Dicarlo JA, Yun HM, Morscher GN, et al. Progress in SiC/SiC composites for engine applications. In: High Temperature Ceramic Matrix Composites. Krenkel W, Naslain R, Schneider H, Eds. Weinheim, Germany: Wiley-VCH Verlag GmbH & Co. KGaA, 2001: 777–782.
Naslain RR, Pailler RJF, Lamon JL. Single- and multilayered interphases in SiC/SiC composites exposed to severe environmental conditions: An overview. Int J Appl Ceram Technol 2010, 7: 263–275.
Naslain RR. SiC-matrix composites: Nonbrittle ceramics for thermo-structural application. Int J Appl Ceram Technol 2005, 2: 75–84.
Dicarlo JA, van Roode M. Ceramic composite development for gas turbine engine hot section components. In: Proceedings of the ASME Turbo Expo 2006: Power for Land, Sea, and Air, Barcelona, Spain, 2008: 221–231.
Christin F. Design, fabrication, and application of thermostructural composites (TSC) like C/C, C/SiC, and SiC/SiC composites. Adv Eng Mater 2002, 4: 903–912.
Pierce JL, Zawada LP, Srinivasan R. Tensile properties of nicalon fiber-reinforced carbon following aerospace turbine engine testing. J Mater Eng Perform 2003, 12: 354–362.
Staehler JM, Zawada LP. Performance of four ceramic-matrix composite divergent flap inserts following ground testing on an F110 turbofan engine. J Am Ceram Soc 2004, 83: 1727–1738.
Cavalier JC, Berdoyes I, Bouillon E. Composites in aerospace industry. Advances in Sci & Tech 2006, 50: 153–162.
Boyle RJ, Parikh AH, Nagpal VK, et al. Ceramic matrix composites for high pressure turbine vanes. In: Proceeding of the ASME Turbo Expo 2014: Turbine Technical Conference and Exposition, Düsseldorf, Germany, 2014, GT2014-27136, V006T02A013.
Grujicic M, Snipes J, Yavari R, et al. Computational investigation of foreign object damage sustained by environmental barrier coatings (EBCs) and SiC/SiC ceramic-matrix composites (CMCs). Multidiscip Modeling Mater Struct 2015, 11: 238–272.
Liu QM, Huang SZ, He AJ. Research progress in environmental barrier coatings of SiC ceramic matrix composites. J Mater Eng 2018, 46: 1–8. (in Chinese)
Lu YH, Wang YG. Formation and growth of silica layer beneath environmental barrier coatings under water-vapor environment. J Alloys Compd 2018, 739: 817–826.
Heveran CM, Xu JP, Sarin VK, et al. Simulation of stresses in TBC-EBC coating systems for ceramic components in gas turbines. Surf Coat Technol 2013, 235: 354–360.
Lee KN. Current status of environmental barrier coatings for Si-based ceramics. Surf Coat Technol 2000, 133–134: 1–7.
Naslain R. Challenging ceramic matrix composites for applications in severe environments. Adv Compos Mater 1995, 5: 35–44.
Cavalier J C, Berdoyes I, Bouillon E. Composites in aerospace industry. Adv Sci Technol 2006, 50: 153–162.
Yun HM, Dicarlo JA, Bhatt RT, et al. Processing and structural advantages of the Sylramic-iBN SiC fiber for SiC/SiC components. In: the 27th Annual Cocoa Beach Conference on Advanced Ceramics and Composites: B: Ceramic Engineering and Science Proceedings, Volume 24. Kriven WM, Lin HT, Eds. Westerville, USA: The American Ceramic Society 735 Ceramic Place, 2003: 247–253.
Naslain R, Langlais F, Fedou R. The CVI-processing of ceramic matrix composites. J Phys Colloques 1989, 50: C5-191–C5-207. (in French)
Yin XW, Cheng LF, Zhang LT, et al. Fibre-reinforced multifunctional SiC matrix composite materials. Int Mater Rev 2017, 62: 117–172.
Mingazzini C, Brentari A, Burgio F, et al. Optimization of a pyrolysis procedure for obtaining SiC-SiCf CMC by PIP for thermostructural applications. Adv Sci Technol 2013, 77: 153–158.
