Instrumented nanoindentation in musculoskeletal research
Tài liệu tham khảo
Abraham, 2015, Multiscale predictors of femoral neck in situ strength in aging women: contributions of BMD, cortical porosity, reference point indentation, and nonenzymatic glycation, J. Bone Miner. Res., 30, 2207, 10.1002/jbmr.2568
Aifantis, 2011, Transverse mechanical properties of collagen fibers from nanoindentation, J. Mater. Sci. Mater. Med., 22, 1375, 10.1007/s10856-011-4320-9
Alves, 2018, Improved tribocorrosion performance of bio-functionalized TiO2 nanotubes under two-cycle sliding actions in artificial saliva, J. Mech. Behav. Biomed. Mater., 80, 143, 10.1016/j.jmbbm.2018.01.038
Anstis, 1981, A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements, J. Am. Ceram. Soc., 64, 533, 10.1111/j.1151-2916.1981.tb10320.x
Aruwajoye, 2017, Material properties of bone in the femoral head treated with ibandronate and BMP-2 following ischemic osteonecrosis, J. Orthop. Res., 35, 1453, 10.1002/jor.23402
Asgari, 2019, Material anisotropy and elasticity of cortical and trabecular bone in the adult mouse femur via AFM indentation, J. Mech. Behav. Biomed. Mater., 93, 81, 10.1016/j.jmbbm.2019.01.024
Aziz, 2017, Mechanical characterization of sequentially layered photo-clickable thiol-ene hydrogels, J. Mech. Behav. Biomed. Mater., 65, 454, 10.1016/j.jmbbm.2016.09.007
Balooch, 2004, Evaluation of a new modulus mapping technique to investigate microstructural features of human teeth, J. Biomech., 37, 1223, 10.1016/j.jbiomech.2003.12.012
Balooch, 2007, The aminobisphosphonate risedronate preserves localized mineral and material properties of bone in the presence of glucocorticoids, Arthritis Rheum., 56, 3726, 10.1002/art.22976
Bergholt, 2019, Raman spectroscopy: guiding light for the extracellular matrix, Front. Bioeng. Biotechnol., 7, 303, 10.3389/fbioe.2019.00303
Berman, 2022, Effects of Raloxifene and tibial loading on bone mass and mechanics in male and female mice, Connect. Tissue Res., 63, 3, 10.1080/03008207.2020.1865938
Beutel, 2015, Characterization of damage mechanisms associated with reference point indentation in human bone, Bone, 75, 1, 10.1016/j.bone.2015.01.019
Bi, 2011, Raman and mechanical properties correlate at whole bone- and tissue-levels in a genetic mouse model, J. Biomech., 44, 297, 10.1016/j.jbiomech.2010.10.009
Boyde, 2011, Cartilage damage involving extrusion of mineralisable matrix from the articular calcified cartilage and subchondral bone, Eur. Cell. Mater., 21, 470, 10.22203/eCM.v021a35
Brodt, 1999, Growing C57Bl/6 mice increase whole bone mechanical properties by increasing geometric and material properties, J. Bone Miner. Res., 14, 2159, 10.1359/jbmr.1999.14.12.2159
Burket, 2011, Microstructure and nanomechanical properties in osteons relate to tissue and animal age, J. Biomech., 44, 277, 10.1016/j.jbiomech.2010.10.018
Busa, 2005, Rapid establishment of chemical and mechanical properties during lamellar bone formation, Calcif. Tissue Int., 77, 386, 10.1007/s00223-005-0148-y
Bushby, 2004, Nanoindentation of bone: comparison of specimens tested in liquid and embedded in polymethylmethacrylate, J. Mater. Res., 19, 24, 10.1557/jmr.2004.19.1.249
Cao, 2006, Compressive properties of mouse articular cartilage determined in a novel micro-indentation test method and biphasic finite element model, J. Biomech. Eng., 128, 766, 10.1115/1.2246237
Carter, 1977, The compressive behavior of bone as a two-phase porous structure, J. Bone Joint Surg. Am., 59, 954, 10.2106/00004623-197759070-00021
Chandrasekaran, 2017, Biomechanical properties of murine TMJ articular disc and condyle cartilage via AFM-nanoindentation, J. Biomech., 60, 134, 10.1016/j.jbiomech.2017.06.031
