Degradation of HDPE, LLDPE, and blended polyethylene geomembranes in extremely low and high pH mining solutions at 85 °C

Geotextiles and Geomembranes - Tập 51 - Trang 27-38 - 2023
F.B. Abdelaal1, R. Kerry Rowe2, M.S. Morsy3, R.A. e Silva4
1GeoEngineering Centre at Queen's-RMC, Queen's University, Ellis Hall, Kingston, ON, K7L 3N6, Canada
2Barrington Batchelor Distinguished University Professor and Canada Research Chair in Geotechnical and Geoenvironmental Engineering, GeoEngineering Centre at Queen's-RMC, Queen's University, Ellis Hall, Kingston, ON, K7L 3N6, Canada
3Soil Mechanics and Foundation Engineering Unit, Structural Engineering Department, Faculty of Engineering, Ain Shams University, Cairo, 11535, Egypt
4GeoEngineering Centre at Queen's-RMC, Queen's University, Kingston, ON, K7L 3N6, Canada

Tài liệu tham khảo

Abdelaal, 2014, Antioxidant depletion from a LLDPE geomembrane in an extremely high pH solution Abdelaal, 2014, Effect of high temperatures on antioxidant depletion from different HDPE geomembranes, Geotext. Geomembranes, 42, 284, 10.1016/j.geotexmem.2014.05.002 Abdelaal, 2017, Effect of high pH found in low-level radioactive waste leachates on the antioxidant depletion of a HDPE geomembrane, J. Hazard., Toxic, Radioact. Waste, 21, D4015001, 10.1061/(ASCE)HZ.2153-5515.0000262 Abdelaal, 2023, Degradation of physical and mechanical properties of a HDPE geomembrane with HALS in ten different low and high pH mining environments, Can. Geotech. J., 10.1139/cgj-2022-0419 Abdelaal, 2014, Effect of leachate composition on the long-term performance of a HDPE geomembrane, Geotext. Geomembranes, 42, 348, 10.1016/j.geotexmem.2014.06.001 Abdelaal, 2019, Long-term performance of a HDPE geomembrane stabilized with HALS in chlorinated water, Geotext. Geomembranes, 47, 815, 10.1016/j.geotexmem.2019.103497 ASTM D1238. Standard Test Method for Melt Flow Rates of Thermoplastics by Extrusion Plastometer. American Society for Testing and Materials, West Conshohocken, PA. ASTM D1505. Standard Test Method for Density of Plastics by the Density-Gradient Technique. American Society for Testing and Materials, West Conshohocken, PA. ASTM D3418. Standard Test Method for Melting and Crystallisation Temperatures by Thermal Analysis. American Society for Testing and Materials, West Conshohocken, PA. ASTM D3895. Standard Test Method for Oxidative Induction Time of Polyolefins by Differential Scanning Calorimetry. American Society for Testing and Materials, West Conshohocken, PA. ASTM D5199. Standard Method for Measuring the Nominal Thickness of Geosynthetics. American Society for Testing and Materials, West Conshohocken, PA. ASTM D5397. Standard Test Method for Evaluation of Stress Crack Resistance of Polyolefin Geomembranes Using Notched Constant Tensile Load Test. American Society for Testing and Materials D5397, West Conshohocken, PA. ASTM D5885. Standard Test Method for Oxidative Induction Time of Polyolefin Geosynthetics by High Pressure Differential Scanning Calorimetry. American Society for Testing and Materials D5885, West Conshohocken, PA. ASTM D6693. Standard Test Method for Determining Tensile Properties of Non-reinforced Polyethylene and Nonreinforced Flexible Polypropylene Geomembranes. American Society for Testing and Materials, West Conshohocken, PA. Barret, 2002, A molecular study towards the interaction of phenolic anti-oxidants, aromatic amines and HALS stabilizers in a thermo-oxidative ageing process, Polym. Degrad. Stab., 76, 441, 10.1016/S0141-3910(02)00047-2 Chen, 2014, Investigations of environmental stress cracking resistance of HDPE/EVA and LDPE/EVA blends, J. Appl. Polym. Sci., 131 Christie, 2013, A brief history of heap leaching, 265 Ewais, 2014, Effect of aging on the stress crack resistance of an HDPE geomembrane, Polym. Degrad. Stabil., 109, 194, 10.1016/j.polymdegradstab.2014.06.013 Ewais, 2014, Degradation behaviour of HDPE geomembranes with high and low initial high pressure oxidative induction time, Geotext. Geomembranes, 42, 111, 10.1016/j.geotexmem.2014.01.004 Ewais, 2018, 17-year elevated temperature study of HDPE geomembrane longevity in air, water and leachate, Geosynth. Int., 25, 525, 10.1680/jgein.18.00016 Földes, 1987, Degradation of HDPE and LLDPE in closed mixing chamber: a comparison, Polym. Bull., 18, 