Jiang JM, Wang S, Li W, et al. Preparation of 3D Cf/ZrC-SiC composites by joint processes of PIP and RMI. Mater Sci Eng A 2014, 607: 334–340.
Naslain RR. SiC-matrix composites: Nonbrittle ceramics for thermo-structural application. Int J Appl Ceram Technol 2005, 2: 75–84.
Cheng LF, Wu SJ, Zhang LT, et al. Mechanical self-adaptability of a SiC/PyC/SiC composite during oxidation in air. J Compos Mater 2009, 43: 305–313.
Cheng LF, Xu YD, Zhang LT, et al. Effect of carbon interlayer on oxidation behavior of C/SiC composites with a coating from room temperature to 1500 °C. Mater Sci Eng A 2001, 300: 219–225.
Wang HL, Gao ST, Peng SM, et al. KD-S SiCf/SiC composites with BN interface fabricated by polymer infiltration and pyrolysis process. J Adv Ceram 2018, 7: 169–177.
Bansal NP, Eldridge JI. Hi-Nicalon fiber-reinforced celsian matrix composites: Influence of interface modification. J Mater Res 1998, 13: 1530–1537.
Hillig WB. Strength and toughness of ceramic matrix composites. Annu Rev Mater Sci 1987, 17: 341–383.
Rebillat F. Advances in Ceramic Matrix Composites, 2nd edn. Cambridge, UK: Woodhead Publishing, 2014.
Goujard S, Vandenbulcke L, Tawil H. The oxidation behaviour of two- and three-dimensional C/SiC thermostructural materials protected by chemical-vapour-deposition polylayers coatings. J Mater Sci 1994, 29: 6212–6220.
Goujard S, Vandenbulcke L, Tawil H. Oxidation behavior of 2D and 3D carbon/carbon thermostructural materials protected by CVD polylayer coatings. Thin Solid Films 1994, 252: 120–130.
Ruggles-Wrenn MB, Pope MT. Creep behavior in interlaminar shear of a SiC/SiC ceramic composite with a self-healing matrix. Appl Compos Mater 2014, 21: 213–225.
Lamouroux F, Bertrand S, Pailler R, et al. Oxidation-resistant carbon-fiber-reinforced ceramic-matrix composites. Compos Sci Technol 1999, 59: 1073–1085.
Lamouroux F, Bertrand S, Pailler R, et al. A multilayer ceramic matrix for oxidation resistant carbon fibers-reinforced CMCs. Key Eng Mater 1999, 164–165: 365–368.
Luan XG, Zou Y, Hai XH, et al. Degradation mechanisms of a self-healing SiC(f)/BN(i)/[SiC-B4C](m) composite at high temperature under different oxidizing atmospheres. J Eur Ceram Soc 2018, 38: 3804–3813.
Zuo XZ, Zhang LT, Liu YS, et al. Oxidation behaviour of two-dimensional C/SiC modified with self-healing Si-B-C coating in static air. Corros Sci 2012, 65: 87–93.
Forio P, Lamon J. Fatigue behavior at high temperatures in Air of a 2D SiC/Si-B-C composite with a self-healing multilayered matrix. In: Advances in Ceramic Matrix Composites VII, Volume 28. Bansal NP, Singh J, Lin HT, Eds. Indianapolis, USA: The American Ceramic Society, 2012: 127–141.
Quemard L, Rebillat F, Guette A, et al. Self-healing mechanisms of a SiC fiber reinforced multi-layered ceramic matrix composite in high pressure steam environments. J Eur Ceram Soc 2007, 27: 2085–2094.
Zhang Q, Zuo XZ, Liu YS, et al. Oxidation behaviors and mechanisms of CVD Si-B-C ceramic in wet oxygen from 700 °C to 1400 °C. J Eur Ceram Soc 2016, 36: 3709–3715.
Cao XY, Yin XW, Fan XM, et al. High-temperature flexural properties of SiBC modified C/SiC composites. Ceram Int 2014, 40: 6185–6190.
Cao XY, Yin XW, Ma XK, et al. Oxidation behavior of SiBC matrix modified C/SiC composites with different PyC interphase thicknesses. Ceram Int 2015, 41: 1695–1700.
