Evolution of the microstructure and tribological performance of Ti–6Al–4V cladding with TiN powder
Tài liệu tham khảo
Bell T. Proceedings of the first Asian international conference on tribology. Beijing: Tsinghua University Press; 1998. p. 421.
Muthukumaran, 2011, Experimental investigation on corrosion and hardness of ion implanted AISI 316L stainless steel, Mater Des, 31, 2813, 10.1016/j.matdes.2010.01.007
Borgioli, 2005, Improvement of wear resistance of Ti–6Al–4V alloy by means of thermal oxidation, Mater Lett, 59, 2159, 10.1016/j.matlet.2005.02.054
Tian, 2006, Microstructures and wear properties of composite coatings produced by laser alloying of Ti–6Al–4V with graphite and silicon mixed powders, Mater Lett, 60, 109, 10.1016/j.matlet.2005.07.082
Shamanian, 2010, Effects of surface alloying on microstructure and wear behavior of ductile iron, Mater Des, 31, 2760, 10.1016/j.matdes.2010.01.017
Arabi Jeshvaghani, 2011, Enhancement of wear resistance of ductile iron surface alloyed by stellite 6, Mater Des, 32, 2028, 10.1016/j.matdes.2010.11.060
Lin, 2003, The wear behaviour of machine tool guideways clad with W–Ni, W–Co and W–Cu using gas tungsten arc welding, Surf Coat Technol, 172, 158, 10.1016/S0257-8972(03)00389-X
Lin Yuan, 2005, Analysis of microstructure and wear performance of WC–Ti clad layers on steel, produced by gas tungsten arc welding, Surf Coat Technol, 200, 2106, 10.1016/j.surfcoat.2005.05.010
Cai, 2007, Microstructure and formation mechanism of titanium matrix composites coating on Ti–6Al–4V by laser cladding, Rare Metals, 26, 342, 10.1016/S1001-0521(07)60226-5
Khan, 1997, The surface modification of a Ti–6Al–4V alloy using a metal arc heat source, 469
Nunogaki, 2001, Transformation of titanium surface to TiC- or TiN-ceramics by reactive plasma processing, Mater Des, 22, 601, 10.1016/S0261-3069(01)00022-X
Hu Rui, 2010, Hardness and wear resistance improvement of surface composite layer on Ti–6Al–4V substrate fabricated by powder sintering, Mater Des, 31, 2670, 10.1016/j.matdes.2009.11.057
Duverneix T, Puig T, Bataille F. ICALEO’90: Laser Materials Processing. In: Ream SL, Dausinger F, Fujioka T, editors. SPIE; 1991. p. 525.
Jiang, 2000, Wear resistance of a laser surface alloyed Ti–6Al–4V alloy, Surf Coat Technol, 130, 24, 10.1016/S0257-8972(00)00680-0
Lin, 2008, Elucidating the microstructure and wear behavior for multicomponent alloy clad layers by in situ synthesis, Surf Coat Technol, 202, 4666, 10.1016/j.surfcoat.2008.03.033
Tina, 2005, Crack-free wear resistance coatings produced on pure titanium and Ti–6Al–4V by laser nitriding, Surf Rev Lett, 12, 741, 10.1142/S0218625X05007657
ASM. Metals Handbook, vol. 3. 8th ed. Alloy Phase Diagrams. ASM International; 1992.
Wu, 1999, In situ formation by laser cladding of a TiC composite coating with a gradient distribution, Surf Coat Technol, 115, 111, 10.1016/S0257-8972(99)00045-6
Kim, 2000, On the rule of mixtures for the hardness of particle reinforced composites, Mater Sci Eng A, 289, 30, 10.1016/S0921-5093(00)00909-6
Straffelini, 1999, Dry sliding wear of Ti–6Al–4V alloy as influenced by the counterface and sliding conditions, Wear, 236, 328, 10.1016/S0043-1648(99)00292-6