Electron Microscopy and Spectroscopy in the Analysis of Friction and Wear Mechanisms
Tóm tắt
Từ khóa
Tài liệu tham khảo
1986, Titanium aluminium nitride films—A new alternative to TiN coatings, J. Vac. Sci. Technol., 4, 2717, 10.1116/1.573713
Paldeys, 2003, Single layer and multilayer wear resistant coatings of (Ti,Al)N: A review, Mater. Sci. Eng., A342, 58, 10.1016/S0921-5093(02)00259-9
Helmersson, 1987, Growth of single-crystal TiN/VN strained-layer superlattices with extremely high mechanical hardness, J. Appl. Phys., 62, 481, 10.1063/1.339770
Donohue, 2000, Properties of various large-scale fabricated TiAlN- and CrN-based superlattice coatings grown by combined cathodic arc-unbalanced magnetron sputter deposition, Surf. Coat. Technol., 125, 269, 10.1016/S0257-8972(99)00572-1
Veprek, 1995, Superhard nanocrystalline composite materials: The TiN/Si3N4 system, Appl. Phys. Lett., 66, 2640, 10.1063/1.113110
Lu, 2006, Recent advances on understanding the origin of superhardness in nanocomposite coatings: A critical review, J. Mater. Sci., 41, 937, 10.1007/s10853-006-6577-9
De Hosson, J.T.M., and Cavaleiro, A. (2006). Physical and mechanical properties of hard nanocomposite films prepared by reactive magnetron sputtering. Nanostructured Hard Coatings, Springer Science.
Justo, 2009, Self-lubricating Ti–C–N nanocomposite coatings prepared by double magnetron sputtering, Solid State Sci., 11, 660, 10.1016/j.solidstatesciences.2008.10.017
Lu, 2007, Nanostructure transition: From solid solution Ti(N,C) to nanocomposite nc-Ti(N,C)/a-(C,CNx), Appl. Phys. Lett., 90, 221913, 10.1063/1.2745261
Erdemir, 2006, Tribology of diamond-like carbon films: Recent progress and future prospects, J. Phys. D Appl. Phys., 39, R311, 10.1088/0022-3727/39/18/R01
Erdemir, 2003, Friction-induced structural transformations of diamondlike carbon coatings under various atmospheres, Surf. Coat. Technol., 163–164, 444
Merkle, 2010, In situ TEM studies of tribo-induced bonding modifications in near-frictionless carbon films, Carbon, 48, 587, 10.1016/j.carbon.2009.08.036
Lindquist, 2009, Tribofilm formation and tribological properties of TiC and nanocomposite TiAlC coatings, Wear, 266, 379, 10.1016/j.wear.2008.04.046
Luo, 2006, TEM-EELS study of low-friction superlattice TiAlN/VN coating: The wear mechaisms, Tribol. Lett., 24, 171, 10.1007/s11249-006-9160-2
Luo, 1995, Effects of microstructure on the abrasive wear behaviour of spheroidal cast iron, Wear, 184, 1, 10.1016/0043-1648(94)06499-7
Luo, 1993, Investigation of the wear failure mechanism of a flour milling roller, Wear, 161, 11, 10.1016/0043-1648(93)90447-T
Luo, 1999, TEM observation of wear mechanisms of TiAlCrN and TiAlN/CrN coatings grown by combined steered-arc/unbalanced magnetron deposition, Wear, 225–229, 74, 10.1016/S0043-1648(99)00049-6
Luo, 2001, TEM study of the wear of TiAlN/CrN superlattice coatings, Scrip. Mater., 45, 399, 10.1016/S1359-6462(01)01018-1
Luo, 2001, Wear mechanisms of monolithic and multicomponent nitride coatings grown by combined arc etching and unbalanced magnetron sputtering, Surf. Coat. Technol., 146–147, 430, 10.1016/S0257-8972(01)01397-4
Inman, 2003, Microscopy of glazed layers formed during high temperature sliding wear, Wear, 254, 461, 10.1016/S0043-1648(03)00134-0
Zhou, 2006, Investigating Worn Surface of NanoscaleTiAlN/VN Coating Using FIB and TEM, EMAG-Nano Imaging Anal. Fabr. Nanoscale J. Phys. Ser., 26, 95
Luo, 2006, Transmission electron microscopy and energy dispersive X-ray spectroscopy on the worn surface of nano-structured TiAlN/VN multilayer coating, Thin Solid Films, 497, 203, 10.1016/j.tsf.2005.10.086
Luo, 2009, Effect of tribofilm formation on the dry sliding friction and wear properties of magnetron sputtered TiAlCrYN coatings, Tribol. Lett., 34, 113, 10.1007/s11249-009-9415-9
Luo, 2007, Structure and wear mechanisms of nano-structured TiAlCN/VCN multilayer coatings, Plasma Processes Polym., 4, S916, 10.1002/ppap.200732205
Wang, Q.J., and Chung, Y.-W. (2013). Tribofilms in solid lubricants. Encyclopedia of Tribology, Springer Science.