Goujard S, Vandenbulcke L, Tawil H. Oxidation tests of carbonaceous composite materials protected by Si-B-C CVD coatings. Thin Solid Films 1994, 245: 86–97.
Luan XG, Wang L, Zou Y, et al. Oxidation behavior of C/SiC-SiBCN composites at high temperature. J Eur Ceram Soc 2019, 39: 3003–3012.
Vandenbulcke L, Fantozzi G, Goujard S, et al. Outstanding ceramic matrix composites for high temperature applications. Adv Eng Mater 2005, 7: 137–142.
Hatta H, Sohtome T, Sawada Y, et al. High temperature crack sealant based on SiO2-B2O3 for SiC coating on carbon-carbon composites. Adv Compos Mater 2003, 12: 93–106.
Han WB, Hu P, Zhang XH, et al. High-temperature oxidation at 1900 °C of ZrB2-xSiC ultrahigh-temperature ceramic composites. J Am Ceram Soc 2008, 91: 3328–3334.
Han JC, Hu P, Zhang XH, et al. Oxidation-resistant ZrB2-SiC composites at 2200 °C. Compos Sci Technol 2008, 68: 799–806.
Rezaie A, Fahrenholtz WG, Hilmas GE. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500 °C. J Eur Ceram Soc 2007, 27: 2495–2501.
Lavrenko VO, Panasyuk AD, Grigorev OM, et al. High-temperature oxidation of ZrB2-SiC and ZrB2-SiC-ZrSi2 ceramics up to 1700 °C in air. Powder Metall Met Ceram 2012, 51: 217–221.
Wang PP, Tong MD, Wang HH, et al. Gradient HfB2-SiC multilayer oxidation resistant coating for C/C composites. Ceram Int 2018, 44: 20968–20973.
Bhatt RT, Choi SR, Cosgriff LM, et al. Impact resistance of uncoated SiC/SiC composites. Mater Sci Eng A 2008, 476: 20–28.
Brewer D. HSR/EPM combustor materials development program. Mater Sci Eng A 1999, 261: 284–291.
Dicarlo JA, Yun HM, Morscher GN, et al. Progress in SiC/SiC ceramic composite development for gas turbine hot-section components under NASA EPM and UEET programs. In: Proceedings of the ASME Turbo Expo 2002: Power for Land, Sea, and Air, Amsterdam, the Netherlands, 2009: 39–45.
Dicarlo JA. Advances in SiC/SiC composites for aero-propulsion. NASA/TM—2013-217889.
Dicarlo JA, Yun HM, Morscher GN, et al. SiC/SiC Composites for 1200 °C and above. In: Handbook of Ceramic Composites. Narottam PB, Ed. Boston, USA: Springer New York, 2005: 77–98.
Dicarlo JA, Yun HM, Hurst JB. Fracture mechanisms for SiC fibers and SiC/SiC composites under stress-rupture conditions at high temperatures. Appl Math Comput 2004, 152: 473–481.
Lang J, Dicarlo JA. Further developments in modeling creep effects within structural SiC/SiC components. In: Peoceedings of the 32nd Annual Conference Composites Materials and Structures, Daytona Beach, USA, 2008: 20080047429.
Bhatt RT, Dicarlo JA, Mccue TR. Thermal stability of melt infiltrated SiC/SiC composites. In: 27th Annual Cocoa Beach Conference on Advanced Ceramics and Composites: B: Ceramic Engineering and Science Proceedings, Volume 24. Kriven WM, Lin HT, Eds. Westerville, USA: The American Ceramic Society 735 Ceramic Place, 2003: 295–300.
Dicarlo JA, Bhatt RT, Mccue TR. Modeling the thermostructural stability of melt infiltrated SiC/SiC composites. In: 27th Annual Cocoa Beach Conference on Advanced Ceramics and Composites: B: Ceramic Engineering and Science Proceedings, Volume 24. Kriven WM, Lin HT, Eds. Westerville, USA: The American Ceramic Society 735 Ceramic Place, 2003: 465–470.
Shimoda K, Hinoki T, Katoh Y, et al. Development of the tailored SiC/SiC composites by the combined fabrication process of ICVI and NITE methods. J Nucl Mater 2009, 384: 103–108.
