Hot corrosion in gas turbine components
Tóm tắt
Từ khóa
Tài liệu tham khảo
Rapp, 1986, Chemistry and electrochemistry of the hot corrosion of metals, Corrosion, 42, 568, 10.5006/1.3583026
Stringer, 1987, High-temperature corrosion of superalloys, Mater. Sci. Technol., 3, 482, 10.1080/02670836.1987.11782259
Hancock, 1987, Vanadic and chloride attack of superalloys, Mater. Sci. Technol., 3, 536, 10.1080/02670836.1987.11782265
Tzvetkoff, 1995, Corrosion of nickel, iron, cobalt and their alloys in molten salt electrolytes: review, J. Mater. Sci., 30, 5561, 10.1007/BF00356688
Goward, 1998, Progress in coatings for gas turbine airfoils, Surf. Coat. Technol., 108-109, 73, 10.1016/S0257-8972(98)00667-7
Gurrappa, 1999, Hot corrosion behavior of CM 247 LC alloy in Na2SO4 and NaCl environments, Oxid. Met., 51, 353, 10.1023/A:1018831025272
Fawley, 1972, Superalloy progress, 3
Endres, 1974, Design principles of gas turbines, 1
Driver, 1981, The gas turbine engine, 1
Desforges, 1979, Metals and alloys for high temperature application: current status and future prospects, 1
Animated jet engine part. http://www.lerc.nasa.gov/WWW/K-12/airplane/animation/turbpar/entb.html
Pratt & Whitney home page. http://www.pratt-whitney.com
Engine terminology. http://www.pratt-whitney.com/engines/terminology.html
Wright IG. High-temperature corrosion. In: Metals handbook, vol. 13. 9th ed. Metals Park: ASM, 1987. p. 97–103.
Jaffee, 1979, High-temperature oxidation and corrosion of superalloys in the gas turbine (a review), 19
Santorelli, 1989, High-temperature corrosion of several commercial Fe–Cr–Ni alloys under a molten sodium sulphate deposit in oxidizing gaseous environments, Mater. Sci. Eng. A, A120, 283, 10.1016/0921-5093(89)90752-1
Pratt & Whitney. Sulphidation attack. S.I.L. no. 1035, 3017, 4010, 5028, 7022, 11008, 12020, 13011, October 1987.
Meier, 1989, A review of advances in high-temperature corrosion, Mater. Sci. Eng. A, 120, 1, 10.1016/0921-5093(89)90712-0
Goebel, 1970, Na2SO4-induced accelerated oxidation (hot corrosion) of nickel, Metall. Trans., 1, 1943, 10.1007/BF02642794
Goebel, 1970, The influence of sulfides on the oxidation behavior of nickel-base alloys, Metall. Trans., 1, 3421, 10.1007/BF03037874
Zhang, 1993, Design and development of hot corrosion-resistant nickel-base single-crystal superalloys by the d-electrons alloy design theory; II: effects of refractory metals Ti, Ta, and Nb on microstructures and properties, Metall. Trans. A, 24A, 2451, 10.1007/BF02646524
Rapp, 1981, The hot corrosion of metals by molten salts, 159
Otsuka, 1990, Hot corrosion of preoxidized Ni by a thin fused Na2SO4 film at 900°C, J. Electrochem. Soc., 137, 46, 10.1149/1.2086436
Beltran AM, Shores DA. Hot corrosion In: Sims CT, Hagel WC, editors. The superalloys. New York: Wiley, 1972. p. 317–39.
Bornstein, 1973, The relationship between relative oxide ion content of Na2SO4, the presence of liquid metal oxides and sulfidation attack, Metall. Trans., 4, 1799, 10.1007/BF02665406
Goebel, 1973, Mechanisms for the hot corrosion of nickel-base alloys, Metall. Trans., 4, 261, 10.1007/BF02649626
Zhang, 1987, Solubilities of CeO2, HfO2 and Y2O3 in fused Na2SO4–30 mol% NaVO3 and CeO2 in pure Na2SO4 at 900°C, Corrosion, 43, 348, 10.5006/1.3583869
Luthra KL. Mechanisms of low temperature hot corrosion. In: Rapp RA, editor. High temperature corrosion. Houston: NACE, 1983. p. 507-18.
Shih, 1989, Sub-melting point hot corrosion of alloys and coatings, Mater. Sci. Eng. A, A120, 277, 10.1016/0921-5093(89)90751-X
Nicholls, 1989, Comparison of hot-salt corrosion behaviour of superalloys in high and low velocity burner rigs, High Temp. Technol., 7, 193, 10.1080/02619180.1989.11753437
Simmons, 1955, Sodium sulfate in gas turbines, Corrosion, 11, 505t
Baudo, 1977, Coatings Corrosion, 1, 11
Gao, 1990, Electrochemical monitoring of high-temperature molten-salt corrosion, Oxid. Met., 33, 79, 10.1007/BF00665670
Hara, 1992, Electrochemical studies on hot corrosion of Ni–Cr–Al alloys in molten Na2SO4–NaCl, Mater. Trans. JIM, 33, 758, 10.2320/matertrans1989.33.758
Kim, 1994, Effects of galvanostatic treatments on hot corrosion of Ni, J. Mater. Sci. Lett., 13, 1573, 10.1007/BF00626513
Rahmel, 1987, Electrochemical aspects of molten-salt-enhanced corrosion, Mater. Sci. Eng., 87, 345, 10.1016/0025-5416(87)90397-1
Baudo, 1970, An electrochemical investigation of corrosion of ferritic steels in molten sulfates, Corrosion, 26, 193, 10.5006/0010-9312-26.7.293
Otsuka, 1990, Effects of chromate and vanadate anions on the hot corrosion of preoxidized Ni by a thin fused Na2SO4 film at 900°C, J. Electrochem. Soc., 137, 53, 10.1149/1.2086437
Zhang, 1993, Design and development of hot corrosion-resistant nickel-base single-crystal superalloys by the d-electrons alloy design theory; I: characterization of the phase stability, Metall. Trans. A, 24A, 2443, 10.1007/BF02646523
Bornstein, 1971, The role of sodium in the accelerated oxidation phenomenon termed sulfidation, Metall. Trans, 2, 2875, 10.1007/BF02813266
Nakamori, 1997, Hot corrosion and its prevention in high temperature heavy oil firing gas turbines, Mater. Sci. Forum, 251-254, 633, 10.4028/www.scientific.net/MSF.251-254.633
Gurrappa, 1998, Thermal barrier coatings for hot corrosion resistance of CM 247 LC superalloy, J. Mater. Sci. Lett., 17, 1267, 10.1023/A:1006547306416
Longa-Nava, 1996, Hot corrosion of nickel–chromium and nickel–chromium–aluminum thermal-spray coatings by sodium sulfate–sodium metavanadate salt, Corrosion, 52, 680, 10.5006/1.3292158
Huo, 1999, Evaluation of NiCrAlYSi overlay coating on Ni3Al based alloy IC-6 after an engine test, Surf. Coat. Technol., 114, 174, 10.1016/S0257-8972(99)00035-3
Brady, 1996, The oxidation and protection of gamma titanium aluminides, JOM, 48, 46, 10.1007/BF03223244
Tang, 2000, Effect of Al2O3 and enamel coatings on 900°C oxidation and hot corrosion behaviors of gamma-TiAl, Mater. Sci. Eng. A, A276, 70, 10.1016/S0921-5093(99)00513-4
Viswanathan R. Corrosion of combustion turbines. In: Metals handbook, vol. 13. 9th ed. Metals Park: ASM, 1987. p. 999–1001.