Fracture studies on bi-metallic pipe weld joints under monotonic and cyclic loading

S. Vishnuvardhan1, M. Saravanan1, P. Gandhi1, G. Raghava2,3, Suranjit Kumar4, I.A. Khan4, P.K. Singh4
1CSIR - Structural Engineering Research Centre, Taramani, Chennai - 600113, India
2Former Chief Scientist, CSIR - Structural Engineering Research Centre, Taramani, Chennai - 600113, India
3Professor in Civil Engineering, Nitte Meenakshi Institute of Technology, Yelahanka, Bengaluru - 560064, India
4Reactor Safety Division, Bhabha Atomic Research Centre, Mumbai - 400085, India

Tóm tắt

Từ khóa


Tài liệu tham khảo

Brocks, 2002, Fracture mechanics assessment of a bi-metallic welded joint

Faidy, 2001, BIMET: Structural integrity of bi-metallic components, Nucl. Eng. Des., 209, 79, 10.1016/S0029-5493(01)00390-9

Guozhen Wang, Haitao Wang, Fuzhen Xuan and Shantung Tu, Local fracture behavior and integrity assessment of a dissimilar metal welded joint in nuclear power systems, Proceedings of 13th International Conference on Fracture, Beijing, China, June 16-21, 2013.

Schwalbe, 2004, Fracture mechanics analysis of the BIMET welded pipe tests, Int. J. Pres. Ves. Pip., 81, 251, 10.1016/j.ijpvp.2003.12.016

Jiang, 2003, Evaluation of interfacial crack growth in bimaterial metallic joints loaded by symmetric three-point bending, Int. J. Pres. Ves. Pip., 80, 129, 10.1016/S0308-0161(03)00004-8

Khan, 2004, An estimation procedure to evaluate limit loads of bi-metallic specimens. PART-1, Int. J. Pres. Ves. Pip., 81, 451, 10.1016/j.ijpvp.2004.03.003

Devaux, 2000, Evaluation of the integrity of PWR bimetallic welds, J. Pressure Vessel Technol., 122, 368, 10.1115/1.556194

Kumar, 2017, Experimental investigation of local tensile and fracture resistance behaviour of dissimilar metal welded joint: SA508 Gr.3 Cl.1 and SA312 Type 304LN, Fatig. Fract. Eng. Mater. Struct., 40, 190, 10.1111/ffe.12484

2014

2014

2010

Suranjit Kumar, Singh, P. K., Khan, I. A., Bhasin, V., Singh, R. K., Vaze, K. K., Karn, K. N., Joyson Derose, Srivastava, S.P. and Sinha, A.K., reportEvaluation of Tensile and Fracture Properties of Dissimilar Metal Pipe Weld: Low Alloy Ferritic Steel and Austenitic Stainless Steel, Technical Report, BARC/2014/E/2014, Bhabha Atomic Research Centre, Mumbai.

2014

Zahoor, 1990, vol. 2

Raghava, 2016, Monotonic fracture studies on bi-metallic pipe weld joints having circumferential through-wall crack, 419

Saravanan, M., Vishnuvardhan, S., Raghava, G. and Gandhi, P., reportMonotonic and Cyclic Fracture Studies on Bi-metallic Pipe Weld Joints, Sponsored Research Report No. R&D 03-SSP 14541-SR-3, CSIR - Structural Engineering Research Centre, Chennai, India, September 2015.

Maurício Barreto de Azevedo, 2018, Microstructural and mechanical characterization of the transition zone of 9%Ni steel cladded with Ni-based superalloy 625 by GTAW-HW, Metals, 8

Vishnuvardhan, S., Raghava, G., Saravanan, M., Gandhi, P., Suranjit Kumar, Singh, P. K., Gupta, S. K. and Bhasin, V., Fracture studies on circumferentially cracked bi-metallic pipe weld joints under quasi-static cyclic loading, Proceedings of the 10th Structural Engineering Convention (SEC-2016), Chennai, India, December 2016.

Wang, 2013, An experimental investigation of local fracture toughness and crack growth paths in a dissimilar metal welded joint, Mater. Des., 44, 179, 10.1016/j.matdes.2012.07.067