Enhanced piezoelectric properties and lowered sintering temperature of Ba(Zr0.07Ti0.93)O3 by B2O3 addition

Current Applied Physics - Tập 10 Số 2 - Trang 557-560 - 2010
Parkpoom Jarupoom1, Kamonpan Pengpat1, Gobwute Rujijanagul1
1Department of Physics and Materials Science, Faculty of Science, Chiang Mai University, Chiang Mai 50200, Thailand

Tóm tắt

Từ khóa


Tài liệu tham khảo

Yu, 2002, Appl. Phys. Lett., 81, 1285, 10.1063/1.1498496

Ciomaga, 2006, Phase. Transit., 79, 389, 10.1080/01411590600892120

Yu, 2000, J. Appl. Phys., 88, 410, 10.1063/1.373674

Bhaskar Reddy, 2007, Appl. Phys. A, 89, 1011, 10.1007/s00339-007-4208-1

Kantha, 2009, Curr. Appl. Phys., 9, 460, 10.1016/j.cap.2008.04.004

Valant, 2004, J. Am. Ceram. Soc., 87, 1222, 10.1111/j.1151-2916.2004.tb07716.x

Prakash, 2000, J. Solid State Chem., 155, 86, 10.1006/jssc.2000.8895

Rhim, 2000, J. Am. Ceram. Soc., 83, 1145, 10.1111/j.1151-2916.2000.tb01345.x

Rhim, 2000, J. Am. Ceram. Soc., 83, 3009, 10.1111/j.1151-2916.2000.tb01675.x

Qi, 2004, J. Appl. Phys., 96, 6937, 10.1063/1.1814167

Qi, 2002, Mater. Sci. Eng. B, 95, 283, 10.1016/S0921-5107(02)00287-8

Wang, 2005, Appl. Phys. A, 80, 333, 10.1007/s00339-003-2210-9

Singh, 2007, Appl. Phys. Lett., 91, 112913, 10.1063/1.2784968

Wang, 2009, J. Eur. Ceram. Soc., 29, 1183, 10.1016/j.jeurceramsoc.2008.08.016

Haertling, 1966, Am. Ceram. Soc. Bull., 45, 1084

Moulson, 2003

Shrout, 2007, J. Electroceram., 19, 111, 10.1007/s10832-007-9095-5

Xu, 2005, Mater. Lett., 59, 2437, 10.1016/j.matlet.2005.03.020