Evaluating performance, degradation, and release behavior of a nanoform pigmented coating after natural and accelerated weathering
Tài liệu tham khảo
Al-Kattan, 2013, Release of TiO2 from paints containing pigment-TiO2 or nano-TiO2 by weathering, Environ. Sci.: Processes Impacts, 15, 2186
Al-Kattan, 2015, Characterization of materials released into water from paint containing nano-SiO2, Chemosphere, 119, 1314, 10.1016/j.chemosphere.2014.02.005
Althues, 2007, Functional inorganic nanofillers for transparent polymers, Chem. Soc. Rev., 36, 1454, 10.1039/b608177k
2018
Arvidsson, 2013, Review of potential environmental and health risks of the nanomaterial graphene, Hum. Ecol. Risk Assess. Int. J., 19, 873, 10.1080/10807039.2012.702039
Auffan, 2014, Long-term aging of a CeO2 based nanocomposite used for wood protection, Environ. Pollut., 188, 1, 10.1016/j.envpol.2014.01.016
Babick, 2016, How reliably can a material be classified as a nanomaterial? Available particle-sizing techniques at work, J. Nanopart. Res., 18, 1, 10.1007/s11051-016-3461-7
Bernard, 2011, Fate of grapheme in polymer nanocomposite exposed to UV radiation, J. Phys. Conf. Ser., 304, 10.1088/1742-6596/304/1/012063
Bigelow, 1998, The USDA ultraviolet radiation monitoring program, Bull. Am. Meteorol. Soc., 79, 601, 10.1175/1520-0477(1998)079<0601:TUURMP>2.0.CO;2
Crewdson, 2016
Diepens, 2011, Outdoor and accelerated weathering studies of bisphenol A polycarbonate, Polym. Degrad. Stab., 96, 649, 10.1016/j.polymdegradstab.2010.12.009
ECHA, 2017
Fiorentino, 2015, Influence of paints formulations on nanoparticles release during their life cycle, J. Nanopart. Res., 17, 149, 10.1007/s11051-015-2962-0
Goodwin, 2018, Detection and quantification of graphene-family nanomaterials in the environment, Environ. Sci. Technol., 52, 4491, 10.1021/acs.est.7b04938
Han, 2018, Environmental aging and degradation of multiwalled carbon nanotube reinforced polypropylene, Carbon, 129, 137, 10.1016/j.carbon.2017.10.038
Harper, 2015, Measuring nanomaterial release from carbon nanotube composites: review of the state of the science, J. Phys. Conf. Ser., 617
Hirth, 2013, Scenarios and methods that induce protruding or released CNTs after degradation of composite materials, J. Nanopart. Res., 15, 1504, 10.1007/s11051-013-1504-x
Hsu, 2007, Evaluation of nanoparticles emission for TiO2 nanopowder coating materials, J. Nanopart. Res., 9, 157, 10.1007/s11051-006-9185-3
Hsueh, 2017, Kinetics of photodegradation and nanoparticle surface accumulation of a nanosilica/epoxy coating exposed to UV light, J. Coat. Technol. Res., 1
Jacobs, 2016, Surface degradation and nanoparticle release of a commercial nanosilica/polyurethane coating under UV exposure, J. Coat. Technol. Res., 13, 735, 10.1007/s11998-016-9796-2
Kaegi, 2008, Synthetic TiO2 nanoparticle emission from exterior facades into the aquatic environment, Environ. Pollut., 156, 233, 10.1016/j.envpol.2008.08.004
Kaegi, 2010, Release of silver nanoparticles from outdoor facades, Environ. Pollut., 158, 2900, 10.1016/j.envpol.2010.06.009
Klingshirn, 2010, Zinc Oxide: From fundamental properties towards novel applications, Springer Ser. Mater. Sci., 120, 325, 10.1007/978-3-642-10577-7_13
Koivisto, 2017, Quantitative material releases from products and articles containing manufactured nanomaterials: towards a release library, NanoImpact, 5, 119, 10.1016/j.impact.2017.02.001
Lankone, 2017, Photodegradation of polymer-CNT nanocomposites: effect of CNT loading and CNT release characteristics, Environ. Sci.: Nano, 4, 967
Lankone, 2017, Methodology for quantifying engineered nanomaterial release from diverse product matrices under outdoor weathering conditions and implications for life cycle assessment, Environ. Sci.: Nano, 4, 1784
Lederer, K.; Kastner, E.; Grestenberger, G., Composition with improved long term scratch resistance and reduced surface tack. US Patent Application Publication 2014, US 2014/0303301 A1.
