In vitro ageing of composite restorative materials

Clinical Materials - Tập 3 - Trang 209-221 - 1988
James L. Drummond1
1Department of Operative Dentistry, University of Illinois at Chicago, USA

Tài liệu tham khảo

Craig, 1981, Chemistry, composition, and properties of composite resins, Dent Clin North Am, 25, 219, 10.1016/S0011-8532(22)02805-1 Lutz, 1983, Dental restorative resins, Dent Clin North Am, 27, 697, 10.1016/S0011-8532(22)02284-4 Powers, 1981, In vitro accelerated ageing of composites and a sealant, J Dent Res, 60, 1672, 10.1177/00220345810600090701 Powers, 1983, Comparison of in vitro and in vivo wear of composites, J Dent Res, 62, 1089, 10.1177/00220345830620101801 McKinney, 1982, Relationship between subsurface damage and wear of dental restorative composites, J Dent Res, 61, 1083, 10.1177/00220345820610091101 Söderholm, 1984, Hydrolytic degradation of dental composites, J Dent Res, 63, 1248, 10.1177/00220345840630101701 Söderholm, 1981, Degradation of filler in experimental composites, J Dent Res, 60, 1867, 10.1177/00220345810600110701 Söderholm, 1982, Relationship between compressive yield strength and filler fractions of PMMA composite, Acta Odontol Scand, 40, 145, 10.3109/00016358209012723 Braden, 1984, Water absorption characteristics of dental microfine composite filling materials, Biomat, 5, 369, 10.1016/0142-9612(84)90038-3 Draughn, 1979, Compressive fatigue limits of composite restorative materials, J Dent Res, 58, 1093, 10.1177/00220345790580031101 Wu, 1984, Subsurface damage layer of in vivo worn dental composite restorations, J Dent Res, 63, 675, 10.1177/00220345840630051401 Wu, 1982, Influence of chemicals on wear of dental composites, J Dent Res, 61, 1180, 10.1177/00220345820610101501 Carfagna, 1983, Effects of postcuring and water sorption on the mechanical properties of composite dental restorative materials, Biomat, 4, 228, 10.1016/0142-9612(83)90018-2 Söderholm, 1983, Effect of water on glass-filled methacrylate resins, J Mater Sci, 18, 2957, 10.1007/BF00700777 Calais, 1988, Influence of filler type and water exposure on flexural strength of experimental composite resins, J Dent Res, 67, 83640, 10.1177/00220345880670050801 1981, C674 International Standard 4049, 1978, Resin-based dental fillings, 1