.81B5.9454

10.1302/0301-620X.85B4.13397

10.1302/0301-620X.84B5.12679

Caton J, Bouraly JP, Reynaud P Merabet Z. 2004. Phase Transformation in Zirconia Heads after THA: Myth or Reality. Proc. BIOLOX Symp., 9th, Paris, pp.73–74. Darmstadt, Ger.: Steinkopff-Verlag

10.1007/s00776-004-0777-4

Cales B. 2000. Fractures of zirconia hip joint heads. Maîtrise orthopédique.http://www.maitrise-orthop.com/corpusmaitri/orthopaedic/96/cales/cales.shtml

10.1097/00003086-200010000-00013

Agence Française de Sécurité Sanitaire et des Produits de Santé. 2001. Décision portant sur la suspension d’utilisation de certaines têtes de prothèse de hanche en céramique de zircone.http://agmed.sante.gouv.fr/htm/alertes/filalert/dm010811.htm

10.1302/0301-620X.86B8.15012

10.1016/j.arth.2004.02.045

10.1016/S0021-9290(03)00186-6

10.1111/j.1151-2916.1986.tb04786.x

10.1557/JMR.2003.0337

10.1111/j.1151-2916.1996.tb08980.x

10.1016/S0272-8842(96)00074-0

10.1111/j.1151-2916.2003.tb03483.x

10.1016/j.biomaterials.2004.01.002

10.1016/S0921-5093(00)01276-4

10.1016/j.biomaterials.2005.11.021

10.1111/j.1151-2916.1985.tb15239.x

Green DJ, Hannink RHJ, Swain MV. 1989. Transformation Toughening of Ceramics. Boca Raton, FL: CRC Press. 232 pp.

10.1039/jm9960601805

10.1021/cm950558j

10.1111/j.1151-2916.2000.tb01202.x

10.1016/S0272-8842(97)00036-9

10.1111/j.1151-2916.1991.tb06892.x

10.1016/S0167-577X(97)00122-5

10.1007/BF00351622

10.1007/BF00544531

10.1111/j.1151-2916.1991.tb06905.x

10.1016/S1359-6462(01)01076-4

10.1023/A:1018567414745

10.1111/j.1151-2916.1987.tb04853.x

10.1016/S1359-6454(00)00252-4

10.1111/j.1151-2916.2002.tb00103.x

10.4028/www.scientific.net/KEM.233-236.655

10.1111/j.1151-2916.1997.tb03163.x

10.4028/www.scientific.net/KEM.206-213.669

10.1016/S0955-2219(03)00307-8

10.1002/adma.200390117

10.1016/S1359-6454(01)00413-X

10.1016/S0955-2219(03)00313-3

10.1111/j.1151-2916.2003.tb03287.x

10.1021/nl050492j