Chandrasekaran, 2021, Type V collagen regulates the structure and biomechanics of TMJ condylar cartilage: a fibrous-hyaline hybrid, Matrix Biol., 102, 1, 10.1016/j.matbio.2021.07.002
Chery, 2020, Early changes in cartilage pericellular matrix micromechanobiology portend the onset of post-traumatic osteoarthritis, Acta Biomater., 111, 267, 10.1016/j.actbio.2020.05.005
Chudoba, 1999, New possibilities of mechanical surface characterization with spherical indenters by comparison of experimental and theoretical results, Thin Solid Films, 355–356, 284, 10.1016/S0040-6090(99)00445-9
Cohen, 2013, Dynamic nanoindentation by instrumented nanoindentation and force microscopy: a comparative review, Beilstein J. Nanotechnol., 4, 815, 10.3762/bjnano.4.93
Connizzo, 2013, Structure-function relationships of postnatal tendon development: a parallel to healing, Matrix Biol., 32, 106, 10.1016/j.matbio.2013.01.007
Coutts, 2015, Variability in reference point microindentation and recommendations for testing cortical bone: location, thickness and orientation heterogeneity, J. Mech. Behav. Biomed. Mater., 46, 292, 10.1016/j.jmbbm.2015.02.004
Dall'Ara, 2013, Tissue properties of the human vertebral body sub-structures evaluated by means of microindentation, J. Mech. Behav. Biomed. Mater., 25, 23, 10.1016/j.jmbbm.2013.04.020
Dall'Ara, 2012, Microindentation can discriminate between damaged and intact human bone tissue, Bone, 50, 925, 10.1016/j.bone.2012.01.002
Diez-Perez, 2010, Microindentation for in vivo measurement of bone tissue mechanical properties in humans, J. Bone Miner. Res., 25, 1877, 10.1002/jbmr.73
Dokukin, 2015, High-resolution high-speed dynamic mechanical spectroscopy of cells and other soft materials with the help of atomic force microscopy, Sci. Rep., 5, 10.1038/srep12630
Donnelly, 2006, Effects of surface roughness and maximum load on the mechanical properties of cancellous bone measured by nanoindentation, J. Biomed. Mater. Res., 77, 426, 10.1002/jbm.a.30633
Donnelly, 2010, Effects of tissue age on bone tissue material composition and nanomechanical properties in the rat cortex, J. Biomed. Mater. Res., 92, 1048, 10.1002/jbm.a.32442
Doube, 2010, Combined nanoindentation testing and scanning electron microscopy of bone and articular calcified cartilage in an equine fracture predilection site, Eur. Cell. Mater., 19, 242, 10.22203/eCM.v019a23
Doyran, 2017, Nanoindentation modulus of murine cartilage: a sensitive indicator of the initiation and progression of post-traumatic osteoarthritis, Osteoarthritis Cartilage, 25, 108, 10.1016/j.joca.2016.08.008
Duarte Sosa, 2015, Are the high hip fracture rates among Norwegian women explained by impaired bone material properties?, J. Bone Miner. Res., 30, 1784, 10.1002/jbmr.2537
Ebenstein, 2006, Nanoindentation of biological materials, Nano Today, 1, 26, 10.1016/S1748-0132(06)70077-9
Efremov, 2019, Anisotropy vs isotropy in living cell indentation with AFM, Sci. Rep., 9, 5757, 10.1038/s41598-019-42077-1
Eidelman, 2009, Microstructure and mineral composition of dystrophic calcification associated with the idiopathic inflammatory myopathies, Arthritis Res. Ther., 11, R159, 10.1186/ar2841
Emig, 2019, Human atrial fibroblast adaptation to heterogeneities in substrate stiffness, Front. Physiol., 10, 1526, 10.3389/fphys.2019.01526
Faingold, 2014, The effect of hydration on mechanical anisotropy, topography and fibril organization of the osteonal lamellae, J. Biomech., 47, 367, 10.1016/j.jbiomech.2013.11.022
Fan, 2003, Effects of viscoelasticity and time-dependent plasticity on nanoindentation measurements of human cortical bone, J. Biomed. Mater. Res., 67, 208, 10.1002/jbm.a.10027
Feng, 2012, Mechanical properties of porcine femoral cortical bone measured by nanoindentation, J. Biomech., 45, 1775, 10.1016/j.jbiomech.2012.05.001
