Effect of deteriorated microstructures on stress corrosion cracking of X70 pipeline steel in acidic soil environment

Zhiyong Liu1, Guoli Zhai1, Xiaogang Li1, Cuiwei Du1
1Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083, China