Dong SM, Katoh Y, Kohyama A. Processing optimization and mechanical evaluation of hot pressed 2D Tyranno-SA/SiC composites. J Eur Ceram Soc 2003, 23: 1223–1231.
Katoh Y, Dong SM, Kohyama A. Thermo-mechanical properties and microstructure of silicon carbide composites fabricated by nano-infiltrated transient eutectoid process. Fusion Eng Des 2002, 61–62: 723–731.
Park JS, Jung HC, Ooi Y, et al. Fabrication of environmentally resistant NITE-SiC/SiC composites. IOP Conf Ser Mater Sci Eng 2011, 18: 202012.
Sigl LS, Evans AG. Effects of residual stress and frictional sliding on cracking and pull-out in brittle matrix composites. Mech Mater 1989, 8: 1–12.
Morscher GN, Gregory N. Matrix cracking in four different 2D SiC/SiC composite systems. In: Proceedings of the 35th International SAMPE Technical Conference, Dayton, USA, 2003: 20040031565.
Morscher GN, Yun HM, Dicarlo JA. Matrix cracking in 3D orthogonal melt-infiltrated SiC/SiC composites with various Z-fiber types. J Am Ceram Soc 2005, 88: 146–153.
Morscher GN, Yun HM, Dicarlo JA. In-plane cracking behavior and ultimate strength for 2D woven and braided melt-infiltrated SiC/SiC composites tensile loaded in off-axis fiber directions. J Am Ceram Soc 2007, 90: 3185–3193.
Morscher GN, Dicarlo JA, Kiser JD, et al. Effects of fiber architecture on matrix cracking for melt-infiltrated SiC/SiC composites. Int J Appl Ceram Technol 2010, 7: 276–290.
Li LB. Synergistic effects of temperature and oxidation on matrix cracking in fiber-reinforced ceramic-matrix composites. Appl Compos Mater 2017, 24: 691–715.
Li LB. Modeling matrix multicracking development of fiber-reinforced ceramic-matrix composites considering fiber debonding. Int J Appl Ceram Technol 2019, 16: 97–107.
Naslain RR. The design of the fibre-matrix interfacial zone in ceramic matrix composites. Compos A Appl Sci Manuf 1998, 29: 1145–1155.
Cook J, Gordon JE. A mechanism for the control of crack propagation in all-brittle systems. Proc Roy Soc A Math Phys Eng Sci 1964, 282: 508–520.
Pompidou S, Lamon J. Analysis of crack deviation in ceramic matrix composites and multilayers based on the Cook and Gordon mechanism. Compos Sci Technol 2007, 67: 2052–2060.
Ma XK, Yin XW, Cao XY, et al. Effect of heat treatment on the mechanical properties of SiCf/BN/SiC fabricated by CVI. Ceram Int 2016, 42: 3652–3658.
Lowden RA, More KL. The effect of fiber coatings on interfacial shear strength and the mechanical behavior of ceramic composites. MRS Proc 1989, 170: 205–214.
Zhu GX, Xue YD, Hu JB, et al. Influence of boron nitride nanotubes on the damage evolution of SiCf/SiC composites. J Eur Ceram Soc 2018, 38: 4614–4622.
Feng W, Zhang LT, Liu YS, et al. The improvement in the mechanical and thermal properties of SiC/SiC composites by introducing CNTs into the PyC interface. Mater Sci Eng A 2015, 637: 123–129.
Morscher GN, Singh M, Kiser JD, et al. Modeling stress-dependent matrix cracking and stress-strain behavior in 2D woven SiC fiber reinforced CVI SiC composites. Compos Sci Technol 2007, 67: 1009–1017.
Bunsell AR, Piant A. A review of the development of three generations of small diameter silicon carbide fibres. J Mater Sci 2006, 41: 823–839.
Pavia F, Letertre A, Curtin WA. Prediction of first matrix cracking in micro/nanohybrid brittle matrix composites. Compos Sci Technol 2010, 70: 916–921.
Park JY, Kang SM, Kim WJ, et al. Characterization of the SiCf/SiC composite fabricated by the whisker growing assisted CVI process. Key Eng Mater 2005, 287: 200–205.