Ferguson, 2003, Nanomechanical properties and mineral concentration in articular calcified cartilage and subchondral bone, J. Anat., 203, 191, 10.1046/j.1469-7580.2003.00193.x
Fischer-Cripps, 2006, Critical review of analysis and interpretation of nanoindentation test data, Surf. Coating. Technol., 200, 4153, 10.1016/j.surfcoat.2005.03.018
Franke, 2011, Dynamic nanoindentation of articular porcine cartilage, Mater. Sci. Eng. C, 31, 789, 10.1016/j.msec.2010.12.005
Fratzl-Zelman, 2009, Combination of nanoindentation and quantitative backscattered electron imaging revealed altered bone material properties associated with femoral neck fragility, Calcif. Tissue Int., 85, 335, 10.1007/s00223-009-9289-8
Fraulob, 2020, Multimodal characterization of the bone-implant interface using Raman spectroscopy and nanoindentation, Med. Eng. Phys., 84, 60, 10.1016/j.medengphy.2020.07.013
Gamonpilas, 2004, On the effect of substrate properties on the indentation behaviour of coated systems, Mater. Sci. Eng., 380, 52, 10.1016/j.msea.2004.04.038
Gamsjaeger, 2014, Vibrational spectroscopic imaging for the evaluation of matrix and mineral chemistry, Curr. Osteoporos. Rep., 12, 454, 10.1007/s11914-014-0238-8
Gonzalez, 2014, Mechanical properties of polyvinylalcohol/hydroxyapatite cryogel as potential artificial cartilage, J. Mech. Behav. Biomed. Mater., 34, 47, 10.1016/j.jmbbm.2014.01.019
Gourion-Arsiquaud, 2007, Fourier transform infrared and Raman microspectroscopy and microscopic imaging of bone, Curr. Opin. Orthop., 18, 499, 10.1097/BCO.0b013e3282b97133
Granke, 2014, Insights into reference point indentation involving human cortical bone: sensitivity to tissue anisotropy and mechanical behavior, J. Mech. Behav. Biomed. Mater., 37, 174, 10.1016/j.jmbbm.2014.05.016
Granke, 2015, Identifying novel clinical surrogates to assess human bone fracture toughness, J. Bone Miner. Res., 30, 1290, 10.1002/jbmr.2452
Grant, 2001, Mapping the structural properties of the lumbosacral vertebral endplates, Spine, 26, 889, 10.1097/00007632-200104150-00012
Grant, 2002, The effects of bone density and disc degeneration on the structural property distributions in the lower lumbar vertebral endplates, J. Orthop. Res., 20, 1115, 10.1016/S0736-0266(02)00039-6
Güerri-Fernández, 2013, Microindentation for in vivo measurement of bone tissue material properties in atypical femoral fracture patients and controls, J. Bone Miner. Res., 28, 162, 10.1002/jbmr.1731
Gupta, 2005, Two different correlations between nanoindentation modulus and mineral content in the bone-cartilage interface, J. Struct. Biol., 149, 138, 10.1016/j.jsb.2004.10.010
Gupta, 2006, Mechanical modulation at the lamellar level in osteonal bone, J. Mater. Res., 21, 1913, 10.1557/jmr.2006.0234
Habelitz, 2002, Nanoindentation and storage of teeth, J. Biomech., 35, 995, 10.1016/S0021-9290(02)00039-8
Han, 2021
Han, 2019, Decorin regulates the aggrecan network integrity and biomechanical functions of cartilage extracellular matrix, ACS Nano, 13, 11320, 10.1021/acsnano.9b04477
Han, 2017, AFM-nanomechanical test: an interdisciplinary tool that links the understanding of cartilage and meniscus biomechanics, osteoarthritis degeneration, and tissue engineering, ACS Biomater. Sci. Eng., 3, 2033, 10.1021/acsbiomaterials.7b00307
Han, 2019, Rate-dependent crack nucleation in cartilage under microindentation, J. Mech. Behav. Biomed. Mater., 96, 186, 10.1016/j.jmbbm.2019.04.015
Han, 2018, Uncoupled poroelastic and intrinsic viscoelastic dissipation in cartilage, J. Mech. Behav. Biomed. Mater., 84, 28, 10.1016/j.jmbbm.2018.04.024
Han, 2011, Time-dependent nanomechanics of cartilage, Biophys. J., 100, 1846, 10.1016/j.bpj.2011.02.031
