Hard and superhard nanocomposite coatings

Surface and Coatings Technology - Tập 125 Số 1-3 - Trang 322-330 - 2000
J. Musil1
1Department of Physics, University of West Bohemia, P.O. Box 314, 30614 Plzeň, Czech Republic

Tóm tắt

Từ khóa


Tài liệu tham khảo

Sproul, 1996, Science, 273, 889, 10.1126/science.273.5277.889

Holleck, 1985, J. Vac. Sci. Technol. A, 3, 234, 10.1116/1.572879

Holleck, 1986, J. Vac. Sci. Technol. A, 4, 2661, 10.1116/1.573700

Brookes, 1979, 383

Kramer, 1985, J. Vac. Sci. Technol. A, 3, 2439, 10.1116/1.572854

Münz, 1986, J. Vac. Sci. Technol. A, 4, 2717, 10.1116/1.573713

Voevodin, 1998, Diamond Relat. Mater., 7, 463, 10.1016/S0925-9635(97)00214-8

Sjöström, 1996, Phys. Rev. Lett., 76, 56, 10.1103/PhysRevLett.76.2205.2

Sjöström, 1996, J. Vac. Sci. Technol. A, 14, 56, 10.1116/1.579880

Helmersson, 1987, J. Appl. Phys., 62, 481, 10.1063/1.339770

Chu, 1993, Surf. Coat. Technol., 57, 13, 10.1016/0257-8972(93)90331-H

Vepřek, 1995, Appl. Phys. Lett., 66, 2640, 10.1063/1.113110

Musil, 1999, ZrN/Cu nanocomposite film — novel superhard material

Min, 1999, Thin Solid Films, 228, 204

Helmersson, 1987, J. Appl. Phys., 62, 481, 10.1063/1.339770

Mirakami, 1990, Appl. Phys. Lett., 57, 2654, 10.1063/1.104189

Shinn, 1992, J. Mater. Res., 7, 901, 10.1557/JMR.1992.0901

Chu, 1992, J. Vac. Sci. Technol. A, 10, 1604, 10.1116/1.578030

Chu, 1993, Surf. Coat. Technol., 57, 13, 10.1016/0257-8972(93)90331-H

Li, 1996, Appl. Phys. Lett., 68, 1211, 10.1063/1.115972

Wu, 1997, Thin Solid Films, 308/309, 113, 10.1016/S0040-6090(97)00429-X

Jensen, 1997, Surf. Coat. Technol., 94/95, 174, 10.1016/S0257-8972(97)00421-0

Jensen, 1998, J. Vac. Sci. Technol. A, 16, 1180, 10.1116/1.581122

Kryanowski, 1992, Mater. Res. Soc. Symp. Proc., 239, 509, 10.1557/PROC-239-509

Barnett, 1993, 1

Shinn, 1992, J. Mater. Res., 7, 901, 10.1557/JMR.1992.0901

Chu, 1995, J. Appl. Phys., 77, 4403, 10.1063/1.359467

Wendler, 1998, 6

Wendler, 1998, 423

Shih, 1992, Appl. Phys. Lett., 61, 654, 10.1063/1.107812

X. Chu, M.S. Wong, W.D. Sproul, A.S. Barnett, Mechanical properties and microstructures of polycrystalline metal/ceramic superlattices, TiN/Ni and TiN/Ni0.9Cr0.1, paper presented at ICMCTF-20, San Diego, CA, 1993.

Madan, 1996, Appl. Phys. Lett., 68, 2198, 10.1063/1.116011

Madan, 1998, J. Appl. Phys., 84, 776, 10.1063/1.368137

Schneider, 1997, J. Vac. Sci. Technol. A, 15, 1084, 10.1116/1.580434

Schneider, 1998, Reactive pulsed dc magnetron sputtering and control

Vepřek, 1995, Thin Solid Films, 268, 64, 10.1016/0040-6090(95)06695-0

Siegel, 1996, Nanophase materials: Structure, defects and properties, 1

Butyagin, 1997, Colloid J., 59, 112

Musil, 1998, Czech. J. Phys., 48, 1209, 10.1023/A:1022814319240

Musil, 1999, Magnetron sputtering of alloy and alloy-based films, Thin Solid Films, 343–344, 47, 10.1016/S0040-6090(98)01567-3

Leedy, 1996, J. Vac. Sci. Technol. A, 14, 2202, 10.1116/1.580047

Musil, 1998, Vacuum, 50, 363, 10.1016/S0042-207X(98)00068-2

Musil, 1996, J. Vac. Sci. Technol. A, 14, 2247, 10.1116/1.580055

Musil, 1998, J. Vac. Sci. Technol. A, 16, 3301, 10.1116/1.581537

Musil, 1999, Hard nanocomposite Zr–Y–N coatings. Correlation between hardness and structure

Musil, 1999, Czech. J. Phys., 49, 359, 10.1023/A:1022853101763

Musil, 1999, Surf. Coat. Technol., 115, 32, 10.1016/S0257-8972(99)00065-1

J. Musil, Z. Soukup, unpublished results.

Musil, 1999, Superhard nanocomposite Ti1−xAlxN films prepared by magnetron sputtering, 1605

Musil, 1999, Vacuum, 52, 269, 10.1016/S0042-207X(98)00297-8

Johnson, 1986, Progr. Mater. Sci., 30, 81, 10.1016/0079-6425(86)90005-8

Weigang, 1995, Z. Phys. B, 96, 349, 10.1007/BF01313057

Ding, 1992, Appl. Phys. Lett., 60, 994, 10.1063/1.108471

Mišina, 1998, Surf. Coat. Technol., 110, 168, 10.1016/S0257-8972(98)00688-4

Liu, 1997, J. Vac. Sci. Technol. B, 15, 1990, 10.1116/1.589590

May, 1995, J. Vac. Sci. Technol. B, 13, 361, 10.1116/1.587946

Voevodin, 1997, J. Appl. Phys. Lett., 82, 855

Vepřek, 1998, Surf. Coat. Technol., 108/109, 138, 10.1016/S0257-8972(98)00618-5

Benda, 1999, Vacuum, 55, 171, 10.1016/S0042-207X(99)00145-1

Min, 1999, Thin Solid Films, 339, 238

Louro, 1998, Hardness versus structure in W–Si–N sputtered coatings

Diserens, 1998, Surf. Coat. Technol., 108/109, 241, 10.1016/S0257-8972(98)00560-X

Mitterer, 1998, Vacuum, 50, 313, 10.1016/S0042-207X(98)00059-1

Mitterer, 1999

Voevodin, 1999, Surf. Coat. Technol.

Wahlström, 1993, Thin Solid Films, 235, 62, 10.1016/0040-6090(93)90244-J

Field, 1979

Gorbatkin, 1994, Appl. Phys. Lett., 65, 2672, 10.1063/1.112598

Oliver, 1991, J. Mater. Res., 7, 1564, 10.1557/JMR.1992.1564

Vepřek, 1998, Thin Solid Films, 317, 449, 10.1016/S0040-6090(97)00665-2

Vepřek, 1997, Thin Solid Films, 297, 145, 10.1016/S0040-6090(96)09480-1

Musil, 1999, Structure and microhardness of magnetron sputtered nanocrystalline CrNi–N films, 1617

Voevodin, 1998, J. Mater. Sci., 33, 319, 10.1023/A:1004307426887

Tsui, 1995, Mater. Res. Soc. Symp. Proc., 383, 447, 10.1557/PROC-383-447

Cavaleiro, 1998, Deposition and characterization of fine-grained W–Ni–C/N ternary films, 265