Luo, 2010, Origin of friction in running-in sliding wear of nitride coatings, Tribol. Lett., 37, 529, 10.1007/s11249-009-9548-x
Zhou, 2010, Wear and friction of TiAlN/VN coatings against Al2O3 in air at room and elevated temperatures, Acta Mater., 58, 2912, 10.1016/j.actamat.2010.01.020
Luo, 2011, Structure characterization and tribological study of magnetron sputtered nanocompositenc-TiAlV(N,C)/a-C coatings, J. Mater. Chem., 21, 9746, 10.1039/c1jm10707k
Luo, 2011, Temperature dependent friction and wear of magnetron sputtered coating TiAlN/VN, Wear, 271, 2058, 10.1016/j.wear.2011.01.054
Abbasi, 2018, Cast study: Wear mechanisms of NiCrVMo-steel and CrB-steel scrap shear blades, Wear, 398–399, 29, 10.1016/j.wear.2017.11.014
Ibrahim, 2017, Biomedical materials and techniques to improve the tribological, mechanical and biomedical properties of orthopaedic implants—A review article, J. Alloy. Compd., 714, 636, 10.1016/j.jallcom.2017.04.231
Sierevelt, 2015, Titanium nitride coating of orthopaedic implants: A review of the literature, BioMed. Res. Int., 2015, 1
Lapaj, 2016, Retrieval analysis of titanium nitrtide (TiN) coated prosthetic demoral heads articulating with polyethylene, J. Mech. Behav. Biomed. Mater., 55, 127, 10.1016/j.jmbbm.2015.10.012
Affatato, 2016, Does metal transfer affect the tribological behaviour of demoral heads? Roughness and phase transformation analyses on retrieved zirconia and Biolox Delta composites, Compos. Part B, 92, 290, 10.1016/j.compositesb.2016.02.020
Namus, 2017, Correlation of the wear transition in CoCrMo alloys with the formation of a nanocrystalline surface layer and a proteinaceous surface film, Wear, 376–377, 223, 10.1016/j.wear.2016.11.046
Zeng, 2015, Subsurface characterisation of wear on mechanically polished and electro-polished bilmedical grade CoCrMo, Wear, 332–333, 650, 10.1016/j.wear.2015.02.007
Slonaker, 2004, Review of wear mechnaisms in hip implants: Paper II—Ceramics IG004712, Mater. Des., 25, 395, 10.1016/j.matdes.2003.11.011
Zeng, 2012, Transmission electron microscopy analysis of worn alumina hip replacement prostheses, Acta Mater., 60, 2061, 10.1016/j.actamat.2012.01.009
Zeng, 2017, Characterisation of the wear mechanisms in retrieved aluminium-on-alumina total hip replacements, Wear, 376–377, 212, 10.1016/j.wear.2016.11.045
Luo, 2004, Transmission electron microscopy and X-ray diffrac-tion investigation of the microstructure of nano-scale multilayers TiAlN/VN grown by unbalanced magne-tron deposition, J. Mater. Res., 19, 1093, 10.1557/JMR.2004.0143
Lewis, 2004, The effect of (Ti + Al): V ratio on the structure and oxidation behavior of TiAlN/VN nano-scale multilayer coatings, Surf. Coat. Technol., 177–178, 252, 10.1016/j.surfcoat.2003.09.041
Hovsepian, 2005, TiAlN based nanoscale multilayer PVD coatings designed to adapt their tribological properties at elevated temperatures, Thin Solid Films, 485, 160, 10.1016/j.tsf.2005.03.048
Luo, 2005, Performance of nano-structured multilayer PVD coating TiAlN/VN in dry high speed milling of aerospace aluminium 7010-T7651, Surf. Coat. Technol., 200, 123, 10.1016/j.surfcoat.2005.02.017
Luo, 2005, Tribological perperties of unbalanced magnetron sputtered nanoscale multilayer coatings TiAlN/VN and TiAlCrYN deposited on plasma nitrided steels, Surf. Coat. Technol., 193, 39, 10.1016/j.surfcoat.2004.07.058