Hayot, 2012, Viscoelastic properties of cell walls of single living plant cells determined by dynamic nanoindentation, J. Exp. Bot., 63, 2525, 10.1093/jxb/err428
He, 2007, Influence of environment on the mechanical behaviour of mature human enamel, Biomaterials, 28, 4512, 10.1016/j.biomaterials.2007.06.020
Heveran, 2019, Chronic kidney disease and aging differentially diminish bone material and microarchitecture in C57Bl/6 mice, Bone, 127, 91, 10.1016/j.bone.2019.04.019
Hoffler, 2005, An application of nanoindentation technique to measure bone tissue Lamellae properties, J. Biomech. Eng., 127, 1046, 10.1115/1.2073671
Huang, 2018, A calcium mediated mechanism coordinating vascular smooth muscle cell adhesion during KCl activation, Front. Physiol., 9, 1810, 10.3389/fphys.2018.01810
Imbert, 2014, Mechanical and mineral properties of osteogenesis imperfecta human bones at the tissue level, Bone, 65, 18, 10.1016/j.bone.2014.04.030
Indermaur, 2021, Compressive strength of iliac bone ECM is not reduced in osteogenesis imperfecta and increases with mineralization, J. Bone Miner. Res., 36, 1364, 10.1002/jbmr.4286
Islam, 2012, Mechanistic modeling of a nanoscratch test for determination of in situ toughness of bone, J. Mech. Behav. Biomed. Mater., 5, 156, 10.1016/j.jmbbm.2011.08.019
Jenkins, 2016, Site-dependent reference point microindentation complements clinical measures for improved fracture risk assessment at the human femoral neck, J. Bone Miner. Res., 31, 196, 10.1002/jbmr.2605
Johnston, 2011, Predicting subchondral bone stiffness using a depth-specific CT topographic mapping technique in normal and osteoarthritic proximal tibiae, Clin. Biomech., 26, 1012, 10.1016/j.clinbiomech.2011.06.009
Joves, 2014, Nanoindentation hardness of intertubular dentin in sound, demineralized and natural caries-affected dentin, J. Mech. Behav. Biomed. Mater., 32, 39, 10.1016/j.jmbbm.2013.12.017
Kasra, 1994, Effect of long-term ovariectomy on bone mechanical properties in young female cynomolgus monkeys, Bone, 15, 557, 10.1016/8756-3282(94)90281-X
Kataruka, 2017, Microscopic assessment of bone toughness using scratch tests, Bone Rep., 6, 17, 10.1016/j.bonr.2016.12.001
Katsamenis, 2015, Toughness and damage susceptibility in human cortical bone is proportional to mechanical inhomogeneity at the osteonal-level, Bone, 76, 158, 10.1016/j.bone.2015.03.020
Kaufman, 2009, Surface detection errors cause overestimation of the modulus in nanoindentation on soft materials, J. Mech. Behav. Biomed. Mater., 2, 312, 10.1016/j.jmbbm.2008.08.004
Kavukcuoglu, 2007, Osteopontin deficiency and aging on nanomechanics of mouse bone, J. Biomed. Mater. Res., 83, 136, 10.1002/jbm.a.31081
Kazakia, 2006, Effects of in vitro bone formation on the mechanical properties of a trabeculated hydroxyapatite bone substitute, J. Biomed. Mater. Res., 77, 688, 10.1002/jbm.a.30644
Kim, 2014, Elastic, viscoelastic, and fracture properties of bone tissue measured by nanoindentation, 1321
Kim, 2010, Relationships of viscosity with contact hardness and modulus of bone matrix measured by nanoindentation, J. Biomech. Eng., 132, 10.1115/1.4000936
Kim, 2015, Regional variation of bone tissue properties at the human mandibular condyle, Bone, 77, 98, 10.1016/j.bone.2015.04.024
Kim, 2020, Bone regeneration into side openings and hollow inner channel of a dental implant, J. Mech. Behav. Biomed. Mater., 101, 10.1016/j.jmbbm.2019.103416
Kim, 2014, Reduced tissue-level stiffness and mineralization in osteoporotic cancellous bone, Calcif. Tissue Int., 95, 125, 10.1007/s00223-014-9873-4
Krege, 2016, Reference point indentation is insufficient for detecting alterations in traditional mechanical properties of bone under common experimental conditions, Bone, 87, 97, 10.1016/j.bone.2016.04.002