Kim WJ, Kang SM, Park JY, et al. Effect of a SiC whisker formation on the densification of Tyranno SA/SiC composites fabricated by the CVI process. Fusion Eng Des 2006, 81: 931–936.
Kim WJ, Kang SM, Park JY. Microstructure and properties of SiC nanowire-reinforced SiCf/SiC composites. Adv Mater Res 2009, 59: 279–282.
Li YJ, Zhang Y, Wang YS. Structure and oxidation behavior of high temperature ZrB2-SiBCN ceramics with polyborosilazane as a sintering additive. J Ceram Soc Jpn 2013, 121: 520–523.
Guo QG, Song JR, Liu L, et al. Relationship between oxidation resistance and structure of B4C-SiC/C composites with self-healing properties. Carbon 1999, 37: 33–40.
Tang BJ, Feng ZL, Hu SJ, et al. Preparation and anti-oxidation characteristics of ZrSiO4-SiBCN(O) amorphous coating. Appl Surf Sci 2015, 331: 490–496.
Shan QL, Feng Q, Hu JB, et al. Oxidation behavior in wet oxygen environment of Al2O3 added reaction-sintered Si-B-C ceramics. Ceram Int 2018, 44: 4009–4015.
Feng JP, Yan YY, Chen DP, et al. Study of thermal stability of fumed silica based thermal insulating composites at high temperatures. Compos B Eng 2011, 42: 1821–1825.
Xie J, Li KZ, Li HJ, et al. Ablation behavior and mechanism of C/C-ZrC-SiC composites under an oxyacetylene torch at 3000 °C. Ceram Int 2013, 39: 4171–4178.
Tan WL, Li KZ, Li HJ, et al. Ablation behavior and mechanism of C/C-HfC-SiC composites. Vacuum 2015, 116: 124–129.
Wang YG, Liu W, Cheng LF, et al. Preparation and properties of 2D C/ZrB2-SiC ultra high temperature ceramic composites. Mater Sci Eng A 2009, 524: 129–133.
Feng B, Li HJ, Zhang YL, et al. Effect of SiC/ZrC ratio on the mechanical and ablation properties of C/C-SiC-ZrC composites. Corros Sci 2014, 82: 27–35.
Lohfeld S, Schütze M, Böhm A, et al. Oxidation behaviour of particle reinforced MoSi2 composites at temperatures up to 1700 °C. Mater Corros 2005, 56: 250–258.
Ball RGJ, Mignanelli MA, Barry TI, et al. The calculation of phase equilibria of oxide core-concrete systems. J Nucl Mater 1993, 201: 238–249.
Shin D, Arróyave R, Liu ZK. Thermodynamic modeling of the Hf-Si-O system. Calphad 2006, 30: 375–386.
Jacobson NS, Lee KN, Fox DS. Reactions of silicon carbide and silicon(IV) oxide at elevated temperatures. J Am Ceram Soc 1992, 75: 1603–1611.
Borisov VG, Yudin BF. Reaction thermodynamics in the SiO2-SiC system. Refractories 1968, 9: 162–165.
Liu YS, Zhang LT, Cheng LF, et al. Preparation and oxidation resistance of 2D C/SiC composites modified by partial boron carbide self-sealing matrix. Mater Sci Eng A 2008, 498: 430–436.
Zuo XZ, Zhang LT, Liu YS, et al. Oxidation behaviour of two-dimensional C/SiC modified with self-healing Si-B-C coating in static air. Corros Sci 2012, 65: 87–93.
Liu F, Kong J, Luo CJ, et al. High temperature self-healing SiBCN ceramics derived from hyperbranched polyborosilazanes. Adv Compos Hybrid Mater 2018, 1: 506–517.
Xu YD, Cheng LF, Zhang LT, et al. Oxidation behavior and mechanical properties of C/SiC composites with Si-MoSi2 oxidation protection coating. J Mater Sci 1999, 34: 6009–6014.
Carney CM, Parthasarathy TA, Cinibulk MK. Oxidation resistance of hafnium diboride ceramics with additions of silicon carbide and tungsten boride or tungsten carbide. J Am Ceram Soc 2011, 94: 2600–2607.