Dave, 2004, New Tool Coatings for Light Metal Cutting, Trans. Mater. Heat Treat., 25, 832
Lewis, 2004, Interrelationship between atomic species, bias voltage, texture and microstructure of nano-scale multilayers, Surf. Coat. Technol., 184, 225, 10.1016/j.surfcoat.2003.11.005
Leyens, 2002, Novel Coating Systems Produced by the Combined Cathodic Arc/Unbalanced Magnetron Sputtering for Environmental Protection of Titanium Alloys and Titanium Aluminides, Surf. Coat. Technol., 155, 103, 10.1016/S0257-8972(02)00063-4
Luo, 2017, Tribological properties and wear mechanisms of DC pulse plasma nitrided austenitic stainless steel in dry reciprocating sliding tests, Wear, 376–377, 1640, 10.1016/j.wear.2016.12.022
Sigle, 2005, Analytical transmission electron microscopy, Ann. Rev. Mater. Res., 35, 239, 10.1146/annurev.matsci.35.102303.091623
Ponsonnet, 1998, EELS analysis of hydrogenated diamond-like carbon films, Thins Solid Films, 319, 97, 10.1016/S0040-6090(97)01094-8
Mitternauer, 2004, Electron energy loss near edge structure as a fingerprint for identifying chromium nitrides, Solid State Commun., 130, 209, 10.1016/j.ssc.2004.01.045
Kothleitner, 2005, A combined SNMS and EFTEM/EELS study on focused ion beam prepared vanadium nitride thin films, Appl. Surf. Sci., 252, 66, 10.1016/j.apsusc.2005.02.013
Kohl, 2000, Methods for ELNES-quantification: Characterization of the degree of inversion of Mg-Al-spinels, Micron, 31, 347, 10.1016/S0968-4328(99)00113-4
Hofer, 2001, Electron energy loss near edge structure on the nitrogen K-edge in vanadium nitrides, J. Microsc., 204, 166, 10.1046/j.1365-2818.2001.00946.x
Bouchet, 2003, Experimental study of ELNES at grain boundaries in alumina: Intergranular radiation damage effects on A1-L23 and O-K edges, Ultramicroscopy, 96, 139, 10.1016/S0304-3991(02)00437-0
Lu, 2012, ELNES for boron, carbon, and nitrogen K-edges with different chemical environments in layered materials studied by density functional theory, Ultramicroscopy, 112, 61, 10.1016/j.ultramic.2011.10.011
Fang, 1987, Abrasive wear resistance of Cr-family white cast irons, Acta Metall. Sin., 23, 575
Xing, 1992, Influence of carbon content on the oxidation and wear resistance of 20% Cr alloy at elevated temperature, J. Mech. Eng., 28, 32
Qiu, 2006, Correlation between the characteristics of the thermo-mechanical mized layer and wear behaviour of Ti–6Al–4V alloy, Tribol. Lett., 22, 227, 10.1007/s11249-006-9088-6
Abrahams, 1974, Cross-sectional specimens for transmission electron microscopy, J. Appl. Phys., 45, 3315, 10.1063/1.1663778
Helmersson, 1986, Cross-sectional preparation for TEM of film-substrate combinations with a large difference in sputtering yields, J. Electron Microsc. Tech., 4, 361, 10.1002/jemt.1060040406
Giannuzzi, 1999, A review of focused ion beam milling techniques for TEM specimen preparation, Micron, 30, 197, 10.1016/S0968-4328(99)00005-0
Reyntjens, 2001, A review of focused ion beam applications in microsystem technology, J. Micromech. Microeng., 11, 287, 10.1088/0960-1317/11/4/301
Dieterle, 2011, Optimized Ar ion milling procedure for TEM cross-sectional sample preparation, Ultramicroscopy, 111, 1636, 10.1016/j.ultramic.2011.08.014
Suess, 2011, Minimization of amorphous layer in Ar+ ion milling for UHR-EM, Ultramicroscopy, 111, 1224, 10.1016/j.ultramic.2011.03.004