Kruzic, 2009, Indentation techniques for evaluating the fracture toughness of biomaterials and hard tissues, J. Mech. Behav. Biomed. Mater., 2, 384, 10.1016/j.jmbbm.2008.10.008
Lane, 2006, Glucocorticoid-treated mice have localized changes in trabecular bone material properties and osteocyte lacunar size that are not observed in placebo-treated or estrogen-deficient mice, J. Bone Miner. Res., 21, 466, 10.1359/JBMR.051103
Lee, 2010, Dynamic mechanical properties of the tissue-engineered matrix associated with individual chondrocytes, J. Biomech., 43, 469, 10.1016/j.jbiomech.2009.09.053
Levenston, 1994, Improved method for analysis of whole bone torsion tests, J. Bone Miner. Res., 9, 1459, 10.1002/jbmr.5650090919
Li, 2015, Biomechanical properties of murine meniscus surface via AFM-based nanoindentation, J. Biomech., 48, 1364, 10.1016/j.jbiomech.2015.02.064
Li, 2020, Mediation of cartilage matrix degeneration and fibrillation by decorin in post-traumatic osteoarthritis, Arthritis Rheumatol., 72, 1266, 10.1002/art.41254
Li, 2017, Micromechanical anisotropy and heterogeneity of the meniscus extracellular matrix, Acta Biomater., 54, 356, 10.1016/j.actbio.2017.02.043
Li, 2018, Impacts of maturation on the micromechanics of the meniscus extracellular matrix, J. Biomech., 72, 252, 10.1016/j.jbiomech.2018.02.037
Li, 2007, Microindentation test for assessing the mechanical properties of cartilaginous tissues, J. Biomed. Mater. Res. B Appl. Biomater., 80B, 25, 10.1002/jbm.b.30564
Listrat, 2016, How muscle structure and composition influence meat and flesh quality, Sci. World J., 2016, 10.1155/2016/3182746
Liu, 2017, Progress in indentation study of materials via both experimental and numerical methods, Crystals, 7, 258, 10.3390/cryst7100258
Lu, 2009, Electrospun submicron bioactive glass fibers for bone tissue scaffold, J. Mater. Sci. Mater. Med., 20, 793, 10.1007/s10856-008-3649-1
Mabilleau, 2014, Beneficial effects of a N-terminally modified GIP agonist on tissue-level bone material properties, Bone, 63, 61, 10.1016/j.bone.2014.02.013
Main, 2020, Murine axial compression tibial loading model to study bone mechanobiology: implementing the model and reporting results, J. Orthop. Res., 38, 233, 10.1002/jor.24466
Mandair, 2015, Contributions of Raman spectroscopy to the understanding of bone strength, BoneKEy Rep., 4, 620, 10.1038/bonekey.2014.115
Martin, 1998, 29
Matsiko, 2013, Advanced strategies for articular cartilage defect repair, Materials, 6, 637, 10.3390/ma6020637
Mellibovsky, 2015, Bone tissue properties measurement by reference point indentation in glucocorticoid-induced osteoporosis, J. Bone Miner. Res., 30, 1651, 10.1002/jbmr.2497
Mieczkowska, 2013, Glucose-dependent insulinotropic polypeptide (GIP) receptor deletion leads to reduced bone strength and quality, Bone, 56, 337, 10.1016/j.bone.2013.07.003
Miller, 2010, Use of microindentation to characterize the mechanical properties of articular cartilage: comparison of biphasic material properties across length scales, Osteoarthritis Cartilage, 18, 1051, 10.1016/j.joca.2010.04.007
Milovanovic, 2014, Nano-structural, compositional and micro-architectural signs of cortical bone fragility at the superolateral femoral neck in elderly hip fracture patients vs. healthy aged controls, Exp. Gerontol., 55, 19, 10.1016/j.exger.2014.03.001
Milovanovic, 2015, Multi-level characterization of human femoral cortices and their underlying osteocyte network reveal trends in quality of young, aged, osteoporotic and antiresorptive-treated bone, Biomaterials, 45, 46, 10.1016/j.biomaterials.2014.12.024
Mirzaali, 2016, Mechanical properties of cortical bone and their relationships with age, gender, composition and microindentation properties in the elderly, Bone, 93, 196, 10.1016/j.bone.2015.11.018
