Rummel, 1970, Determination of the post-failure behavior of brittle rock using a servo-controlled testing machine, Rock Mech., 2, 189, 10.1007/BF01245574
Hudson, 1972, Soft, stiff servo-controlled testing machines: a review with reference to rock failure, Engng Geol., 6, 155, 10.1016/0013-7952(72)90001-4
Okubo, 1985, Uniaxial compression testing using a linear combination of stress and strain as the control variable, Int. J. Rock Mech. Min. Sci. & Geomech. Abstr., 22, 323, 10.1016/0148-9062(85)92064-9
Okubo, 1988, The control performance of servo-controlled testing machines, J. MMIJ, 104, 63
Okubo, 1987, Time dependent behaviour in uniaxial compression (rheological behaviour of rock in post-failure region), J. MMIJ, 103, 177
Okubo, 1987, Simulation of rock deformation around roadway by non-linear rheological model, J. MMIJ, 103, 293