In vitro comparison of conventional crowns and a new all-ceramic system

Journal of Dentistry - Tập 21 - Trang 47-51 - 1993
N.J.A. Grey1, V. Piddock1, M.A. Wilson1
1Department of Restorative Dentistry, University of Manchester Dental Hospital, Manchester, UK

Tài liệu tham khảo

Adair, 1984, The castable ceramic crown, Int. J Periodont. Rest. Dent., 2, 33 Ludwig, 1991, Untersuchungen zur Bruchfestigkeit von Vollkeramikkronen, Dent. Labor., 39, 647 Hobo, 1985, Castable apatite ceramics as a new biocompatible restorative material. II. Fabrication of the restoration, Quintessence Int., 16, 207 Maruyama, 1991, Clinical use of a new castable glass ceramic material, Int. J. Prosthodont., 4, 138 McLean, 1965, The reinforcement of dental porcelain with ceramic oxides, Br. Dent. J., 119, 251 Piddock, 1987, The mechanical strength and microstructure of all-ceramic crowns, J. Dent., 15, 153, 10.1016/0300-5712(87)90141-2 Pröbster, 1992, Slip-casting alumina ceramics for crown and bridge restorations, Quintessence Int., 23, 25 Sozio, 1983, The shrink-free ceramic crown, J. Prosthet. Dent., 49, 182, 10.1016/0022-3913(83)90497-3