Mittra, 2006, The effects of embedding material, loading rate and magnitude, and penetration depth in nanoindentation of trabecular bone, J. Biomed. Mater. Res., 79A, 86, 10.1002/jbm.a.30742
Mow, 2005, Basic orthopaedic biomechanics and mechano-biology
Nayar, 2012, Elastic and viscoelastic characterization of agar, J. Mech. Behav. Biomed. Mater., 7, 60, 10.1016/j.jmbbm.2011.05.027
Ng, 2007, Nanomechanical properties of individual chondrocytes and their developing growth factor-stimulated pericellular matrix, J. Biomech., 40, 1011, 10.1016/j.jbiomech.2006.04.004
Noshchenko, 2013, Correlation of vertebral strength topography with 3-dimensional computed tomographic structure, Spine, 38, 339, 10.1097/BRS.0b013e31826c670d
Nyman, 2011, Differential effects between the loss of MMP-2 and MMP-9 on structural and tissue-level properties of bone, J. Bone Miner. Res., 26, 1252, 10.1002/jbmr.326
Ojanen, 2015, Relationships between tissue composition and viscoelastic properties in human trabecular bone, J. Biomech., 48, 269, 10.1016/j.jbiomech.2014.11.034
Olesiak, 2010, Viscous-elastic-plastic behavior of bone using Berkovich nanoindentation, Mech. Time-Dependent Mater., 14, 111, 10.1007/s11043-009-9098-5
Oliver, 1992, An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments, J. Mater. Res., 7, 1564, 10.1557/JMR.1992.1564
Oxland, 2003, Effects of endplate removal on the structural properties of the lower lumbar vertebral bodies, Spine, 28, 771, 10.1097/01.BRS.0000060259.94427.11
Oyen, 2012, Size effects in indentation of hydrated biological tissues, J. Mater. Res., 27, 245, 10.1557/jmr.2011.322
Park, 2004, Mechanical response of bovine articular cartilage under dynamic unconfined compression loading at physiological stress levels, Osteoarthritis Cartilage, 12, 65, 10.1016/j.joca.2003.08.005
Paschalis, 2011, Lathyrism-induced alterations in collagen cross-links influence the mechanical properties of bone material without affecting the mineral, Bone, 49, 1232, 10.1016/j.bone.2011.08.027
Pathak, 2011, Measuring the dynamic mechanical response of hydrated mouse bone by nanoindentation, J. Mech. Behav. Biomed. Mater., 4, 34, 10.1016/j.jmbbm.2010.09.002
Pathak, 2011, Measuring the dynamic mechanical response of hydrated mouse bone by nanoindentation, J. Mech. Behav. Biomed. Mater., 4, 34, 10.1016/j.jmbbm.2010.09.002
Peters, 2018, The effect of ageing and osteoarthritis on the mechanical properties of cartilage and bone in the human knee joint, Sci. Rep., 8, 5931, 10.1038/s41598-018-24258-6
Pharr, 2011, On the generality of the relationship among contact stiffness, contact area, and elastic modulus during indentation, J. Mater. Res., 7, 61
Polly, 2012, Intrinsic material properties of trabecular bone by nanoindentation testing of biopsies taken from healthy women before and after menopause, Calcif. Tissue Int., 90, 286, 10.1007/s00223-012-9575-8
Qian, 2018, Nanoindentation of soft biological materials, Micromachines, 9, 10.3390/mi9120654
Qian, 2018, Influence of strain rate on indentation response of porcine brain, J. Mech. Behav. Biomed. Mater., 82, 210, 10.1016/j.jmbbm.2018.03.031
Qian, 2020, Investigation of nanoscale failure behaviour of cortical bone under stress by AFM, J. Mech. Behav. Biomed. Mater., 112, 10.1016/j.jmbbm.2020.103989
Querido, 2021, Applications of vibrational spectroscopy for analysis of connective tissues, Molecules, 26, 10.3390/molecules26040922
Raghavan, 2012, Age-specific profiles of tissue-level composition and mechanical properties in murine cortical bone, Bone, 50, 942, 10.1016/j.bone.2011.12.026
Rodriguez-Florez, 2015, An investigation of the mineral in ductile and brittle cortical mouse bone, J. Bone Miner. Res., 30, 786, 10.1002/jbmr.2414