Cheng LF, Xu YD, Zhang LT, et al. Effect of glass sealing on the oxidation behavior of three dimensional C/SiC composites in air. Carbon 2001, 39: 1127–1133.
Fan SW, Zhang LT, Cheng LF, et al. Preparation and properties of self-healing coating for C/SiC brake materials. Int J Appl Ceram Technol 2008, 5: 204–209.
Isola C, Appendino P, Bosco F, et al. Protective glass coating for carbon-carbon composites. Carbon 1998, 36: 1213–1218.
Huang JF, Zhang YL, Zhu KJ, et al. Microstructure and oxidation protection of borosilicate glass coating prepared by pulse arc discharge deposition for C/C composites. Ceram Int 2015, 41: 4662–4667.
Liu YS, Men J, Zhang LT, et al. Microstructural evolution and self-healing mechanism of a 2D C/SiC-BCx composite under constant load in static wet oxygen and dynamic combustion atmosphere. Mater Corros 2015, 66: 128–136.
Ye F, Zhang LT, Yin XW, et al. Fabrication of Si3N4-SiBC composite ceramic and its excellent electromagnetic properties. J Eur Ceram Soc 2012, 32: 4025–4029.
Liu YS, Wan JJ, Zuo XZ, et al. Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si-B-C/SiC coatings under wet oxygen atmosphere. Appl Surf Sci 2015, 353: 214–223.
Dong N, Zuo XZ, Liu YS, et al. Fatigue behavior of 2D C/SiC composites modified with Si-B-C ceramic in static air. J Eur Ceram Soc 2016, 36: 3691–3696.
Carrère P, Lamon J. Fatigue behavior at high temperature in air of a 2D woven SiC/SiBC with a self healing matrix. Key Eng Mater 1998, 164–165: 321–324.
Forio P, Lamon J. Fatigue behavior at high temperatures in air of a 2D SiC/Si-B-C composite with a self-healing multilayered matrix. In: Advances in Ceramic Matrix Composites VII, Volume 128. Bansal NP, Singh JP, Lin HT, Eds. Westerville, USA: The American Ceramic Society, 2001: 127–141.
Viricelle JP, Goursat P, Bahloul-Hourlier D. Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m. Compos Sci Technol 2001, 61: 607–614.
Bouillon EP, Spriet PC, Habarou G, et al. Engine test and post engine test characterization of self-sealing ceramic matrix composites for nozzle applications in gas turbine engines. In: Proceedings of the ASME Turbo Expo 2004: Power for Land, Sea, and Air, Vienna, Austria, 2008: 409–416.
Christin FA. A global approach to fiber nD architectures and self-sealing matrices: From research to production. Int J Appl Ceram Technol 2005, 2: 97–104.
Bouillon E, Lamouroux F, Baroumes L, et al. An improved long life duration CMC for jet aircraft engine applications. In: Proceedings of the ASME Turbo Expo 2002: Power for Land, Sea, and Air, Amsterdam, the Netherlands, 2009: 119–125.
Lamouroux F, Bouillon E, Cavalier JC, et al. An improved long life duration CMC for jet aircraft engine applications. In: High Temperature Ceramic Matrix Composites. Krenkel W, Naslain R, Schneider H, Eds. Weinheim, Germany: Wiley-VCH Verlag GmbH & Co. KGaA, 2001: 783–788.
Lacombe A, Spriet P, Habarou G, et al. Ceramic matrix composites to make breakthroughs in aircraft engine performance. In: Proceedings of the 50th AIAA/ASME/ASCE/AHS/ASC Structures, Structural Dynamics, and Materials Conference, Palm Springs, USA, 2009: 2009–2675.
Cao XY, Yin XW, Fan XM, et al. Effect of PyC interphase thickness on mechanical behaviors of SiBC matrix modified C/SiC composites fabricated by reactive melt infiltration. Carbon 2014, 77: 886–895.
Zhao DL, Fan XM, Yin XW, et al. Oxidation behavior of tyranno ZMI-SiC fiber/SiC-SiBC matrix composite from 800 to 1200 °C. Materials 2018, 11: 1367.
