Crack initiation mechanism of laser powder bed fusion additive manufactured Al-Zn-Mg-Cu alloy
Tài liệu tham khảo
Zhou, 2020, Selective laser melting additive manufacturing of 7xxx series Al-Zn-mg-cu alloy: cracking elimination by co-incorporation of Si and TiB2, Addit. Manuf., 36
Wang, 2021, Fast aging strengthening by hybrid precipitates in high pressure die-cast Al-Si-cu-mg-Zn alloy, Mater. Charact., 179, 10.1016/j.matchar.2021.111312
Dong, 2020, Wire arc additive manufacturing of Al-Zn-mg-cu alloy: microstructures and mechanical properties, Addit. Manuf., 36
Klein, 2021, Wire-arc additive manufacturing of a novel high-performance Al-Zn-mg-cu alloy: processing, characterization and feasibility demonstration, Addit. Manuf., 37
Yi, 2022, A novel hierarchical manufacturing method of the selective laser melted Al 7075 alloy, SSRN Electron. J., 191
Satoh, 2013, Strength and microstructure of laser fusion-welded Ti-SS dissimilar material pair, Int. J. Adv. Manuf. Technol., 66, 469, 10.1007/s00170-012-4342-6
Leon, 2017, Effect of surface roughness on corrosion fatigue performance of AlSi10Mg alloy produced by selective laser melting (SLM), Mater. Charact., 131, 188, 10.1016/j.matchar.2017.06.029
Martin, 2017, 3D printing of high-strength aluminium alloys, Nature., 549, 365, 10.1038/nature23894
Gu, 2021, Material-structure-performance integrated laser-metal additive manufacturing, Science (80), 372
Cao, 2016, Effects of Cu addition on the precipitation hardening response and intergranular corrosion of Al-5.2Mg-2.0Zn (wt.%) alloy, Mater. Charact., 122, 177, 10.1016/j.matchar.2016.11.004
Dong, 2019, Effects of Cu content on microstructure and properties of super-high-strength Al-9.3Zn-2.4Mg-xCu-Zr alloy, J. Alloys Compd., 788, 329, 10.1016/j.jallcom.2019.02.228
Zuo, 2017, The mechanism of grain refinement and plasticity enhancement by an improved thermomechanical treatment of 7055 Al alloy, Mater. Sci. Eng. A, 702, 42, 10.1016/j.msea.2017.06.106
DebRoy, 2018, Additive manufacturing of metallic components – process, structure and properties, Prog. Mater. Sci., 92, 112, 10.1016/j.pmatsci.2017.10.001
Holzer, 2016, Change of hot cracking susceptibility in welding of high strength aluminum alloy AA 7075, Phys. Procedia, 83, 463, 10.1016/j.phpro.2016.08.048
Kusoglu, 2020, Research trends in laser powder bed fusion of Al alloys within the last decade, Addit. Manuf., 36
Casati, 2019, Development of a high strength Al–Zn–Si–mg–cu alloy for selective laser melting, J. Alloys Compd., 801, 243, 10.1016/j.jallcom.2019.06.123
Montero Sistiaga, 2016, Changing the alloy composition of Al7075 for better processability by selective laser melting, J. Mater. Process. Technol., 238, 437, 10.1016/j.jmatprotec.2016.08.003
Otani, 2019, Microstructure and mechanical properties of A7075 alloy with additional Si objects fabricated by selective laser melting, Mater. Trans., 60, 2143, 10.2320/matertrans.Y-M2019837
Li, 2022, Investigation into the effect of energy density on densification, surface roughness and loss of alloying elements of 7075 aluminium alloy processed by laser powder bed fusion, Opt. Laser Technol., 147, 10.1016/j.optlastec.2021.107621
Tan, 2021, A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting, Mater. Sci. Eng. A, 821, 10.1016/j.msea.2021.141638
Zhang, 2022, Towards understanding metallurgical defect formation of selective laser melted wrought aluminum alloys, Adv. Powder Mater., 1
Wang, 2021, Microstructure evolution and properties of nanoparticulate SiC modified AlSi10Mg alloys, Mater. Sci. Eng. A, 808, 10.1016/j.msea.2021.140864
Liu, 2022, High power laser powder bed fusion of AlSi10Mg alloy: effect of layer thickness on defect, microstructure and mechanical property, Mater. Sci. Eng. A, 842, 10.1016/j.msea.2022.143107
Liu, 2021, Hot cracking in ZK60 magnesium alloy produced by laser powder bed fusion process, Mater. Lett., 301, 10.1016/j.matlet.2021.130283
Qiu, 2019, On the solidification behaviour and cracking origin of a nickel-based superalloy during selective laser melting, Mater. Charact., 148, 330, 10.1016/j.matchar.2018.12.032
Chandra, 2021, A generalised hot cracking criterion for nickel-based superalloys additively manufactured by electron beam melting, Addit. Manuf., 37
Chen, 2016, Dendritic microstructure and hot cracking of laser additive manufactured Inconel 718 under improved base cooling, J. Alloys Compd., 670, 312, 10.1016/j.jallcom.2016.01.250
Kontis, 2019, Atomic-scale grain boundary engineering to overcome hot-cracking in additively-manufactured superalloys, Acta Mater., 177, 209, 10.1016/j.actamat.2019.07.041
Sun, 2019, Revealing hot tearing mechanism for an additively manufactured high-entropy alloy via selective laser melting, Scr. Mater., 168, 129, 10.1016/j.scriptamat.2019.04.036
Sufiiarov, 2017, The effect of layer thickness at selective laser melting, Proc. Eng., 174, 126, 10.1016/j.proeng.2017.01.179
Shi, 2020, Effect of high layer thickness on surface quality and defect behavior of Ti-6Al-4V fabricated by selective laser melting, Opt. Laser Technol., 132, 10.1016/j.optlastec.2020.106471
Tang, 2012, Orientation selection process during the early stage of cubic dendrite growth: a phase-field crystal study, Acta Mater., 60, 5501, 10.1016/j.actamat.2012.07.012
Kou, 2015, A criterion for cracking during solidification, Acta Mater., 88, 366, 10.1016/j.actamat.2015.01.034
Zhang, 2021, A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting, Addit. Manuf., 38
Chen, 2017, Strength and strain hardening of a selective laser melted AlSi10Mg alloy, Scr. Mater., 141, 45, 10.1016/j.scriptamat.2017.07.025
Xiao, 2022, Niobium nanoparticle-enabled grain refinement of a crack-free high strength Al-Zn-mg-cu alloy manufactured by selective laser melting, J. Alloys Compd., 900, 10.1016/j.jallcom.2021.163427
Schaffnit, 2015, A Scheil–Gulliver model dedicated to the solidification of steel, Calphad., 48, 184, 10.1016/j.calphad.2015.01.002