Lv, 2015, Outdoor and accelerated laboratory weathering of polypropylene: a comparison and correlation study, Polym. Degrad. Stab., 112, 145, 10.1016/j.polymdegradstab.2014.12.023
McNally, 2011
Miklečić, 2015, Influence of TiO2 and ZnO nanoparticles on properties of waterborne polyacrylate coating exposed to outdoor conditions, Prog. Org. Coat., 89, 67, 10.1016/j.porgcoat.2015.07.016
Ministère de l’Environnement, de l’Énergie et de la Mer, 2015
Mitrano, 2015, Review of nanomaterial aging and transformations through the life cycle of nano-enhanced products, Environ. Int., 77, 132, 10.1016/j.envint.2015.01.013
Mohanty, 2015
Neubauer, 2017, Nanoscale coloristic pigments: upper limits on releases from pigmented plastic during environmental aging, in food contact, and by leaching, Environ. Sci. Technol., 51, 11669, 10.1021/acs.est.7b02578
Nguyen, 2017, Impact of UV irradiation on multiwall carbon nanotubes in nanocomposites: formation of entangled surface layer and mechanisms of release resistance, Carbon, 116, 191, 10.1016/j.carbon.2017.01.097
Nichols, 2013, An improved accelerated weathering protocol to anticipate Florida exposure behavior of coatings, J. Coat. Technol. Res., 10, 153, 10.1007/s11998-012-9467-x
Pacurari, 2016, A review on the respiratory system toxicity of carbon nanoparticles, Int. J. Environ. Res. Public Health, 13, 325, 10.3390/ijerph13030325
Pickett, 2005, Global weathering of aromatic engineering thermoplastics, Polym. Degrad. Stab., 90, 405, 10.1016/j.polymdegradstab.2005.04.011
Platten, 2016, Estimating dermal transfer of copper particles from the surfaces of pressure-treated lumber and implications for exposure, Sci. Total Environ., 548–549, 441, 10.1016/j.scitotenv.2015.12.108
Rabek, 1995
Rabek, 1996
Riedl, 2006, Überblick über die Methoden der Bewitterungs- und Lichtechtheitsprüfung in der Automobilindustrie, Galvanotechnik, 97, 420
Ruggiero, 2019
Santos, 2013, Outdoor and accelerated weathering of acrylonitrile-butadiene-styrene: a correlation study, Polym. Degrad. Stab., 98, 2111, 10.1016/j.polymdegradstab.2013.07.016
Scifo, 2017
SRI_consulting, 2011
Sung, 2015, A quantitative study of nanoparticle release from nanocoatings exposed to UV radiation, J. Coat. Technol. Res., 12, 121, 10.1007/s11998-014-9620-9
2003
Upadhyay, 2011, Chemical speciation of PM2.5 and PM10 in South Phoenix, AZ, J. Air Waste Manage. Assoc., 61, 302, 10.3155/1047-3289.61.3.302
Wigger, 2018, Redefining environmental nanomaterial flows: consequences of the regulatory nanomaterial definition on the results of environmental exposure models, Environ. Sci.: Nano, 5, 1372
Wohlleben, 2017, NanoRelease: pilot interlaboratory comparison of a weathering protocol applied to resilient and labile polymers with and without embedded carbon nanotubes, Carbon, 113, 346, 10.1016/j.carbon.2016.11.011
Wohlleben, 2019, The nanoGRAVUR framework to group (nano) materials for their occupational, consumer, environmental risks based on a harmonized set of material properties, applied to 34 case studies, Nanoscale, 11, 17637, 10.1039/C9NR03306H
Zaidi, 2010, Effect of natural weather on the structure and properties of polylactide/Cloisite 30B nanocomposites, Polym. Degrad. Stab., 95, 1751, 10.1016/j.polymdegradstab.2010.05.014
Zepp, 2019