Sun XN, Yin XW, Fan XM, et al. Oxidation resistance of SiC/SiC composites containing SiBC matrix fabricated by liquid silicon infiltration. J Eur Ceram Soc 2018, 38: 479–485.
Ma XK, Yin XW, Fan XM, et al. Improved tensile strength and toughness of dense C/SiC-SiBC with tailored PyC interphase. J Eur Ceram Soc 2019, 39: 1766–1774.
Zhang PF, Jia DC, Yang ZH, et al. Progress of a novel non-oxide Si-B-C-N ceramic and its matrix composites. J Adv Ceram 2012, 1: 157–178.
Wang ZC, Aldinger F, Riedel R. Novel silicon-boron-carbon-nitrogen materials thermally stable up to 2200 °C. J Am Ceram Soc 2001, 84: 2179–2183.
Baldus HP, Jansen M, Wagner O. New materials in the system Si-(N,C)-B and their characterization. Key Eng Mater 1993, 89–91: 75–80.
Riedel R, Kienzle A, Dressler W, et al. A silicoboron carbonitride ceramic stable to 2,000 °C. Nature 1996, 382: 796–798.
Cinibulk MK, Parthasarathy TA. Characterization of oxidized polymer-derived SiBCN fibers. J Am Ceram Soc 2001, 84: 2197–2202.
Baldus HP, Passing G, Scholz H, et al. Properties of amorphous SiBNC-ceramic fibres. Key Eng Mater 1996, 127–131: 177–184.
Zhang CY, Han KQ, Liu Y, et al. A novel high yield polyborosilazane precursor for SiBNC ceramic fibers. Ceram Int 2017, 43: 10576–10580.
Rooke MA, Sherwood PMA. Surface studies of potentially oxidation protective Si-B-N-C films for carbon fibers. Chem Mater 1997, 9: 285–296.
Luan XG, Xu XM, Zou Y, et al. Wet oxidation behavior of SiC/(SiC-SiBCN)x composites prepared by CVI combined with PIOP process. J Am Ceram Soc 2019, 102: 6239–6255.
Tan X, Liu W, Cao LM, et al. Oxidation behavior of a 2D-SiCf/BN/SiBCN composite at 1350–1650 °C in air. Mater Corros 2018, 69: 1227–1236.
Butchereit E, Nickel KG, Müller A. Precursor-derived Si-B-C-N ceramics: Oxidation kinetics. J Am Ceram Soc 2001, 84: 2184–2188.
Lu B, Zhang Y. Oxidation behavior of SiC-SiBCN ceramics. Ceram Int 2015, 41: 1023–1030.
Li DX, Yang ZH, Jia DC, et al. Effects of boron addition on the high temperature oxidation resistance of dense sSiBCN monoliths at 1500 °C. Corros Sci 2017, 126: 10–25.
Liang B, Yang ZH, Jia DC, et al. Amorphous silicoboron carbonitride monoliths resistant to flowing air up to 1800 °C. Corros Sci 2016, 109: 162–173.
Zhang M, Chen QQ, He YP, et al. A comparative study on high temperature oxidation behavior of SiC, SiC-BN and SiBCN monoliths. Corros Sci 2021, 192: 109855.
Li DX, Yang ZH, Jia DC, et al. High-temperature oxidation behavior of dense SiBCN monoliths: Carbon-content dependent oxidation structure, kinetics and mechanisms. Corros Sci 2017, 124: 103–120.
Luan XG, Xu XM, Wang L, et al. Self-healing enhancing tensile creep of 2D-satin weave SiC/(SiC-SiBCN)x composites in wet oxygen environment. J Eur Ceram Soc 2020, 40: 3509–3519.
Xu HM, Peng YQ, Wei ZH, et al. Oxidation behavior of 3D SiCf/SiBCN composites at 800–1200 °C. J Eur Ceram Soc 2021, 41: 148–157.
Ding Q, Ni DW, Wang Z, et al. Mechanical properties and microstructure evolution of 3D Cf/SiBCN composites at elevated temperatures. J Am Ceram Soc 2018, 101: 4699–4707.
