Delta phase precipitation in Inconel 718
Tóm tắt
Từ khóa
Tài liệu tham khảo
Brown, 1987, Nickel–iron alloys, 165
Chang, 1989, Rene 220: 100 °F improvement over alloy 718, 631
Azadian, 2001, Precipitation in spray-formed IN 718, 617
Oblak, 1969, Coherency strengthening in Ni base alloys hardened by DO22 γʺ precipitates, Metall. Mater. Trans., 62, 611
Brooks, 1988, Metallurgical stability of Inconel alloy 718, 33
Oradei-Basile, 1991, A current T–T–T diagram for wrought alloy 718, 325
Slama, 1997, Aging of the Inconel 718 alloy between 500 and 750 °C, J. Mater. Res., 12, 2298, 10.1557/JMR.1997.0306
Lu O. HAZ Microstructural evolution in alloy 718 after multiple repair and PWHT cycles, PhD thesis, Ohio State University, Ohio, United States; 1999.
Desvallées, 1994, Delta phase in Inconel 718: mechanical properties and forging process requirements, 281
Muller, 1975, 211
Sjöberg, 1991, Grain boundary δ-phase morphology, carbides and notch rupture sensitivities of cast alloy 718, 603
Azadian S, Wei LY, Warren R. Ageing response of spray formed Inconel 718 between 600° and 1000 °C. Submitted to Mater. Sci. Technol.
Underwood, 1970
Sundararaman, 1988, Some aspects of the precipitation of metastable intermetallic phases in Inconel 718, Metall. Mater. Trans., A, 19, 453, 10.1007/BF02649259
He, 1994, γʺ precipitate in Inconel 718, Mater. Sci. Technol., 10, 293
Liu, 1999, Effect of cold rolling on the precipitation behaviour of δ-phase in Inconel 718, Metall. Mater. Trans., A, 30, 31, 10.1007/s11661-999-0193-7
Collier, 1988, The effect of varying Al, Ti, and Nb content on the phase stability of Inconel 718, Metall. Mater. Trans., A, 19, 1566, 10.1007/BF02645133
Burke, 1991, Precipitation in Inconel 718: a combined AEM and APFIM investigation, 337
Li, 2002, Isolation and determination for δ, γ′ and γʺ phases in Inconel 718 alloy, Scr. Mater., 46, 635, 10.1016/S1359-6462(02)00041-6
Stockinger, 2001, Modelling of δ-phase dissolution during preheating of Inconel 718 turbine disks, 141