Roschger, 2010, Bone material quality in transiliac bone biopsies of postmenopausal osteoporotic women after 3 years of strontium ranelate treatment, J. Bone Miner. Res., 25, 891, 10.1359/jbmr.091028
Roy, 1999, Mechanical and morphological variation of the human lumbar vertebral cortical and trabecular bone, J. Biomed. Mater. Res., 44, 191, 10.1002/(SICI)1097-4636(199902)44:2<191::AID-JBM9>3.0.CO;2-G
Rudäng, 2016, Bone material strength is associated with areal BMD but not with prevalent fractures in older women, Osteoporos. Int., 27, 1585, 10.1007/s00198-015-3419-0
Ryou, 2012, Nanoscopic dynamic mechanical properties of intertubular and peritubular dentin, J. Mech. Behav. Biomed. Mater., 7, 3, 10.1016/j.jmbbm.2011.08.010
Ryou, 2015, Importance of age on the dynamic mechanical behavior of intertubular and peritubular dentin, J. Mech. Behav. Biomed. Mater., 42, 229, 10.1016/j.jmbbm.2014.11.021
Sakamoto, 2009, Viscoelastic properties of microstructural components of rat cortical bone tissue as measured by dynamic nanoindentation, J. Jpn. Soc. Exp. Mech., 9, s151
Samuels, 1957, An experimental investigation of the deformed zone associated with indentation hardness impressions, J. Mech. Phys. Solid., 5, 125, 10.1016/0022-5096(57)90056-X
Seidel, 2019, Mechanical properties of stingray tesserae: high-resolution correlative analysis of mineral density and indentation moduli in tessellated cartilage, Acta Biomater., 96, 421, 10.1016/j.actbio.2019.06.038
Sepitka, 2014, Compression tests of a living cell: a contact detection problem, Comput. Methods Biomech. Biomed. Eng., 17, 40, 10.1080/10255842.2014.931093
Sferra, 1995, Biomechanical analysis of canine bone lengthened by the callotasis method, Clin. Orthop. Relat. Res., 222–6
Shah, 2019, 50 years of scanning electron microscopy of bone-a comprehensive overview of the important discoveries made and insights gained into bone material properties in health, disease, and taphonomy, Bone Res., 7, 15, 10.1038/s41413-019-0053-z
Shah, 2018, Multiscale characterization of cortical bone composition, microstructure, and nanomechanical properties in experimentally induced osteoporosis, J. Biomed. Mater. Res., 106, 997, 10.1002/jbm.a.36294
Sharma, 2018, The effects of estrogen deficiency on cortical bone microporosity and mineralization, Bone, 110, 1, 10.1016/j.bone.2018.01.019
Sheng, 2021, AFM-based indentation method for measuring the relaxation property of living cells, J. Biomech., 122, 10.1016/j.jbiomech.2021.110444
Sherk, 2021, Sex differences in the effect of diet, obesity, and exercise on bone quality and fracture toughness, Bone, 145, 10.1016/j.bone.2021.115840
Shoaib, 2020, Nanoscale insight into the degradation mechanisms of the cartilage articulating surface preceding OA, Biomater. Sci., 8, 3944, 10.1039/D0BM00496K
Silva, 2013, Nanostructured 3D constructs based on chitosan and chondroitin sulphate multilayers for cartilage tissue engineering, PLoS One, 8
Sinder, 2016, Effect of anti-sclerostin therapy and osteogenesis imperfecta on tissue-level properties in growing and adult mice while controlling for tissue age, Bone, 84, 222, 10.1016/j.bone.2016.01.001
Smith, 2010, The role of mineral content in determining the micromechanical properties of discrete trabecular bone remodeling packets, J. Biomech., 43, 3144, 10.1016/j.jbiomech.2010.07.038
Staunton, 2016, Correlating confocal microscopy and atomic force indentation reveals metastatic cancer cells stiffen during invasion into collagen I matrices, Sci. Rep., 6, 10.1038/srep19686
Sudharshan Phani, 2019, A critical assessment of the effect of indentation spacing on the measurement of hardness and modulus using instrumented indentation testing, Mater. Des., 164, 10.1016/j.matdes.2018.107563