Butchereit E, Nickel KG. Beneficial effect of Aluminium on the oxidation behvior of precursor-derived ceramics. In: High Temperature Corrosion and Materials Chemistry IV. Opila E, Ed. Washington, USA: The Electrochemical Society, 2001: 325–338.
Müller A, Gerstel P, Butchereit E, et al. Si/B/C/N/Al precursor-derived ceramics: Synthesis, high temperature behaviour and oxidation resistance. J Eur Ceram Soc 2004, 24: 3409–3417.
Shan QL, Xue YD, Hu JB, et al. More effective crack self-healing capability of SiCf/SiC-B4C with Al2O3 modified under wet environment. J Am Ceram Soc 2020, 103: 7247–7258.
Shan QL, Wang QL, Xue YD, et al. The surface cracking resistance of Al2O3-modified SiCf/SiC-B4C composites after cyclic oxidation in wet environment. Adv Eng Mater 2019, 21: 1900458.
Miao Y, Yang ZH, Liang B, et al. A novel in situ synthesis of SiBCN-Zr composites prepared by a sol-gel process and spark plasma sintering. Dalton Trans 2016, 45: 12739–12744.
Miao Y, Yang ZH, Liang B, et al. Oxidation behavior of SiBCN-Zr composites at 1500 °C prepared by reactive spark plasma sintering. Corros Sci 2018, 132: 293–299.
Miao Y, Yang ZH, Wang WX, et al. Microstructure and thermal shock behavior of sol-gel introduced ZrB2 reinforced SiBCN matrix. J Sol Gel Sci Technol 2018, 86: 365–373.
Yao XY, Li HJ, Zhang YL, et al. A SiC-Si-ZrB2 multiphase oxidation protective ceramic coating for SiC-coated carbon/carbon composites. Ceram Int 2012, 38: 2095–2100.
Miao Y, Zhang FN, Yang ZH, et al. Incorporation of BN-coated carbon fibers into ZrB2/SiBCN ceramic composites and their ablation behavior. J Eur Ceram Soc 2020, 40: 1078–1085.
Li DX, Yang ZH, Jia DC, et al. Preparation, microstructures, mechanical properties and oxidation resistance of SiBCN/ZrB2-ZrN ceramics by reactive hot pressing. J Eur Ceram Soc 2015, 35: 4399–4410.
Kaiser A, Lobert M, Telle R. Thermal stability of zircon (ZrSiO4). J Eur Ceram Soc 2008, 28: 2199–2211.
Ouyang HB, Li CY, Huang JF, et al. Self-healing ZrB2-SiO2 oxidation resistance coating for SiC coated carbon/carbon composites. Corros Sci 2016, 110: 265–272.
Wang SH, Zhang YC, Sun Y, et al. Synthesis and characteristic of SiBCN/HfN ceramics with high temperature oxidation resistance. J Alloys Compd 2016, 685: 828–835.
Luan XG, Zhang JH, Wang L, et al. Wet oxidation behavior of C/SiC-SiHf(B)CN composites at high temperature. Adv Compos Hybrid Mater 2020, 3: 415–429.
Verdon C, Szwedek O, Allemand A, et al. High temperature oxidation of two- and three-dimensional hafnium carbide and silicon carbide coatings. J Eur Ceram Soc 2014, 34: 879–887.
Wang YJ, Li HJ, Fu QG, et al. SiC/HfC/SiC ablation resistant coating for carbon/carbon composites. Surf Coat Technol 2012, 206: 3883–3887.
Huang D, Zhang MY, Huang QZ, et al. Mechanical property, oxidation and ablation resistance of C/C-ZrB2-ZrC-SiC composite fabricated by polymer infiltration and pyrolysis with preform of Cf/ZrB2. J Mater Sci Technol 2017, 33: 481–486.
Shi XH, Huo JH, Zhu JL, et al. Ablation resistance of SiC-ZrC coating prepared by a simple two-step method on carbon fiber reinforced composites. Corros Sci 2014, 88: 49–55.
Jia YJ, Li HJ, Fu QG, et al. A ZrC-SiC/ZrC-LaB6/ZrC multilayer ablation resistance coating for SiC-coated carbon/carbon composites. Surf Coat Technol 2017, 309: 545–553.