525, 10.1007/BF00255337 2021 Gulmine, 2002, Polyethylene characterization by FTIR, Polym. Test., 21, 557, 10.1016/S0142-9418(01)00124-6 Hsuan, 1998, Antioxidant depletion lifetime in high density polyethylene geomembranes, J. Geotech. Geoenviron. Eng., 124, 532, 10.1061/(ASCE)1090-0241(1998)124:6(532) Hsuan, 2008 Jergensen, 1999 Lee, 1998, Effect of comonomer sequence distribution of LLDPE on miscibility of HDPE/LLDPE blends in the melt state, J. Ind. Eng. Chem., 4, 170 Lu, 1991, Discontinuous crack growth in polyethylene under a constant load, J. Mater. Sci., 26, 917, 10.1007/BF00576768 Lupo, 2010, Liner system design for heap leach pads, Geotext. Geomembranes, 28, 163, 10.1016/j.geotexmem.2009.10.006 Lustiger, 1985 Martuscelli, 1980, Properties of polyethylene‐polypropylene blends: crystallization behavior, Makromol. Chem.: Macromol. Chem. Phys., 181, 957, 10.1002/macp.1980.021810417 Morsy, 2017, Performance of blended polyolefin geomembrane in various incubation media based on Std-OIT, Geotech. Front., 2017, 1 Morsy, 2020, Effect of texturing on the longevity of high-density polyethylene (HDPE) geomembranes in municipal solid waste landfills, Can. Geotech. J., 57, 61, 10.1139/cgj-2019-0047 Morsy, 2020, Longevity of twelve geomembranes in chlorinated water, Can. Geotech. J., 58, 479, 10.1139/cgj-2019-0520 Müller, 2003, Oxidative resistance of high density polyethylene geomembranes, Polym. Degrad. Stab., 79, 161, 10.1016/S0141-3910(02)00269-0 Munaro, 2008, Polyethylene blends: a correlation study between morphology and environmental resistance, Polym. Degrad. Stabil., 93, 43, 10.1016/j.polymdegradstab.2007.10.017 Queja, 1995 Rachtanapun, 2004, Effect of the high‐density polyethylene melt index on the microcellular foaming of high‐density polyethylene/polypropylene blends, J. Appl. Polym. Sci., 93, 364, 10.1002/app.20428 Rowe, 1988, Contaminant migration through groundwater: the role of modelling in the design of barriers, Can. Geotech. J., 25, 778, 10.1139/t88-087 Rowe, 2011, Systems engineering: the design and operations of municipal solid waste landfills to minimize leakage of contaminants to groundwater, Geosynth. Int., 16, 391, 10.1680/gein.2011.18.6.391 Rowe, 2016, Antioxidant depletion in HDPE geomembrane with HALS in low pH heap leach environment, Can. Geotech. J., 53, 1612, 10.1139/cgj-2016-0026 Rowe, 2003, Evaluation of an HDPE geomembrane after 14 years as a leachate lagoon liner, Can. Geotech. J., 40, 536, 10.1139/t03-019 Rowe, 2009, Ageing of HDPE geomembrane exposed to air, water and leachate at different temperatures, Geotext. Geomembranes, 27, 137, 10.1016/j.geotexmem.2008.09.007 Rowe, 2010, Antioxidant depletion from an HDPE geomembrane under simulated landfill conditions, ASCE J. Geotech. Geoenviron., 136, 930, 10.1061/(ASCE)GT.1943-5606.0000302 Rowe, 2013, Effect of underliner on geomembrane strains in heap leach pad applications, Geotext. Geomembranes, 40, 37, 10.1016/j.geotexmem.2013.07.009 Rowe, 2014, Aging of HDPE geomembrane of three different thicknesses. Journal of Geotechnical and Geoenvironmental Engineering, ASCE, 140, 1 Rowe, 2019, Representative stress crack resistance of polyolefin geomembranes used in waste management, Waste Manag., 100, 18, 10.1016/j.wasman.2019.08.028 Rowe, 2020, An approach to HDPE geomembrane selection for challenging design requirements, Can. Geotech. J., 57, 1550, 10.1139/cgj-2019-0572 Scheirs, 2009 Schellenberg, 1998, Environmental stress cracking resistance of blends of high‐density polyethylene with other polyethylenes, Polym. Eng. Sci., 38, 1413, 10.1002/pen.10311 Seeger, 2003, Theoretical approach to designing protection: selecting a geomembrane strain criterion, 137 Smith, 2008, Emerging issues in heap leaching technology Teh, 1994, A review of polyethylene–polypropylene blends and their compatibilization, Adv. Polym. Technol.: J. Polym. Proc. Inst., 13, 1, 10.1002/adv.1994.060130101 Thiel, 2004, State of the practice review of heap leach pad design issues, Geotext. Geomembranes, 22, 555, 10.1016/j.geotexmem.2004.05.002 Wong, 2011 Zha, 2022, Review on lifetime predictions of polyethylene pipes: limitations and trends, Int. J. Pres. Ves. Pip., 198, 10.1016/j.ijpvp.2022.104663 Abdelaal, 2011, OIT Depletion in HDPE GMBs used in contact with solutions having very high and low pH