Tamay, 2022, Corrosion resistance and cytocompatibility of magnesium-calcium alloys modified with zinc- or gallium-doped calcium phosphate coatings, ACS Appl. Mater. Interfaces, 14, 104, 10.1021/acsami.1c16307
Taylor, 2020, Raman and Fourier transform infrared imaging for characterization of bone material properties, Bone, 139, 10.1016/j.bone.2020.115490
Thurner, 2009, The effect of NaF in vitro on the mechanical and material properties of trabecular and cortical bone, Adv. Mater., 21, 451, 10.1002/adma.200801204
Toledano, 2017, Nanostructure in the trabecular bone of postmenopausal women: mechanical and chemical analysis, Injury, 48, S26, 10.1016/S0020-1383(17)30791-X
Toledano, 2018, Assessing bone quality through mechanical properties in postmenopausal trabecular bone, Injury, 49, S3, 10.1016/j.injury.2018.07.035
Tovar, 2018, Form and functional repair of long bone using 3D-printed bioactive scaffolds, J. Tiss. Eng. Regen. Med., 12, 1986, 10.1002/term.2733
Ünal, 2016, Fundamentals of musculoskeletal biomechanics, 15
Vahidi, 2021, Bone biomechanical properties and tissue-scale bone quality in a genetic mouse model of familial dysautonomia, Osteoporos. Int., 32, 2335, 10.1007/s00198-021-06006-1
Wahlquist, 2017, Indentation mapping revealed poroelastic, but not viscoelastic, properties spanning native zonal articular cartilage, Acta Biomater., 64, 41, 10.1016/j.actbio.2017.10.003
Wang, 2020, Type III collagen is a key regulator of the collagen fibrillar structure and biomechanics of articular cartilage and meniscus, Matrix Biol., 85–86, 47, 10.1016/j.matbio.2019.10.001
Wang, 2018, Solute transport in the bone lacunar-canalicular system (LCS), Curr. Osteoporos. Rep., 16, 32, 10.1007/s11914-018-0414-3
Wang, 2019, Finite element simulation for the effect of loading rate on visco-hyperelastic characterisation of soft materials by spherical nanoindentation, IET Nanobiotechnol., 13, 578, 10.1049/iet-nbt.2019.0046
Wilusz, 2012, Immunofluorescence-guided atomic force microscopy to measure the micromechanical properties of the pericellular matrix of porcine articular cartilage, J. R. Soc. Interface, 9, 2997, 10.1098/rsif.2012.0314
Wilusz, 2014, The structure and function of the pericellular matrix of articular cartilage, Matrix Biol., 39, 25, 10.1016/j.matbio.2014.08.009
Wilusz, 2013, Micromechanical mapping of early osteoarthritic changes in the pericellular matrix of human articular cartilage, Osteoarthritis Cartilage, 21, 1895, 10.1016/j.joca.2013.08.026
Wu, 2018, Young's modulus of trabecular bone at the tissue level: a review, Acta Biomater., 78, 1, 10.1016/j.actbio.2018.08.001
Xu, 2003, Atomic force microscopy and nanoindentation characterization of human lamellar bone prepared by microtome sectioning and mechanical polishing technique, J. Biomed. Mater. Res., 67, 719, 10.1002/jbm.a.10109
Yi, 2020, Comparison of dynamic mechanical properties of dentin between deciduous and permanent teeth, Connect. Tissue Res., 1
Yu, 2013, Strontium ranelate reduces cartilage degeneration and subchondral bone remodeling in rat osteoarthritis model, Acta Pharmacol. Sin., 34, 393, 10.1038/aps.2012.167
Yvanoff, 2022, Development of bone cell microarrays in microfluidic chips for studying osteocyte-osteoblast communication under fluid flow mechanical loading, Biofabrication, 14
Zhou, 2017, Rho kinase regulates aortic vascular smooth muscle cell stiffness via actin/SRF/myocardin in hypertension, Cell. Physiol. Biochem., 44, 701, 10.1159/000485284
Zhuang, 2021, Preliminary study on mechanical characteristics of maxillofacial soft and hard tissues for virtual surgery, Int. J. Comput. Assist. Radiol. Surg., 16, 151, 10.1007/s11548-020-02257-1
Zysset, 1999, Elastic modulus and hardness of cortical and trabecular bone lamellae measured by nanoindentation in the human femur, J. Biomech., 32, 1005, 10.1016/S0021-9290(99)00111-6